A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Tests on the effectiveness of concentrated borate wood preservative
2009 - IRG/WP 09-30500
Tests were carried out to examine the toxicity of concentrated borate wood preservative to termites, fungi and mammals. The results showed that the preservative treated timber had high resistance to termite or decay and its acute oral toxicity belonged to low grade. The research shows that concentrated borate solution is an environmentally sound preservative and can be used in non-pressure treatin...
Su Haitao, Zhang Yanjun, Xie Guijun, Chen Lifang, He Xuexiang


Albumin borate: A new non-toxic, wide-spectrum, long-term wood preservative
1998 - IRG/WP 98-30167
Boron, widely recognized for its broad range of activity towards both fungi and insects and for its low mammalian toxicity, can not provide long term protection to treated timber due to its high leachability. Boron, in the form of boric acid, can be partially fixed to timber by the formation of an association with egg albumin, which is insolubilized by heat-induced coagulation. Chemical investiga...
M-F Thévenon, A Pizzi, J-P Haluk


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


European laboratory termite testing
1986 - IRG/WP 1299
As with all testing of wood preservatives the evaluation of the resistance to termites of treated wood requires methodology which is approriate to, and can be readily extrapolated to, the practical situation. Thus not only must the variations in possible treatment systems be taken into account (eg dip, brush or pressure application) so too must the range of termite species and the type of exposure...
R W Berry


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


Fungus cellar and field tests with tall oil derivatives. Final report after 11 years' testing
1993 - IRG/WP 93-30007
Two derivatives of tall oil were tested as wood preservatives in a fungus cellar and in ground contact (field test). Stakes of Pinus sylvestris sapwood were used in the tests. For the field test the size of the stakes was 20 x 50 x 500 mm³ and for the fungus cellar test 20 x 20 x 250 mm³. The stakes were vacuum-pressure treated with the two products and exposed in 1981. The field test site used ...
J Jermer, Ö Bergman, T Nilsson


Comparison between agar-block and soil-block methods for wood-destroying Basidiomycetes
1992 - IRG/WP 92-2401
The object of this work is to compare these methods in order to provide some information to help in the choice between them. The comparison was made by a statistical analysis (factorial completely randomized design) and by a discussion about other aspects of each method. An evaluation of some fungi on attacking wood and a comparison between Picnoporus sanguineus isolated from carpophore and decaye...
M B B Monteiro, S Brazolin, G Catanozi


Performance of copper-based wood preservatives in above ground and ground contact tests
1994 - IRG/WP 94-30057
The relative performance of a range of copper-based wood preservatives was compared using above ground and ground contact procedures. The data, accumulated after several years' testing, show that on an equivalent active ingredient basis, differences in performance of the preservative systems tested can vary quite markedly. The contribution of co-biocides to the overall performance of thes...
A F Preston, K J Archer, L Jin, W Metzner, D Seepe


The case for non-chemical termite barriers in termite control
1989 - IRG/WP 1381
A brief outline of current non-chemical barriers in subterranean termite control and their use in Australia is presented. Recent use of non-chemical barriers in Hawaii has led to their evaluation in termite control here and elsewhere. In Australia, preliminary laboratory and field experiments have shown similar results to those found against Coptotermes formosanus in Hawaii, namely, Australian Cop...
J R J French


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


Microscopical analysis of formaldehyde-acid modified wood
1981 - IRG/WP 3182
Cross-linking of wood with gaseous formaldehyde improves its hygroscopic and dimensional behaviour, and its resistance against micro-organisms. However, formaldehyde cross-linking reactions take place only in the presence of an acid catalyst, which results in losses in mechanical By optimization of a formaldehyde-sulfur dioxide vapour phase process the reaction conditions were established to limit...
M Stevens, N Parameswaran


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny


A termite field test with diffusion treated lumber
1991 - IRG/WP 3648
Douglas fir lumber, diffusion treated with concentrated sodium octaborate solutions, was tested against Coptotermes formosanus in an above ground field test wherein the samples were not exposed to a direct leaching hazard during the test period. After 2.5 years exposure, the untreated control samples were almost completely destroyed while poorly treated controls pressure treated with chromated cop...
K J Archer, D A Fowlie, A F Preston, P J Walcheski


Collaborative soft rot tests: Paper for discussion in Working Group II
1970 - IRG/WP II 5A
An account of the major part of the collaborative work on laboratory tests of toxicity of preservatives to soft rot fungi initiated by the European Homologation Committee at Delft in 1966 has been published in ‘Material und Organismen’ (1970) as a report of progress. The main objective of these collaborative tests, namely to establish a reliable and acceptable standard test method was not acco...
J G Savory, A F Bravery


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


The effectiveness of deltamethrin against subterranean termites (final report)
1993 - IRG/WP 93-30011
Two series of block tests of Pinus sp were treated by dipping them for 1 (one) minute in a solution with 0.015 (w/w) and 0.05 (w/w) of deltamethrin, respectively. In both cases, an average retention of 47 kg/m³ (0.32 l/m) was reached. One part of the block tests remained under laboratory conditions during 9 months, and the other was stored during equal period of time in a theater basement submitt...
P A Zanotto


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...