Lignin blocking effects on weathering process of wood plastic composites
2010 - IRG/WP 10-40529
The weathering of wood–plastic composites (WPC) causes discoloration which affects their aesthetic aspects. It has been proved that these discolorations are due to lignin degradation. Effects of blocking the susceptible structure of lignin assessed by chemical treatment such as acetylation and methylation are reported in this study. Surface chemical change of wood plastic composite (WPC) formula...
P Darabi, A Naghi karimi, S Ahmade Mirshokraie, M-F Thévenon


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


The effects of acetylation level on the growth of Postia placenta
2011 - IRG/WP 11-10751
To understand the defence mechanisms utilized by decay fungi when exposed to different wood protection systems the study of gene expression can give us some answers. When the DNA sequences are known, primers can be designed to detect transcripts of genes with gene products related to basic cellular processes and hyphal growth. The characteristic gene products induced in different fungi by differen...
A Pilgård, G Alfredsen, C G Fossdal, C J Long II


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Effects of Nano-Wollastonite on Ignition Time Reduction in MDF
2012 - IRG/WP 12-40576
Effects of wollastonite nano-fibers on ignition time reduction in medium density fiberboard were studied. Nanowollastonite was applied at 5, 10, 15, and 20 g/kg dry weight basis of wood fibers and compared with control specimens. Two application methods of nanowollastonite were used: surface application, and internal application. Specimens of 150×130×9 mm were prepared and the ignition times wer...
H Reza Taghiyari, H Rangavar, P Noori, A Karimi


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


The effects of acetylation level on the growth of Postia placenta over 36 weeks
2012 - IRG/WP 12-40589
Genomic sequencing gives us a tool to systematically and rapidly discover novel genes, how their products function in the cell, and explore their interactions. When the DNA sequences are known, primers can be designed to detect transcripts of genes with gene products related to basic cellular processes and hyphal growth. The characteristic gene products induced in different fungi by different wood...
A Pilgård, G Alfredsen, C G Fossdal, C J Long II


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Use of Acoustic Emission (AE) to detect activity of common European dry-woodboring insects: some practical considerations
2013 - IRG/WP 13-10803
Old house borer (Hylotrupes bajulus), Furniture beetle (Anobium punctatum), and Deathwatch beetle (Xestobium rufovillosum) are common dry-woodboring insects occurring throughout Europe. With the aim to prevent unnecessary use of biocidal products, to protect valuable wooden elements and objects from unwanted influences, and to have a more objective method, SHR has started to study the use of acous...
J G M Creemers


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


The effects of copper proximity on oxalate production in Fibroporia radiculosa
2014 - IRG/WP 14-10823
Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess d...
K M Jenkins, C A Clausen, F Green III


Effects of thermal modification on properties of Douglas-fir heartwood
2014 - IRG/WP 14-40663
The flexural properties and mass losses of thermal modified Douglas-fir pretreated with boron or glycerol were examined. Pretreatments were associated with slight, but not significant, reductions in modulus of rupture (MOR) and modulus of elasticity (MOE)of Douglas-fir at different thermal treatment levels. Boron pretreatment had the greatest effect on MOR. MOR of non-pretreated and ...
Li Yan, J J Morrell


Borate treatment of green ties: An initial report on the effects on mechanical properties
2014 - IRG/WP 14-40686
Borates are increasingly used as components of wood preservative systems for railway cross ties (“sleepers”) in the USA. A variety of methods exist for incorporating the borate component; however, the so-called ‘two-step’ treatment, which involves treating the green tie in borate, followed by a pressure treatment with creosote or copper naphthenate after drying (‘seasoning’), offers th...
A M Taylor, J D Lloyd


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Effects of geographical and dietary variation on the symbiotic flagellate protists communities of the subterranean termite Reticulitermes grassei Clément
2015 - IRG/WP 15-10847
Despite their importance on diverse ecosystems, termites may also be considered severe pests of wood in service, and also as agricultural and forestry pests. Subterranean termites’ ability to digest lignocellulose relies not only on their digestive tract physiology, but also on the symbiotic relationships established with flagellate protists and bacteria. In this tripartite lignocellulolytic sy...
S Duarte, M Duarte, P A V Borges, L Nunes


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Study on the Effects of Flame Retardant in Dancheong for Korea Wooden Cultural Heritage
2015 - IRG/WP 15-40692
This study identifies the effect of the agent depending on environment change and conducted basic study to prepare criteria for stable application. Dancheong sample, which is similar to wooden cultural heritage, was manufactured to study the effect of the agent on dancheong. Regular observation on the samples located in inland and shoreline area in the country detected visible phenomena. Whitening...
Hwa Soo Lee, So Jung Lee, Gyu Seong Han, Yong Jae Chung


Evaluating the Effects of Post Dip-Treatment Laser Marking on Resistance to Feeding by Subterranean Termites
2016 - IRG/WP 16-10854
Dip-treatment of wood packing materials is often used instead of pressure treatment mainly because of issues relating to simplicity and cost. Packaging boxes fabricated for the United States Army are required to be dip-treated for at least one minute in an approved preservative solution prior to use. These boxes are expected to have a service life of up to 20 years in a wide variety of environment...
R A Arango, B Woodward, S Lebow