IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 159 documents. Displaying 25 entries per page.


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields


Bending properties of wood after its decay with Coniophora puteana and subsequent modification with selected chemicals
1999 - IRG/WP 99-40146
Mechanical properties of wood are often decreased due to decay processes caused by biotic and/or abiotic factors. Damaged wooden elements (e.g. historical structures) can be reinforced by more methods, including their modification with convenient chemicals. This paper presents influences of selected chemicals on basic bending properties (modulus of elasticity - MOE, modulus of rupture - MOR) of so...
L Reinprecht, S Varinska


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


The effect of heat treatment on the properties of spruce
1994 - IRG/WP 94-40032
The effect of high temperature treatment (above 150°C) on the wood quality is studied at the VTT. Improved dimensional stability, lower equilibrium moisture content and increased durability against biodeterioration is achieved, depending on the environmental factors. The biodeterioration resistance of spruce is improved due to changes in chemical composition and lower equilibrium moisture content...
H Viitanen, S Jämsä, L Paajanen, A J Nurmi, P Viitaniemi


Fungal decay of acrylate treated wood
2004 - IRG/WP 04-30357
Natural durability of wood species is variable. Chemical wood preservatives, such as biocides are necessary for extension of their service life. Many methods have been developed to increase the resistance of wood and wood products against wood-destroying organisms during the last years. The most frequently used methods are chemical and thermal modification of wood. In wood modification the basic c...
Z Tiralova, L Reinprecht


The true dry rot fungus (Serpula lacrymans) as a wound parasite of living Norway spruce (Picea abies) in the Czech Republic
2001 - IRG/WP 01-10389
Some late 19th century Central European mycologist reported finds of the true dry rot fungus (Serpula lacrymans) from nature. They even suggested that it could be a parasite of living trees. However examination of herbarium material has shown that the species they found was thin-fleshed dry rot (Serpula himantioides) rather than Serpula lacrymans. In 1992 the Czech mycologist Kotlaba reported find...
J Bech-Andersen, S A Elborne, J Andreasson, J Ch Sterler


Laser incising of spruce lumber for improved preservative penetration
1991 - IRG/WP 3646
Red spruce heartwood specimens were incised using a range of laser beam power levels and pulse durations. The penetration of CCA through these holes into the wood was monitored after pressure treatment. In addition, green and dried spruce samples were incised using two patterns with incision densities of either 16.1 holes/in² or 21.3 holes/in². Following CCA pressure treatment the samples were t...
B Goodell, F A Kamke, Jing Liu


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


Influence of the decay of spruce chips by the selected fungi on their chemical structure and the pulp properties
2004 - IRG/WP 04-10510
The paper focuses on changes in the weight and in the molecular structure of spruce chips submitted to long-term storing as well as to medium- and long-term model rotting degradation caused by some chosen fungi identified at storing processes on the pile. For the model decay of chips under laboratory conditions during 3 or 6 weeks the white-rot fungi: Phanerochaete chrysosporium, Heterobasidion an...
R Solár, L Reinprecht, A Geffert, F Kacík


Proposal for a method aiming at the quantification of the impact of wood extraction in Life Cycle Assessment
1998 - IRG/WP 98-50113
Life Cycle Assessment has been accepted as an instrument for the assessment of the environmental impact of products. Characterisation factors for impact assessment of emissions from products have been established. To date no characterisation factor exists for the extraction of biotic resources, for example wood. Since the main disadvantage of using wood as a material lies in the extraction of reso...
P Esser, E Van der Voet


The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Bending strength of heat-treated spruce and pine timber
2002 - IRG/WP 02-40242
Heat-treatment of spruce (Picea abies) and pine (Pinus sylvestris) beams (45 x 145 mm) gave a reduction in bending strength of approximately 50%. The bending stiffness (modulus of elasticity) only decreased by 3.5%. Tests were carried out according to EN 408. Another effect of the heat-treatment was increased variation in bending strength. The 5th percentile value of the bending strength, the so c...
C Bengtsson, J Jermer, F Brem


Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Formosan Subterranean Termite Resistance to Heat Treatment of Scots Pine and Norway Spruce
2003 - IRG/WP 03-40264
New challenges to the durability of wood building materials have arisen in the U.S. The Formosan subterranean termite (Coptotermes formosanus Shiraki) now infests sizable portions of the U.S. south and their range is extending. Heat treatments offer a unique opportunity for wood-based composites because many of the process techniques already employ various thermal applications and could be easil...
W R Smith, A O Rapp, C R Welzbacher, J E Winandy


The effect of kerfing on check formation in treated white spruce (Picea glauca) poles
1981 - IRG/WP 3167
62 white spruce poles, 6 m in length, were cut from full size utility poles commercially pressure treated with preservative. 21 of the poles were treated with pentachlorophenol, while of the remainder, all of which were treated with ammoniacal copper arsenate, 22 were kerfed and 19 were unkerfed. The poles were installed in the Westham Island field test site, near Vancouver, and inspected annually...
J N R Ruddick


Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


Previous Page | Next Page