Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Investigations into the use of Maleic Anhydride/Sodium Hypophosphite as a Wood Modification Process
2020 - IRG/WP 20-40891
The formation of crosslinked bonds between wood constituents is believed to be an effective way to stabilize wood against wet conditions. The possibility to use maleic anhydride (MA) combined with sodium hypophosphite (SHP) as crosslinking agents was studied, using Scots pine sapwood and a model compound. The modified wood showed weight gain and bulking effect after treatment and subsequent Soxhle...
I Kim, D Jones, O Karlsson, D Sandberg, O N Antzutkin, F Ullah Shah


Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga


Utilization of Pressure Treated Lumber in Cross Laminated Timber Manufacture and its Impact on Bondline
2022 - IRG/WP 22-40953
Mass timber building construction is increasing dramatically across North America which presents challenges to these structures not seen in Northern Europe. Large parts of the United States harbor termites and existing mass timber building technologies that rely solely on moisture exclusion to increase durability are insufficient in these areas. The successful expansion of mass timber construction...
G Presley, C Wainscott, J Valenti, S Noble


Identifying compatible waterborne timber preservatives and fire retardants for use in a VPI system: a practical approach
2023 - IRG/WP 23-30796
To enhance the use and suitability of timber in all applications in both exterior and interior settings, timber typically needs to be treated with a preservative and/or a fire retardant chemical. Combining fire retardants with preservatives into a single treatment process has been a long-term aim of researchers in the timber preservative industry because of the significant logistic and economic ad...
R Robinson, S Meldrum


Field test methods as long-term aging – report of selective wood properties
2023 - IRG/WP 23-40962
Wood samples from a long-term field test are a valuable compendium of information about the material in the context of its aging processes. In the current work, wood samples from the round-robin test within the ECOMOD project were used as a material for the natural aging process (III and IV class of utility). The research scope was to determine selected properties of this wood which can be partial...
W Perdoch, M Benc, B Mazela, A Szulc, J Cegiela


Non-vacuum/pressure ACQ treatment
2023 - IRG/WP 23-40971
Many developing countries are located in sub-tropical or tropical regions where rapid wood deterioration results in early failure of many structures. Whilst preservative treatment would help to reduce these losses and extend the forest resource commercial vacuum pressure treatment systems are often too expensive. The use of lower technology treatment systems, while not as quick as vacuum pressure ...
J Norton


New wood-modification process based on grafted urethane groups: Durability of carbamamylated Scots pine (Pinus sylvestris L.) wood
2023 - IRG/WP 23-40974
Substituting commonly used toxic preservatives with wood modification treatments can make the wood material less prone to water and moisture uptake. This approach favours a more sustainable protection of wood against biodegradation. In this study, Scots pine sapwood was full-cell impregnated with an aqueous solution of urea (30%), dried at 40°C for 24h, and subsequently heat-treated at 150°C for...
C-F Lin, O Myronycheva, O Karlsson, D Jones, D Sandberg


Elevated pressure hybrid wood modification: Synergistic effects on durability performance
2024 - IRG/WP 24-20725
The combination of different wood modification technologies to obtain improved performance is increasingly receiving attention in research. In this study, Scots Pine was impregnated with furfuryl alcohol (FFA) in pure aqueous 20, 40 and 60% solution strength without adding any catalyst. In a second step, the FFA was polymerized while simultaneously performing thermal modification in a closed syste...
P Klaas, D Jones


Exploring bio-based chemicals in the residual stream from the thermal wood modification process
2024 - IRG/WP 24-30799
Numerous chemical-free processes have emerged in the wood processing industry to enhance the durability and optimize the service life of wooden elements exposed to exterior conditions. One such method, the hygrothermolytic modification process, patented as FirmoLin®, represents an industrial treatment for thermal modification of wood. This involves subjecting solid wood to a pressurized unsaturat...
R Herrera, W Willems, W Pajerski, A Selmanović, A Sandak