Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


Does Limnoria lignorum (Rathke) or other cold-water xylophagous limnoriid species exist in southern oceans?
1989 - IRG/WP 4152
The question is posed whether the cold-water limnoriid wood borer Limnoria lignorum (Rathke), or any other such cold-water limnoriid exists in southern oceans. The evidence of collections from various high latitude southern coastlines is cited and the singular absence of any cold-water limnoriid borer noted. The need for further. and possibly extensive, searches for such borers is stressed. i.e. i...
J E Barnacle, L J Cookson


Ponding of radiata pine (Pinus radiata) - 1. The effect of bacteria on wood
1998 - IRG/WP 98-10265
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks were examined by light microscopy, confocal laser scanning microscopy (CLSM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) for bacterial colonisation of wood and degradation of pit membranes. After 2 weeks of ponding bacteria colonised the outer few cells of wood, ...
A P Singh, Y S Kim, U Schmitt, B S Dawson


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


Long term experiments for assessing the diffusion of boric acid and diluorides from local preservative pills in spruce and pine
1996 - IRG/WP 96-40065
For the experimental assessment of the diffusion of boric acid and difluorides over a three year period 2 tests were set up. In a test with large spruce blocks (150 x 150 x 300 mm³) 3 different pill types were exposed to 3 different climates: climate room (20°C, 65% r.h.), wet room (20°C, 95% r.h.), and to outside exposure. In a test with open L-joints without paint, with an alkyd paint and wit...
W J Homan, H Militz


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The influence of fungi causing blue – stain on absorptiveness of Scotch pine wood
2005 - IRG/WP 05-10565
The blue-stain fungi cause discoloration of the wood. In the course of their development in wood may have an effect on wood structures and properties influenced on its use value. Investigation has been undertaken to clear the influence of blue-stain fungi on wood absorptiveness as indicators for the wood ability to impregnation with water diluted wood preservatives. The wet sapwood samples of fres...
A Fojutowski


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Effect of humic acid on leaching of CCA from treated wood
2000 - IRG/WP 00-50151
Laboratory studies indicate that relatively high concentrations (1.000 - 10.000 ppm) of humic acids can increase the leaching of chromium and copper from CCA-C treated wood, and that copper is most affected. They also show that leaching with natural water samples can result in higher leaching of all components than leaching with distilled water. Evaluation of CCA component retentions and mass bala...
P A Cooper, D Jeremic, J L Taylor, Y T Ung


Trials of new treatments for prevention of kiln brownstain of white pine (Pinus strobus)
1995 - IRG/WP 95-30068
White pine (Pinus strobus) often develops a surface brown oxidative stain when kiln dried. Such stain downgrades high quality lumber and is most likely to occur when fresh, unseasoned lumber is stacked during warm weather prior to kiln drying. Use of reducing agents or pH alteration has been successful, but may have some practical limitations for general use. This study attempted to prevent browns...
E L Schmidt, E Christopherson, T L Highley, M H Freeman


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


Mold and stain fungi associated with Radiata pine logs imported from New Zealand
2000 - IRG/WP 00-10346
The Korean sawmills have recently realized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of mold and stain fungi colonized commercially important softwood species (Pinus densifl...
Jae-Jin Kim, Gyu-Hyeok Kim


Surface accumulation of copper on CCA-impregnated Pinus patula stakes during marine preservative trials in the southern hemisphere
1992 - IRG/WP 92-4181
Pinus patula stakes treated with CCA to target retentions of 30 kg/m³ salts were exposed to sea water in marine and estuarine ecosystems off the coast of Southern Africa for two years. Samples were then analysed for copper and arsenic. Analysis of samples from the marine ecosystem showed (IRG/WP/4167) that arsenic was longitudinally and transversely leached from the wood, whereas the copper was r...
G D Shelver, C D McQuaid, M Tarin, A A W Baecker


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Assessment of residual retentions in creosote treated Scots pine (Pinus sylvestris) poles after 45 years ground contact service in the Lemstervaart in the Dutch polder
1994 - IRG/WP 94-50022
In a project funded by the Water State Authorities (RWS) and the Noordoostpolder Water Board, the residual retentions in ten creosote treated Scots pine (Pinus sylvestris) poles were examined after 45 years ground contact service along a canal (Lemstervaart) in the Dutch Noordoostpolder. The Lemstervaart location was selected due to the fact that the poles involved had been originally treated and ...
P Esser, W L D Suitela, A J Pendlebury, H Visscher


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Models of the critical time of humidity and temperature conditions for the development of mould fungi in pine and spruce sapwood
1995 - IRG/WP 95-20066
Regression models of the time factor for the growth of mould fungi in pine and spruce sapwood are studied. The first group of models are based on the results of exposures of mould fungi in static humidity and temperature conditions indicating the time for the start of mould growth in wood. The second group of models are based on the exposures of mould fungi in fluctuating or alternating humidity a...
H Viitanen


Laboratory trial to identify potential in-forest treatments to control fungal pre-infections of radiata pine logs
2000 - IRG/WP 00-30220
Development of fungal infections of radiata pine logs by wood degrading fungi commences immediately after tree felling. In general, subsequent antisapstain treatments are unable to control fungal degrade on logs where the pre-treatment log storage time exceeds 2-5 days. However, use of an in-forest treatment of logs may be advantageous to log exporters to control fungal pre-infections during the p...
D R Eden, B Kreber, R N Wakeling, J G Van der Waals, C M Chittenden


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Effect of bioextracts on colonisation of radiata pine sapwood by three sapstain fungi
2003 - IRG/WP 03-10485
The objective of this study was to investigate the effect of aqueous bioextracts prepared following two-week incubation of forest soil, garden compost and chicken manure respectively, on the ability of Ophiostoma flocossum, Leptographium procerum and Sphaeropsis sapinea to colonise unseasoned radiata pine sapwood. The research showed that all bioextracts tested retarded the rate of fungal colonis...
J van der Waals, C Chittenden, B Kreber


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The selected properties of Scots pine wood blue-stained by fungus Cladosporium herbarum
2003 - IRG/WP 03-10484
The fungi causing primary blue-stain of wood may change wood properties especially when acting in mixture of few fungi species. There were been undertaken investigation to clear the influence of pure culture of one fungus species on selected physical and mechanical properties of Scots pine wood. The twin samples of fresh cut Scots pine sapwood (Pinus sylvestris L.) were exposed into pure culture o...
A Fojutowski