IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 581 documents. Displaying 25 entries per page.


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


Effect of incising depth and density on treatment of Douglas fir, hem fir and spruce-pine-fir lumber with CCA, ACZA or ACQ
1997 - IRG/WP 97-40093
Incising markedly improves both the depth and uniformity of preservative treatment of refractory wood species, but there are few studies directly comparing the effects of incising depth and density on penetration and retention of commonly used waterborne preservatives in wood species from the western United States. The effects of two incision densities (7300 and 8900 incisions/square meter) at two...
M Anderson, J J Morrell, J E Winandy


Retention and distribution of copper/chrome/arsenic (CCA) in pressurised sap-displaced UK grown spruce and pine
1986 - IRG/WP 3366
Increment cores were taken from UK grown Scots pine (Pinus sylvestris L.), Corsican pine (Pinus nigra var. maritima Ait), Sitka Spruce (Picea sitchensis (Bong) Carr), and Norway spruce (Picea abies (L) Karst) distribution poles treated by pressurised sap-displacement using a 1.8% copper, chrome, arsenic (CCA) solution. Each increment core was sectioned radially and the copper, chrome, and arsenic ...
P D Evans, G M Smith, B King


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Effects of Trichoderma harzianum on enzyme activity and oxalic acid production of Gloeophyllum trabeum in ponderosa pine sapwood blocks
1992 - IRG/WP 92-1550
The effect of a bioprotectant, Trichoderma harzianum, on the activity of Gloeophyllum trabeum was investigated using a wood wafer sandwich method. Wood weight loss was greatest with Gloeophyllum trabeum exposed wafers, intermediate with those exposed to both the bioprotectant and decay fungus, and lowest with the bioprotectant exposed wafers. Extracts of wood wafers after 2, 4, or 6 weeks of funga...
C M Sexton, J J Morrell


Chemical Analysis of Southern Pine Pole Stubs Thirty-Nine Months Following Treatment with Three Methylisothiocyanate-Based Fumigants
2004 - IRG/WP 04-30349
Agricultural fumigants have been commercially used in the United States for over 20 years to control internal decay in utility poles and other wooden structures. Of the four fumigants which are currently used in the remedial treatment of utility poles, three are based on methylisothiocyanate (MITC) as being the principal fungitoxic component. Two of these MITC-based fumigants, liquid metham sodi...
R J Ziobro, J Fomenko, D J Herdman, J Guzzetta, T Pope


Movement and persistence of Dazomet and pellected methylisothiocyanate in wrapped Douglas fir and southern pine timbers
1991 - IRG/WP 1496
The movement and persistence of Dazomet (tetrahydro-3,5-dimethyl-2 H-1,3,5 thiadiazine-6-thione) and pelleted methylisothiocyanate (MIT) was evaluated in wrapped Douglas-fir and Southern Pine timbers. MIT pellets did not impart a fungistatic effect to any of the timbers. Failure of MIT was probably due to loss of MIT from pellets prior to application. Fungistatic effect of Dazomet was consistently...
T L Highley


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Bending properties of TCMTB-treated Southern pine sapwood using supercritical carbon dioxide impregnation process
1997 - IRG/WP 97-40080
The effects of elevated pressure and treatment with thiocyanomethylthiobenzothiazole (TCMTB) on the bending properties of Southern pine sapwood were evaluated at pressures ranging from 1,800 to 3,600 psi. All bending properties were affected to some extent by supercritical fluid treatment. Modulus of elasticity and work to maximum load were not significantly affected by pressure levels. Modulus of...
Gyu-Hyeok Kim, S Kumar, E S Demessie, K L Levien, J J Morrell


Soft rot studies on CCA treated eucalypt power transmission poles
1981 - IRG/WP 1132
Initial results found for sixty CCA treated eucalypt poles, from a soft-rot survey are discussed. Retentions of CCA within above and below ground pole samples were variable. The variation was attributed mostly to biodegradation and effect of soil environment, rather than leaching. Bacterial decay was found in many poles and was severe in some cases. Although found in the presence of soft-rot decay...
L E Leightley


Comparative moisture uptake of Douglas fir and radiata pine structural lumber when exposed to rain wetting as an indicator of relative decay resistance
2004 - IRG/WP 04-20285
Trials were undertaken to determine the relative resistance of radiata pine and Douglas-fir to wetting when exposed to the weather. Douglas-fir samples were obtained from one Central North Island and three South Island sources and had a heartwood/sapwood mix typical for each resource. Radiata pine sapwood and heartwood samples were obtained from a Central North Island source. Material was exposed...
M E Hedley, G Durbin, L Wichmann-Hansen, L Knowles


Efficacy of linear chain carboxylic acid anhydrides as wood protection chemicals
2002 - IRG/WP 02-30295
This paper presents an assessment of the effectiveness of linear chain carboxylic acid anhydrides namely, acetic, propionic, butyric, valeric and hexanoic anhydride, in improving the decay resistance of Corsican pine (Pinus nigra Schneid) sapwood. Wood-anhydride bond formation was verified by the increase in sample weight and volume. A brown rot fungus [Coniophora puteana (Schum.:Fr)] was selec...
A N Papadopoulos, M D C Hale, C A S Hill


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


The effect of wick action on the moisture distribution in heartwood and sapwood stakes of Pinus radiata D. Don.
1999 - IRG/WP 99-40139
The pattern of moisture distribution in stakes of Pinus radiata D. Don. subjected to "wick action" is investigated. There was incomplete saturation of the stakes even after 93 days of continual soaking. Maximum moisture absorption occurred at the base of the stake and at the air/water interface of the stake. Incomplete saturation of the stake was thought to be due to air embolism within the wood. ...
J Hann, P Vinden


Diffusion of a copper naphthenate/boron paste through Douglas fir heartwood
1991 - IRG/WP 3671
Groundline wraps are an important portion of the remedial treatment strategies for protecting utility poles in North America from surface decay. The compositions of these wraps have recently shifted away from pentachlorophenol and creosote to formulations containing copper naphthenate and boron. These formulations have not yet been extensively tested, although the chemicals have been used for many...
P G Forsyth, J J Morrell


Serviceability of copper naphthenate-treated poles
2000 - IRG/WP 00-30214
Copper naphthenate-treated poles in service were inspected for deterioration, penetration, retention, and serviceability. The study to date has included poles in all hazard zones in the United States. Poles installed by 12 different utilities and eight different treating companies are included in the survey. Both southern pine and Douglas-fir poles and distribution and transmission poles are inclu...
H M Barnes, M H Freeman, J A Brient, C N Kerr Jr


The influence of wood moisture content on the fungitoxicity of methylisothiocyanate in Douglas fir heartwood
1987 - IRG/WP 3430
The fumigant methylisothiocyanate (MIT) effectively controls decay fungi in large wood structures, but the influence of environmental factors on its performance are not well understood. Experiments found wood moisture content to greatly influence the fungitoxicity and sorption of MIT in Douglas fir heartwood. At constant, low MIT vapor concentrations (less than 1 µg/cc air), wood at 10% MC bound ...
A R Zahora, J J Morrell


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


An evaluation of chemical treatments for the protection of radiata pine logs from fungal degrade
1986 - IRG/WP 3377
Busan 30, Busan 1009, Mitrol PQ375. and sodium pentachlorophenoxide (NaPCP) plus have been evaluated as antisapstain treatments for the long-term protection of debarked radiata pine logs. After 3 months' winter-spring storage, treated debarked logs had less surface and internal sapstain than 'control' logs. After 6 months' storage all logs had internal sapstain ...
J A Drysdale, M E Hedley, J A Butcher


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


Previous Page | Next Page