A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


Lindane and permethrin tolerances of different strains of Lyctus brunneus Steph
1986 - IRG/WP 1278
The question about the reproducibility of test data from contact insecticide tests with Lyctus brunneus has been asked within the IRG. Three laboratories decided to interchange their insects and to carry out a comparative test according to the EMPA screening method. In order to get enough animals for the test the three strains had to be grown during three generations in each of the laboratories. D...
E Graf, B Lanz


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Termite resistance of borate-treated lumber in a three-year above-ground field test in Hawaii
2000 - IRG/WP 00-30236
A protected above-ground field test simulating the sill plate (dodai) used in conventional Japanese housing construction was established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg/m3) and ammoniacal copper zinc arsenate (ACZA, 4 kg/m3) were included in the t...
J K Grace, R J Oshiro, A Byrne, P I Morris, K Tsunoda


Borate Protection and Termites: Variation in Protection Thresholds Explained
2006 - IRG/WP 06-20324
Laboratory and field data reported in the literature are confusing with regard to ‘adequate’ protection thresholds for borate timber preservatives against subterranean termites. The confusion is compounded by differences in termite species, timber species and test methodology. Laboratory data indicate a borate retention of 0.5% mass/mass (m/m) boric acid equivalent (BAE) would cause > 90% t...
B C Peters, C J Fitzgerald


The “wire-loop slicing technique” for the rapid field collection of large numbers of Coptotermes acinaciformis termites from above-ground mound colonies
2006 - IRG/WP 06-10583
This technique of rapidly slicing through an above-ground C. acinaciformis mound colony with a steel wire-loop attached to a vehicle allows the collection of large numbers of termites. The sliced mound topples onto a tarpaulin arranged on the ground, the outer wall layers break away in large segments, and the carton materials incorporating the termites are readily collected and transferred to larg...
B M Ahmed, J R J French


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Predicting the decay resistance of timber above-ground: 1. Climate effects
2006 - IRG/WP 06-20330
Despite the benefits of using timber as a building product, it is disadvantaged by current Australian Standard durability classifications which lack the sensitivity desired by engineers and architects. To address the need for more sensitive timber service-life information in Australia, an above-ground durability research program was established in 1987. One focus of research is the relationship be...
L P Francis, J Norton


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


Performance of borate-treated lumber after 8 years in an above-ground termite field test in Hawaii
2006 - IRG/WP 06-30390
We report eight years of field study results from a protected above-ground field test in Hawaii simulating the sill plate (dodai) used in conventional Japanese housing construction. Field tests were established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% BAE shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg...
J K Grace, A Byrne, P I Morris, K Tsunoda


Performance of borate-treated lumber in a protected, above-ground field test in Japan
2006 - IRG/WP 06-30395
This document is supplemental to the previous IRG document (Tsunoda et al. 2004). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Research Institute for Sustainable Humanosphere of Kyoto University in Kagoshima Pref., Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and R...
K Tsunoda, A Byrne, P I Morris, J K Grace


Above and Below-Ground Depletion of Copper, Chromium and Arsenic from Pinus radiata and Fagus sylvatica at Thirteen Test Sites in New Zealand and Australia
2006 - IRG/WP 06-30402
The objective was to determine the significance of site and wood species on preservative depletion for a copper chrome arsenate preservative (CCA) from 20 x 20 x 500 mm field test stakes after 5.5 and 4.5 years for pine and beech respectively. At least 5 sacrificial stakes were used to produce site means. Site and wood species had a major effect on copper, chromium and arsenic loss from CCA treate...
R Wakeling


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


Decay Hazard Classifications in China for Exterior Above-Ground Wood
2007 - IRG/WP 07-20357
A decay hazard map for exterior above-ground wood structures is presented based on Scheffer’s Climate Index, with the major purpose of promoting awareness for proper protection of wood structures in different locations in China. A very large area in the South, including southern Yunnan, most of Sichuan Province and Chongqing, and part of Hunan, Hubei, Anhui, Jiangxi, and Zhejiang, as well as all...
J Wang, X Wu, M Jiang, P I Morris


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Predicting the decay resistance of timber above-ground: 2. When can reliable field data be obtained?
2007 - IRG/WP 07-20368
Application of modern performance-based engineering and design requires building products that are thoroughly characterised in terms of their ability to perform as expected over time. The engineering community is attempting to use this information to provide predicted service-lives for various building elements. Increasingly, this service-life prediction must be based on objective measurement coup...
L P Francis, A J Swain, J J Morrell


Corrosion of metal fasteners in contact with copper preservative treated wood
2007 - IRG/WP 07-20370
The corrosion rates of metal fasteners in contact with alkaline copper quat (ACQ) treated wood with or without commercially available water repellent was compared to that of cedar. In this experiment, fasteners were sandwiched between two pieces of treated wood and exposed to a humid environment at a slightly elevated temperature. The use of a “sandwich” design allowed periodic examination of ...
BaekYong Choi, J N R Ruddick


Expected service life of outdoor wooden structures such as guard fences and noise barriers indicated by questionnaire survey
2007 - IRG/WP 07-20372
Forestry Agency, Japan has intended to expand the utilization of domestic wood in many areas such as not only housing constructions also outdoor structures. In order to respond the policy, actual durability and service life of these structures should be clarified, and the guide line for archiving planned service life also should be established. Japan Wood Preservers Industries Association carried ...
K Yamamoto, A Makita, A Yamaguchi, T Shiraishi, K Maeda, D Tezuka, S Katsumata, M Higaki


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


Previous Page | Next Page