Improvement of intrinsic properties of wood by chemical wood densification - Hydrophobic aspects and durability aspects
1999 - IRG/WP 99-40149
To improve the intrinsic properties of Scot pine wood ((1) hydrophobic surface and (2) durability), two ways of chemical modification have been tested. The first one is the chemical modification of hydroxyl groups by active substances like diisocyanate compounds with a copolymerization step. The second way is a densification by an impregnation of resins and a gamma polymerisation. This second way ...
G Labat, Q K Tran, I Le Bayon


Water repellency of wood treated with alkylammonium compounds and chromated copper arsenate
2000 - IRG/WP 00-30231
The comparative water sorption properties of southern pine treated with CCA and several alkylammonium compounds was evaluated for freshly treated wood and for wood after exposure in a fungus cellar. It was found that CCA imparts considerable water repellency to wood which is reduced somewhat after exposure to wet soil. With the exception of a long chain (C20 -C22) compound, the alkylammonium compo...
D D Nicholas, A Kabir, A D Williams, A F Preston


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora


Determination methods of phytotoxic effect of wood preservatives
1990 - IRG/WP 2349
The phytotoxic effect of wood preservatives so widely used plays a considerable role in the protection of natural environment. A review was made of the existing methods with which to assess the phytotoxicity of the above chemicals and some suggestions were given concerning the methods most appropriate for their unification. Two areas of research are proposed: 1) estimating the direct effect on ind...
A Kundzewicz, J Wazny


Leaching of preservative components from pine decking treated with CCA and copper azole, and interactions of leachates with soils
2001 - IRG/WP 01-50171
Radiata pine decking was treated with CCA and copper azole preservatives to Australian H3 retention using conventional and modified Bethel schedules, and air-dried. Treated decking boards and durable hardwood controls were subjected to leaching in weather-exposed decks, and matching 19mm cubes were leached in extended AWPA E11-97 lab tests. Deck runoff and E11 leachate water was analysed after rai...
M J Kennedy, P A Collins


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


Pentachlorophenol and tributyltin oxide - the performance of treated Pinus radiata after 12 years' exposure
1986 - IRG/WP 3361
Pinus radiata samples were impregnated with a range of light organic solvent preservatives and copper/chrome/arsenic salt and exposed with no surface coating both in and above ground for 12 years. Inspection of the test samples revealed that some formulations of light organic solvent preservatives will give good fungal protection and reduce splitting in Pinus radiata exposed externally without a s...
R S Johnstone


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Effect of nutrient regimes, temperature, pH, and wood sterilization method on performance of selected bioprotectants against wood staining fungi
1992 - IRG/WP 92-1551
The effect of nutrient regimes, incubation temperature, media pH, and wood sterilization method on performance of four potential bioprotectants (Pseudomonas putida, Pseudomonas cepacia, Bacillus subtilis, and Trichoderma harzianum) against wood staining fungi were evaluated using small ponderosa pine samples over a four week period. Incubation at 32°C resulted in slight increases in the degree of...
J J Morrell, C M Secton


Investigations of the treatability of various commercially significant Turkish timbers
1976 - IRG/WP 370 E
Timbers which naturally deteriorate quickly can only be used commercially when their life is increased by the use of chemical treatments. The treatment of the timber can only be planned on a regular basis when the treatability of the wood is known. The purpose of the experiments was therefore to determine to what extent the various types of wood could be sufficiently impregnated. The question of t...
R Ilhan


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Preliminary evaluations of a small wafer assay for screening potential biological control agents
1989 - IRG/WP 2332
Screening potential biological agents for controlling wood decay fungi poses a dilemma. The ideal test would eliminate as many variables as possible. Most tests utilize pure cultures of the test organism on an artificial media which in no way resembles wood. The use of sawdust improves this approach, but the sawdust increases fungal access to the lignocellulose matrix, potentially inflating the im...
C M Freitag, J J Morrell


Movement of water through quaternary ammonium treated wood
1987 - IRG/WP 3440
Radiata pine sapwood stakes were treated with didodecyl methyl 1, 3 dichloropropenyl ammonium chloride and distearyl dimethyl ammonium chloride. Various ratios of these two chemicals were, tested to determine the extent of water movement through the treated wood. Measurements were taken of the amount of water moved through the wood, degree of wetting of various sectors of the stakes, and the distr...
P J Hayward, J Duff


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Proposals for further co-operative studies on determining toxic values against wood-destroying Basidiomycetes
1985 - IRG/WP 2237
Document IRC/WP/2194 reported the status of the programme of co-operative experiments up to and including December 1982. During discussions at IRG-13 in Turkey members endorsed the decision to complete the programme of tests and conduct repeat tests. At IRG-14 in Brisbane the report was noted but no further action agreed. At IRG-15 in Sweden a number of interested parties in the European/Scandinav...
A F Bravery


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Time limits for holding logs to achieve successful antisapstain treatment
1997 - IRG/WP 97-30126
The purpose of these trials was to determine the maximum time that logs can be left in winter and summer before treatment if sapstain, caused by pre-treatment infection, was to be prevented. Pre-treatment storage conditions representative of average temperature and humidity for the winter months of June, July and August, and of moderately severe summer conditions, for the Bay of Plenty, New Zealan...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright