IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 581 documents. Displaying 25 entries per page.


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


An evaluation of chemical pre-treatments for controlling kiln brown stain in radiata pine
1997 - IRG/WP 97-30124
Clear radiata pine (Pinus radiata D. Don) is widely used for fine millwork owing to its attractive light colour. However, kiln drying of radiata pine sapwood often results in the development of a brown stain causing substantial loss in revenues in New Zealand's high-value export markets. In this study chemical pre-treatments were evaluated for their ability to control the formation of kil...
B Kreber, A McDonald


Adsorption of ACQ and CuMEA Wood Preservatives in Red pine
2005 - IRG/WP 05-30374
The rates of stabilization or fixation of ACQ subcomponents (CuO, DDAC and MEA) in red pine (Pinus resinosa) were compared for different solution concentrations (0.75%, 1.5%, 2.25% and 3% ACQ-D) and post treatment conditioning temperatures. Preservative solutions were impregnated into red pine sapwood by a full-cell treatment. Copper and MEA adsorptions from copper monoethanolamine solutions witho...
C Tascioglu, P A Cooper, Y T Ung


The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King


Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang


Feasibility of using biological control agents to arrest and prevent colonization of Douglas fir and southern pine by decay fungi
1988 - IRG/WP 1345
The use of microfungi to control basidiomycetous decay has been evaluated in Europe for many years, where it has produced mixed results against Lentinus lepideus Fries, the fungus presumed to be the major cause of decay in Scots Pine poles. In the United States, remedial decay control has been largely chemical, with little use of alternative decay control strategies. Increasing restrictions on che...
J J Morrell, C M Sexton


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


Ponding of radiata pine (Pinus radiata) - 1. The effect of bacteria on wood
1998 - IRG/WP 98-10265
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks were examined by light microscopy, confocal laser scanning microscopy (CLSM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) for bacterial colonisation of wood and degradation of pit membranes. After 2 weeks of ponding bacteria colonised the outer few cells of wood, ...
A P Singh, Y S Kim, U Schmitt, B S Dawson


Long term experiments for assessing the diffusion of boric acid and diluorides from local preservative pills in spruce and pine
1996 - IRG/WP 96-40065
For the experimental assessment of the diffusion of boric acid and difluorides over a three year period 2 tests were set up. In a test with large spruce blocks (150 x 150 x 300 mm³) 3 different pill types were exposed to 3 different climates: climate room (20°C, 65% r.h.), wet room (20°C, 95% r.h.), and to outside exposure. In a test with open L-joints without paint, with an alkyd paint and wit...
W J Homan, H Militz


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


Detection of brown-rot antigens in southern pine
1996 - IRG/WP 96-20090
Brown rot fungal antigens were detected by particle capture immunoassay (PCI) in southern pine 2 x 4's beyond visible or culturable hyphal growth. Further analysis of test samples revealed changes along the 2 x 4's that could be grouped into zones. Zone 1, the point of inoculation through 6 cm, showed low pH, measurable oxalic acid, high moisture, and high protein. Zone 2, throug...
C A Clausen


The influence of fungi causing blue – stain on absorptiveness of Scotch pine wood
2005 - IRG/WP 05-10565
The blue-stain fungi cause discoloration of the wood. In the course of their development in wood may have an effect on wood structures and properties influenced on its use value. Investigation has been undertaken to clear the influence of blue-stain fungi on wood absorptiveness as indicators for the wood ability to impregnation with water diluted wood preservatives. The wet sapwood samples of fres...
A Fojutowski


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Effect of humic acid on leaching of CCA from treated wood
2000 - IRG/WP 00-50151
Laboratory studies indicate that relatively high concentrations (1.000 - 10.000 ppm) of humic acids can increase the leaching of chromium and copper from CCA-C treated wood, and that copper is most affected. They also show that leaching with natural water samples can result in higher leaching of all components than leaching with distilled water. Evaluation of CCA component retentions and mass bala...
P A Cooper, D Jeremic, J L Taylor, Y T Ung


Trials of new treatments for prevention of kiln brownstain of white pine (Pinus strobus)
1995 - IRG/WP 95-30068
White pine (Pinus strobus) often develops a surface brown oxidative stain when kiln dried. Such stain downgrades high quality lumber and is most likely to occur when fresh, unseasoned lumber is stacked during warm weather prior to kiln drying. Use of reducing agents or pH alteration has been successful, but may have some practical limitations for general use. This study attempted to prevent browns...
E L Schmidt, E Christopherson, T L Highley, M H Freeman


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Mold and stain fungi associated with Radiata pine logs imported from New Zealand
2000 - IRG/WP 00-10346
The Korean sawmills have recently realized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of mold and stain fungi colonized commercially important softwood species (Pinus densifl...
Jae-Jin Kim, Gyu-Hyeok Kim


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling