Your search resulted in 592 documents. Displaying 25 entries per page.


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Blue stain in timber in service. Progress review of Sub-group collaborative tests - 1981/82
1982 - IRG/WP 2178
Following from the discussions after reporting Document IRG/WP/2146 at the Meeting in Sarajevo, 1981, it was decided that 1.) more precise definition was needed of the artificial weathering schedules used in the work - participants to re-check Table 8 and send further details or amendments to Dr Bravery; 2.) a further test employing a wider range of chemicals was necessary using a smaller range of...
A F Bravery, D J Dickinson


Hole delimination inside round timber via ultrasonic techniques
1990 - IRG/WP 2358
A fast and economic circular scanning method to localize and evaluate holes inside round timber is presented. This method consists in measuring transit times of the ultrasonic wave by fixing the transmitter probe in the perimeter of the sample, then moving the receiver probe every ten degrees until completion of the circle. The scanning is done with a cheap and light instrument. Tests are made wit...
G Prieto, A Fernández Cancio


Variation in field test performance of untreated and CCA-treated lesser-known Surinamese wood species
2000 - IRG/WP 00-20213
In Suriname three different field test sites have been used to verify the biological durability of CCA-treated wood and a range of wood species including lesser-known and lesser-used wood species. In total 37 tropical wood species were tested untreated and for 17 of the less durable species CCA-treatments were included as well. Although the three sites are located in the tropical region they diffe...
J Van Acker, M Stevens, L Comvalius


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Testing biological durability of wood-plastic composites
2006 - IRG/WP 06-20347
Testing biological durability is inherently different for wood-plastic composites (WPC) compared to solid timber. However there is clearly a need for more information on the durability of WPC’s, on the effect of decay on the material properties of WPC’s and on methods for assessing decay of WPC’s. For the emerging European WPC market there has been some discussions on how to work on these to...
J Van Acker


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Characteristics of treated oriented strand lumber using recycle chips
2006 - IRG/WP 06-40343
The Kyoto Protocol for preventing global warming has come into effect, and the Cabinet Council was decided on the amount of carbon dioxide exhaust to be reduced in Japan. Moreover, the recycling of demolition waste wood is mandated under the “Construction Material Recycling Law” as one of the mechanisms for Japan to form the recycling society. The law encourages the utilization of demolition w...
T Shibusawa, A Miyatake, K Yamamoto, K Hashimoto, H Sonobe


Resistance of DMDHEU-treated pine wood against termite and fungi attack in field testing according to EN 252. Results after 30 months
2006 - IRG/WP 06-40354
The aim of this study was to determine the effectiveness against decay and termite attack of pine sapwood treated with pure and modified DMDHEU in a field test according to European Standard EN 252. Some of the treatments tested were able to increase, within the period of the test reported (30 months), the resistance of the wood both to micro-organisms and termites. The curing process seems to be ...
S Schaffert, L Nunes, A Krause, H Militz


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Lyctine susceptibility testing and dealing with rarely susceptible hardwood species
2007 - IRG/WP 07-10607
This study examined the lyctine susceptibility of 16 timber species or hybrids. Several of the timbers have been placed previously in a ‘rarely susceptible’ category, but for standards and compliance purposes, such in-between ratings are not acceptable. Timber specimens were spot tested for starch content, and exposed to three species of lyctine beetles in an insectary. New criteria were devel...
L J Cookson, J Carr, N Chew, J W Creffield


Growth and succession of mould on commercial paint systems in two field sites
2007 - IRG/WP 07-30421
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. It is of major importance to find paint systems for wood which are durable and have a high resistance to mould growth. A total of 15 paint systems from 9 different manufacturers were exposed on two field sites, Sørkedalen and Birkenes, ...
L Ross Gobakken, K M Jenssen


The effect of an ionic liquid of imidazolium tetrafluoroborates series on Scots pine wood properties
2007 - IRG/WP 07-40357
Ionic liquids (ILs) of imidazolium tetrafluoroborates series penetrate Scots pine wood very well and are active against wood destroying fungi. The requirement to use ILs as wood preservatives is determined by the liquid influence on the functional properties of wood. Investigations were undertaken to clarify the influence of an ionic liquid, 3-heptyloxymethyl-1-methylimidazolium tetrafluoroborate ...
A Fojutowski, R Szukala, J Pernak


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Anatomical, physical and chemical changes of Bamboo (Phyllostachys puberscence ) during weathering processes
2008 - IRG/WP 08-10650
Bamboo (Phyllostachys puberscence) culms with 1, 2, 3 year old were exposed to natural weathering condition in Gwangju, Korea for 12 months. Changes in color, surface topography, strength and chemical properties were investigated using various microscopic and instrumental techniques. After one year’s weathering, the color of bamboo became lighter but strengths of bamboo did not change significan...
Jong Sik Kim, Kwang Ho Lee, Mi Young Cha, Yoon Soo Kim


Evaluation and identification of extractives from Iranian walnut (Juglans regia L.) by GC/MS technique for protection of non-decay resistant species
2008 - IRG/WP 08-10670
The use of walnut extractives is interest as environment friendly wood preservatives in the wood preservation industry. In this study, organic solvents were used to remove extractives from Iranian walnut heartwood samples. The solvent was removed by rotoevaporation, and Identification of chemical compounds in the Walnut extractives was done by using GC/MS technique. The toxicity of various extract...
S K H Hashemi, D Parsapajouh, H Khademi Eslam


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Previous Page | Next Page