Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Durability testing of coconut shell according to ENV 807
2011 - IRG/WP 11-10761
Coconut shell was tested in the laboratory according to the European standard ENV 807 with three different soil types: compost soil, brown rot/soft rot rich soil and white rot/soft rot rich soil. Mass losses between 14 and 16 % were achieved with all three soils, indicating that the decay type is of little importance in the degradation process. Somewhat higher mass losses, 19-22 % were obtained fo...
J Jermer, A H H Wong, K Segerholm, T Nilsson


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


The durability of acetylated radiata pine sapwood (Accoya). Results from five years testing
2011 - IRG/WP 11-30560
New Zealand grown radiata pine sapwood was modified using the Accsys PLC acetylation process (Accoya). Following treatment, various test samples were exposed in the Scion Accelerated Field Test facility (Fungus Cellar) and in exterior ground contact field tests. In the Fungus Cellar, performance was compared with that of radiata pine treated with CCA to Hazard Classes H3.2 (0.37% m/m Cu+Cr+As) and...
M Hedley, D Page, J van der Waals, K Nasheri, G Durbin


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Study of properties and application of Paulownia in wood industries
2011 - IRG/WP 11-40560
Important of required raw material supply regarding constraint in harvesting, increasingly population, change in consumption pattern and increasingly focus on wood products and per capita in consumption is obvious for anyone. Paulownia is a marvelous tree species with its characteristics of fast-growing, good Wood quality, multiple uses, wide-ranged distribution, easy propagation, deep root system...
M Akhtari


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Extractives in Norwegian-Grown and North American-Grown Western Redcedar and Their Relation to Durability
2012 - IRG/WP 12-10762
The extractives responsible for the natural durability of western redcedar (WRC) are not well understood. Recent work by the Norwegian Institute of Wood Technology and the Norwegian Forest and Landscape Institute has evaluated the natural durability of Norwegian wood species and reference species, including Norwegian-grown WRC and North American-grown WRC, in a series of decay tests. The availabil...
R Stirling, P O Flæte, G Alfredsen, P I Morris


Above Ground Field Evaluation and GC-MS Analysis of Naturally Durable Wood Species
2012 - IRG/WP 12-10764
Nine wood species are being evaluated in above ground field studies in Mississippi and Wisconsin. Candidate naturally durable wood (NDW) species are being rated at yearly intervals for resistance to decay, cupping, and checking. Field ratings after 12 months exposure are presented. To date, Paulownia tomentosa (PAW) and southern yellow pine (SYP) are least durable and cedars are the most durable i...
G T Kirker, A B Blodgett, S T Lebow, C A Clausen


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...