IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 664 documents. Displaying 25 entries per page.


Partial seasoning and preservative treatment systems for pine roundwood
1982 - IRG/WP 3187
Experimental trials at FRI, Rotorua showed that the steaming schedule normally used for steaming and venting is also suitable for steaming and vacuum seasoning. Applying vacuum of up to -84 kPa immediately after steaming did not increase the initial loss of wood moisture significantly in comparison to steam/venting. The main improvement to wood condition by using steam/vacuum appeared to be to dis...
A J Bergervoet


Correlation between modulus of elasticity, mass losses and FTIR spectra of copper treated decayed wood
2006 - IRG/WP 06-10580
The composition of copper-based preservatives will change from copper-chromium to copper-ethanolamine, due to environmental demands. The most important drawback of copper-impregnated wood is the presence of tolerant fungal organisms that have developed an ability to degrade such preserved wood. In order to elucidate these processes, specimens (0.5×1.0×15 cm) made of Norway spruce (Picea abies) w...
M Humar, B Bucar, F Pohleven


Efficacies of an insecticide and a fungicide for preventing blue-stain of Japanese red pine logs
2006 - IRG/WP 06-20329
We examined blue-stain fungi on Japanese red pine at 3 forests and 2 saw mills in Iwate Prefecture, Japan. The isolated ophiostomatoid fungi were Leptographium sp and Ophiostoma sp. There were 3 routes of the blue-stain; fungal growth from the spore or hypha stuck on the cross cut surfaces, fungal spread through the inner bark by bark beetles and fungal invasion around whorled knot. The larger ext...
H Taniuchi, T Koiwa, H Masuya, S Doi


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


Qualitative and quantitative assessment of chemicals used for wood durability improvement by Near Infrared Spectroscopy
2006 - IRG/WP 06-20349
The Near infrared spectroscopy (NIRS) could be a suitable technique to assess chemicals used for wood durability improvement in the forest products industry. NIRS methodology can be used to obtain results more quickly, less costly and without damaging the wood. In this study, wood samples selected from heartwood and sapwood of Maritime Pine (Pinus pinaster) were prepared to assess the artificial d...
S Zahri, F Charrier, H Baillères, B Charrier


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


Ionic liquids with organic and inorganic anions as highly active wood preservatives
2006 - IRG/WP 06-30411
Quaternary ammonium tetrafluoroborates, nitrates(V), propionates, acetates and formates with alkoxymethyl substituents were prepared and tested on wood destroying and sapstaining fungi. These new compounds are ionic liquids (ILs), which penetrate very well into Scot pine wood. Alkoxymethyldecyldimethylammonium tetrafluoroborates and nitrates(V) show better microbial activity against Coniophor...
J Zabielska-Matejuk, A Skrzypczak


Underwater shock treatment for improvement of penetration of wood
2006 - IRG/WP 06-40325
Many of conifers including Beimatsu (Pseudotsuga menziesii Franco; Dougras fir, Oregon pine), Akamatsu (Pinus densiflora Sieb. et Zucc.; Japanese red pine), Dafurica Karamatsu (Larix gmelinii Gordon; Dahurica larch) and Karamatsu (Larix leptolepis GORDON; Japanese larch) generally contains the high moisture content. Although subjected to the drying process, it is difficult to be dried up completel...
S Itoh, H Maehara, K Tanaka, T Echigo, K Morioka, E Shirai, K Nishimoto


Resistance of DMDHEU-treated pine wood against termite and fungi attack in field testing according to EN 252. Results after 30 months
2006 - IRG/WP 06-40354
The aim of this study was to determine the effectiveness against decay and termite attack of pine sapwood treated with pure and modified DMDHEU in a field test according to European Standard EN 252. Some of the treatments tested were able to increase, within the period of the test reported (30 months), the resistance of the wood both to micro-organisms and termites. The curing process seems to be ...
S Schaffert, L Nunes, A Krause, H Militz


Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Preliminary Observations of the Effect of Kerfing on the Surface Checking and Warping of Flat Sawn Southern Pine Decking
2007 - IRG/WP 07-20360
Checking and warping of decking timber are serious defects and methods of reducing their severity are required to ensure that wooden decking can compete with alternative decking materials. Kerfing is effective at reducing the checking and distortion of square cross-section lumber, and the checking of roundwood. In the past it has also been applied to preservative treated decking boards, however, t...
R Ratu, J Weizenegger, P Evans


Effects of heat treatments on decay resistance and material properties of ponderosa pine and yellow poplar
2007 - IRG/WP 07-40374
The potential for using heat treatment to improve the properties of North American fenestration species was evaluated on ponderosa pine (Pinus ponderosa L) and yellow poplar (Liriodendron tulipifera L) treated using the ThermoWood process at various treatment temperatures and times. Soil block tests using Gloeophyllum trabeum, Postia placenta, or Trametes versicolor showed that durability was enh...
C Vidrine, C Freitag, J Nicholson, J J Morrell


Wood furfurylation process development. Part 2: Lowry impregnation trials
2007 - IRG/WP 07-40377
The objective was to evaluate whether Lowry-impregnation of Scots pine with FA100-mix, instead of the FA40-mix, would lead to similar or slightly higher WPGs and to investigate any potential changes in penetration pattern. The results indicate that the penetration was better, also penetrating the outer zone of the heartwood. Furthermore, it was possible to reduce the WPG-levels for pine down to 50...
M Westin, E Larnøy, S Lande


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


The Effect of Solar Radiation on the Surface Checking of Wood
2007 - IRG/WP 07-40356
The aim of this research was to investigate whether exposure to solar radiation increases the checking of wood exposed to the weather, and examine the causes and spectral dependency of such an effect. Lodgepole pine samples were exposed outdoors under filters which transmitted selected regions of the solar spectrum while allowing other weathering factors to act on samples. Surface checking in samp...
P Evans, K Urban


The effect of an ionic liquid of imidazolium tetrafluoroborates series on Scots pine wood properties
2007 - IRG/WP 07-40357
Ionic liquids (ILs) of imidazolium tetrafluoroborates series penetrate Scots pine wood very well and are active against wood destroying fungi. The requirement to use ILs as wood preservatives is determined by the liquid influence on the functional properties of wood. Investigations were undertaken to clarify the influence of an ionic liquid, 3-heptyloxymethyl-1-methylimidazolium tetrafluoroborate ...
A Fojutowski, R Szukala, J Pernak


Comparative study between full cell and passive impregnation method of wood preservation for laser incised Douglas-fir lumber
2007 - IRG/WP 07-40359
Many wood species are highly resistant to conventional pressure treatment. To improve the chemical impregnation into Douglas-fir (Pseudotsuga menziesii Franco) lumber, the passive impregnation method had been developed. In this study, ability of the passive impregnation for lumber was compared with a conventional full cell method. Square Douglas-fir lumber with the incising density of 10,000 holes...
Md N Islam, K Ando, H Yamauchi, Y Kobayashi, N Hattori


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


The effects of chemical modification on the biological properties of alder and spruce particleboards
2007 - IRG/WP 07-40363
This study is evaluated by measuring the weight loss, and the ability of white and brown-rot fungi to attack unmodified and modified particleboards manufactured using spruce (Picea orientalis (L.) Link.) and alder (Alnus glutinosa) chips. The chips were reacted with acetic, succinic, maleic and phthalic anhydride at constant temperature for 3 hours then, hot pressed at 150 °C by using phenol for...
Ü C Yildiz, E Dizman, S Yildiz, A Temiz, M Aslan, E D Gezer


Previous Page | Next Page