Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Preparation and characterization of activated carbon fibers prepared from liquefied wood
2013 - IRG/WP 13-40636
Activated carbon fibers were prepared from liquefied wood through stream activation. The effects of activation temperature and time on the microstructure and surface functional groups of the liquefied wood activated carbon fibers (LWACFs) were studied using analysis of burning behavior, X-ray diffraction, nitrogen adsorption-desorption isotherms, X-ray photoelectron spectroscopy, and SEM. The resu...
Wenjing Liu, Guangjie Zhao


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Visualization of gold/silver nanostars in wood by surface enhanced Raman spectroscopy
2014 - IRG/WP 14-30653
Nanotechnology is a fast growing up-to-date technology and ventures expeditiously in the wood preservative market. However, there is still a huge lack of understanding about the interaction and incorporation of nanoparticles (NSs) in wood. Surface-enhanced Raman scattering (SERS) offers unique advantages as an analytical tool with a high selectivity and sensitivity without matrix interference. Her...
C Geers, L Rodríguez-Lorenzo, M Placencia Peña, P Brodard, T Volkmer, B Rothen-Rutishauser, A Petri-Fink


VOC-free remedial treatment agent on organic solvent basis with surface cleaning by photocatalysis using titanium dioxide
2014 - IRG/WP 14-40651
Due to the EU Regulations according to the harmonisation of the European market of biocidal products and the EU Regulations regarding emissions of volatile organic compounds in residential properties a new VOC free yet organic solvent based remedial treatment agent is introduced including a potential method to clean up the wooden surface of remaining biocides after a remedial treatment using photo...
H Ahl, J Fromm, P Jüngel, E Melcher, M Pallaske


The effect of UV irradiation on some technological properties of different polyurethane varnishes coated plywood panels from veneers dried at different temperatures
2014 - IRG/WP 14-40661
In this study, the effect of UV irradiation on some technological properties of three different polyurethane varnishes coated plywood panels produced from Scots pine (Pinus sylvestris L.) and Maritime pine (Pinus pinaster L.) veneers manuactured and dried at different temperatures was studied. Accordingly, 32°C log peeling temperature and three different veneer drying temperatures (110, 140 and ...
Ö Özgenç, C Demirkir, Ü C Yildiz, G Çolakoğlu


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


Termiticide Residues in Building Foundation Aggregate Fills After Trench and Surface Applications
2015 - IRG/WP 15-30679
Termiticide concentrations (ppm) in aggregate fill were determined by measuring active ingredient (a.i.) residues of two pyrethroid termiticides, Up-Cyde Pro® 2EC-cypermethrin, and BaseLine® EC-bifenthrin, at 24.0 hours, and then at 6.0- and 12.0-months after ‘horizontal’ surface applications, perimeter ‘trenching and rodding’ applications, or ‘rodding only’ trench applications at lo...
B M Kard, C E Koneman, K T Shelton, C C Luper, R A Grantham


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Formation of hydrophobic wood surface by means of thermal treatment and surface modification with alkyl ketene dimer (AKD)
2016 - IRG/WP 16-40738
One of the major shortcomings of wood-based materials compared to technical materials is attributed to their poor dimensional stability in changing climates and in contact with liquid water. Heat treatment induces chemical change with a consequent decreasing of reactivity of the material showing unwanted surface inactivation. Alkyl ketene dimer (AKD) is a widely used sizing agent in papermaking, w...
T Lovaglio, T Meints, L Todaro, W Gindl-Altmutter


The influence of log soaking temperature and thermal modification on the properties of birch veneers
2016 - IRG/WP 16-40749
In veneer manufacture the logs are routinely soaked in heated water baths in order to soften the wood prior to peeling. The temperature of the water may vary greatly between batches; however, the influence of log soaking temperature on veneer properties has had little research attention. Uncontrolled moisture is known to cause problems in wood-based materials, while thermal modification offers a m...
S Källbom, K Laine, M S Moghaddam, A Rohumaa, K Segerholm, M Wålinder


Evaluation of surface cracks on wood – physical assessment versus subjective sensation
2017 - IRG/WP 17-20617
In the presented studies from the University of Goettingen (Study I) and the University of Hannover (Study II), the assessment of cracks with different methods and their acceptance in general as well as depending on different target groups are investigated. The aim was to determine which factors are relevant for a crack evaluation and which visual impression of a wooden surface is tolerable for co...
A Gellerich, C Brischke, L Emmerich, L Meyer-Veltrup, P Kaudewitz


Surface Protection of Wood with Metal Acetylacetonates
2017 - IRG/WP 17-40802
Metal acetylacetonates are coordination complexes of metal ions and the acetylacetonate anion. They have diverse uses as catalysts, cross-linking and curing agents and adhesion promotors. Some metal acetylacetonates can photostabilise polymers whereas others are photocatalysts. We hypothesise that the ability of metal acetylacetonates to photostabilise wood will vary depending on the metal in the ...
Yuner Zhu, P D Evans


Aesthetic changes of coated thermally modified wood after artificial weathering
2017 - IRG/WP 17-40819
The thermal modification process affects the chemical configuration of the wood matrix improving some physical properties and durability. In addition, the distinctive dark tones of thermally modified timber increase the economic value of several light-coloured species. However, heat-treatment alters the substrates and it could influence in the application of coating products, necessaries to mainta...
R Herrera, J Sandak, E Robles, J Labidi


Wood Hydrophobic Modification by Mixed Wax Emulsions
2018 - IRG/WP 18-40839
An environmental-friendly, economical and facile method to construct hydrophobic system for improving wood repellency was applied in this study. Using paraffin wax and carnauba mixed wax O/W emulsions can simultaneously fabricate continuous wax films and rough structures in wood internal and external surface under appropriate heat treatment. In the study, single and mixed wax emulsions of 4% solid...
C Chen, W Wang


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees


Application of diverse hyperspectral imaging systems for evaluation of heritage objects
2020 - IRG/WP 20-10971
Advanced imaging techniques are able to non-invasively characterize, monitor and evaluate the impact of conservation treatments on cultural heritage (CH) objects. In this specific field, hyperspectral imaging (HI) allows non-destructive characterization of materials by identifying and characterizing colouring agents, binders and protective coatings as constituents of an object’s original constru...
J Sandak, A Sandak, L Legan, K Retko, M Kavčič, J Kosel, F Poohphajai, R Herrera Diaz, V Ponnuchamy, N Sajinčič, Č Tavzes, P Ropret


Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi