Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Chapter 7 - Treatment processes of bamboo
2010 - IRG/WP 07-10635-07
For adequate penetration and retention of preservatives in woody bamboos at green, dry, solid and sliced conditions different possible and applied treatment processes have been described along with their classifications. The treated bamboo can be used as building materials; the sufficient treatability ensures its long-term best utilization at ground contact and indoor. All the processes descr...
A K Lahiry


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


A Method for Studying Boron Redistribution and Leaching in Timber Framing
2011 - IRG/WP 11-20476
In typical New Zealand timber framed house construction, the timber framing has a vapour permeable building wrap applied to the exterior and a cladding applied over 20 mm battens. An interior lining usually of gypsum plasterboard is then fixed once the timber framing has a moisture content of < 20%. Timber framing within the building envelope is not expected to be wet in-service or exposed to a le...
J A Drysdale, N Marston, M E Hedley


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson


Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


ISPM No. 15 and the Incidence of Wood Pests: Recent Findings, Policy Changes, and Current Knowledge Gaps
2011 - IRG/WP 11-30568
Largely as a result of international trade, hundreds of species of bark- and wood-infesting insects have become established in countries outside their native range. Many of these exotic insects have caused severe economic and environmental impact to urban and forest trees in the receiving countries. Most bark- and wood-infesting insects have been transported to new countries by means of the wood...
R A Haack, E G Brockerhoff


Protective Levels of Borates in timber Foundation Piles 5 – 18 Years after In-situ Remedial Treatment in Areas with Wet Clay Ground Conditions. The Jerbor and Eurobor Protocol, Part 1.
2011 - IRG/WP 11-30571
Timber has been used as foundation piles and grillages for decades or even centuries. Since the late 1970s a method for investigate, analyze and treat building timber foundations in soft clay grounds against decay fungus with a biocide have been developed and used by the late professor Allan Jerbo. Settling of buildings in soft clay grounds is continuously monitored and if damages to the building ...
M Theorin, K-M Bandh


The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip, flood coat or spray, and rapidly penetrates to the centre of timber substrates, whether containing sapwood or heartwood. However, section ...
B M Ahmed (Shiday), J R J French


The potential of propolis and other naturally occurring products for preventing biological decay
2011 - IRG/WP 11-30575
The potential of using a range of naturally occurring plant extracts and propolis from bee hives for enhancing the durability of timber in service as well as helping with the conservation of archaeological timbers is considered in this paper. Results reported demonstrate that there is some degree of protective effect noted, suggesting a viable treatment option might be developed based on a deeper ...
D Jones, N Howard, E Suttie


Design, synthesis, characterisation and effectiveness of ‘Locked-in-Boron’ chemicals for H3.2 level of wood protection
2011 - IRG/WP 11-30577
Boratrane molecules with five-membered and six-membered molecular ring systems, and with various ring substituents were synthesised, characterised and formulated for wood treatment for accelerated laboratory bioassays using wood decay fungi as test organisms. Six-membered ring boratranes showed lower efficacy in laboratory assays than five-membered ring boratranes. One alkyl-substituted boratran...
R Franich, H Kroese, S Gallagher, S Hill, B Kelly, G Billett, R Meder, W Rae


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Optimization of the bi-oleothermal treatment process for wood preservation and fireproofing
2011 - IRG/WP 11-40566
The bi-oleothermal© process (combination of oil and heat treatment) is a well mastered alternative method for wood protection. However, the fire behavior and resistance to decay of bi-oleothermally treated wood are not good enough to ensure performance which meets the service standards for outdoor applications such as cladding or decking expected by the market. The aim of the present research pro...
F Simon, M Kutnik, M Goyer, M-F Thévenon, C Alfos, M Céron


Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...