Surface color and roughness characteristics of medium density fiberboard (MDF) panels treated with fire retardants
2008 - IRG/WP 08-40420
The objective of this study was to determine surface characteristics and color change properties of Medium Density Fiberboard (MDF) treated by fire retardants (FR) with 10% concentration. Experimental panels were made using by melamine ureaformaldehyde (MUF) adhesive having 10%, 15%, 20% of melamine. The surface properties of the samples were determined using a fine stylus technique. Three roughn...
D Ustaömer, M Usta, S Hiziroglu


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


The Effects of Solar Radiation on the Fungal Colonization and Color of Weathered Wood
2008 - IRG/WP 08-10676
Solar radiation rapidly depolymerizes lignin at wood surfaces exposed outdoors producing a suite of low molecular weight aromatic compounds within weathered wood. Fungi colonizing weathered wood are able to metabolize these aromatic compounds, and many of them also contain high levels of melanin to protect themselves from the harmful effects of UV radiation. Both of these adaptations suggest that ...
V Hernandez, C Breuil, P D Evans


Improving the Dimensional Stability and Fire Resistance of OSB by Roller-Coating Panels with UV-Curable Finishes
2008 - IRG/WP 08-40434
Oriented strandboard was sanded and roller-coated with UV-cured finishes. The effects of these treatments on the surface roughness, dimensional stability and fire resistance of OSB were assessed. Sanding reduced the average roughness of OSB, but it had a smaller effect on maximum roughness because sanded boards still contained surface voids between some strands. Sanded boards absorbed less than ha...
P D Evans, I Cullis


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Differential response of wood to dry air thermal treatment (DATT) and soy oil thermal treatment (SOTT)
2009 - IRG/WP 09-40446
Thermal treatment is an alternative to chemical modification method which has been used to some extent in improving timber quality. In order to get the maximum benefits possible without compromising the various end-use quality requirements of timber, several possibilities have been and are still being investigated in relation to this technique. Clear wood samples (19 x 19 x 150mm) of kiln-dried re...
L Awoyemi


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


The natural durability and preservative treatability of 11 bamboo species
2010 - IRG/WP 10-10708
Tests on the natural durability and preservative treatability of 11 common bamboo species were conducted. The results showed that there was a linear relation between bamboo density and its preservative retention by mass, and the preservative retention of bamboo reduced while its density increased. The test also showed that there were significant differences in the natural durability of bamboos, bu...
Chen Lifang, Su Haitao, Zhang Yanjun, Wang Yuxia, He Xuexiang, Ma Hongxia, Xie Guijun


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Chapter 10 - Preservation of muli bamboo
2007 - IRG/WP 07-10635-10
Environmentally and economically very important mulibamboo (Melocanna baccifera) grown in Bangladesh was fond to be easily pressure treatable with CCA-C at green and air dry conditions. The green and air-dried bamboo treated at same treating conditions and concentration showed 110 per cent (2.10-times) higher retention in air-dried bamboo than green one. Adequate lower retention equivalent t...
A K Lahiry


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Chapter 14 - Accelerated fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-14
Chromated copper arsenate type C (CCA-C) fixation study on impregnated (with adequate w/v 6% CCA solution) then boiled, oven-dried, normal, air-dried and steamed bamboo slices of airdried borakbamboo (Bambusa balcooa Roxb.) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to low fixati...
A K Lahiry


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl