IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 269 documents. Displaying 25 entries per page.


Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot


Surface color and roughness characteristics of medium density fiberboard (MDF) panels treated with fire retardants
2008 - IRG/WP 08-40420
The objective of this study was to determine surface characteristics and color change properties of Medium Density Fiberboard (MDF) treated by fire retardants (FR) with 10% concentration. Experimental panels were made using by melamine ureaformaldehyde (MUF) adhesive having 10%, 15%, 20% of melamine. The surface properties of the samples were determined using a fine stylus technique. Three roughn...
D Ustaömer, M Usta, S Hiziroglu


The Effects of Solar Radiation on the Fungal Colonization and Color of Weathered Wood
2008 - IRG/WP 08-10676
Solar radiation rapidly depolymerizes lignin at wood surfaces exposed outdoors producing a suite of low molecular weight aromatic compounds within weathered wood. Fungi colonizing weathered wood are able to metabolize these aromatic compounds, and many of them also contain high levels of melanin to protect themselves from the harmful effects of UV radiation. Both of these adaptations suggest that ...
V Hernandez, C Breuil, P D Evans


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Control de calidad eficiente de proteccion superficial sobre madera
2008 - IRG/WP 08-20397
Quality control is important to assure efficient protection of wood surfaces. When wood is exposed to the environment, it degrades due to weathering or environmental factors alone. Aging tests are utilized to test coating products. Quality control techniques are performed on exposed products according to standardized methods (NCh, ASTM, ISO, DIN, EN, FTMS, NTF, NBINT, or equivalents). Certified l...
A M Fernández S


Biological efficacy of micronized copper systems
2008 - IRG/WP 08-30485
Soil block, fungal cellar and field stake test data will be presented for micronized copper systems. The copper portion of the formulations is present as a fine dispersion of "micro" particulates while the co-biocide is present as either a soluble quat or an azole containing emulsion. This testing generally used the amine based counterpart as the control preservative system and the micronized fo...
C R McIntyre, M H Freeman


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


The effect of different foundation systems against fungal flora in the crawl space of a new wooden Japanese house
2009 - IRG/WP 09-10700
In order to establish novel preventive measures against damage of wooden houses by decay fungi with less-use or no-use of chemicals, we periodically monitored the fungal flora in the crawl space of a new wooden Japanese house build with recyclable and low-environmental load materials at the Research Institute for Sustainable Humanosphere, Kyoto University. We employed either a layer of concrete or...
A Toyoumi, S Horisawa, T Yoshimura, S Doi,Y Imamura


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Review of candidate graded particle barrier testing methods in Australian Standard (AS 3660.3 – 2000): Assessment criteria for termite management systems
2009 - IRG/WP 09-20417
The Australian Standard (AS. 3660.3 – 2000) for assessment of candidate graded particle termite barriers is reviewed and suggestions for amendments are made. Areas requiring amending in light of current biological knowledge involve the inclusion of proprietary or patented systems rather than generic types; selection of test termites in the genus Coptotermes; duration of test periods; and inadequ...
J R J French, B M Ahmed (Shiday), B L Schafer


Continuous moisture measurement (CMM) to detect failure of moisture resistance
2009 - IRG/WP 09-20422
A wood coating system will fail to perform properly after a certain time of weathering. From that moment, the substrate is especially prone to fungal attack. Moisture plays a key role on weathering performance, wood protection efficacy and decay susceptibility of wood. Therefore, knowledge of the moisture dynamics of the applied wood protection is of significant importance in the prediction of the...
I De Windt, J Van den Bulcke, J Van Acker


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Differential response of wood to dry air thermal treatment (DATT) and soy oil thermal treatment (SOTT)
2009 - IRG/WP 09-40446
Thermal treatment is an alternative to chemical modification method which has been used to some extent in improving timber quality. In order to get the maximum benefits possible without compromising the various end-use quality requirements of timber, several possibilities have been and are still being investigated in relation to this technique. Clear wood samples (19 x 19 x 150mm) of kiln-dried re...
L Awoyemi


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip, flood coat or spray, and rapidly penetrates to the centre of timber substrates, whether containing sapwood or heartwood. However, section ...
B M Ahmed (Shiday), J R J French


Previous Page | Next Page