The Study of the Preparation of Overlaid MDF with the Flame Retardant Impregnated Paper
2018 - IRG/WP 18-40848
The preparation of overlaid medium density fiberboard (MDF) was studied. The flame retardant impregnated papers (FRIP) were overlaid on the surface of the MDF for the fire protection. The results showed that: 1) The production of the FRIP was based on the technology of melamine-impregnated paper, which required the viscosity of the impregnated resin lower than 20s. However, with the addition of th...
W Qu, M Wu, Y-Z Wu


Effect of long-term immersion in fresh and salt water on mould growth on Scots pine (Pinus Sylvestris L.) wood
2020 - IRG/WP 20-10962
Wood exposed outdoors will eventually be degraded by fungi, depending on exposure and material characteristics. Numerous wooden constructions in the Røros municipality have existed since the 17th century, but wood used in recent repairs have decayed faster than expected. Before 1970 timber was mainly transported by log driving or rafting, and the logs were immersed in water for longer or shorter ...
M Sand Austigard, J Mattsson


Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Post-layup protection of mass timber elements in above ground protected exposures: 2-year results
2022 - IRG/WP 22-30766
Mass timber has seen increased use as a building material for low and mid-rise construction in recent decades. The durability of mass timber elements has not been fully examined and the effects of wood destroying organisms on this these materials merits attention. The effectiveness of currently labeled soil termiticides and passively applied biocides at post-construction or as remedial agents need...
M E Mankowski, T G Shelton, G T Kirker, J J Morrell


Investigating the fire properties of a composite material made of MDF-residues, citric acid and sorbitol
2023 - IRG/WP 23-40969
In times of climate change and a shortage of energy and raw materials, it has become apparent, that material reuse of wood in a cascade system can reduce the ecological impact of a material and be cost effective. A new composite material has been developed made from citric acid, sorbitol, water and waste MDF. Not only will there be a material reuse option for waste MDF but due to the small particl...
P T Lewandowski, W Perdoch, E Larnoy, H Militz


Fungicidal properties of black liquor from the waste MDF board digestion in terms of wood protection
2023 - IRG/WP 23-50379
The aim of the work was to determine the fungicidal properties of black liquor as a product of the chemical digestion of waste MDF board. The resistance of wood treated with black liquor from MDF waste pulping process was compared with the resistance of wood treated with black liquor from the pulping process of a by-product from agricultural production. The control material consisted of non-treate...
B Mazela, W Perdoch, A Szulc, I Sieminska


Effectivity of zinc borate in medium density fiberboard (MDF) for ground proximity testing
2024 - IRG/WP 24-20723
Medium-density fiberboard (MDF) is one of the most used and versatile wood composites. Most of its use has been focused on interior applications. Adhesives such as p-MDI (polymeric methyl diphenyl diisocyanate) provide MDF with a better performance against moisture, but resistance against decay is also required for outdoor use. A mix of wood fibers, p-MDI, and 0.75%-1.5% of ZB was made to produce ...
S M Vega Gutierrez, T Olivadoti


Bio-based thermal insulation panels – a way of cascading utilization of post-consumer wood
2024 - IRG/WP 24-50388
Cascading wood utilization is critical to fulfilling a circular economy frame in the wood industry. The work's aim was to apply wood dust from plywood production to the production of innovative bio-based thermal insulation panels. Trametes hirsute fungus was used as a composite binder, and then a composite structure and thermal insulation properties, water absorbability, and strength properties of...
W Perdoch, A Szelag