Thickened boron treatment
1990 - IRG/WP 3632
Commercial trials with thickened boron preservatives "Diffusol™" indicate a number of advantages when compared to traditional methods of dip-boron preservative treatment. These include: (i) more even uptake and distribution of preservative on and within the timber; (ii) faster diffusion times; (iii) the treatment of gauged timber (though improved retention); (iv) saving in energy costs (heating ...
P Vinden, J A Drysdale, M Spence


Treatment of wood with boron esters
1995 - IRG/WP 95-30087
The treatment of wood and wood products with boron esters is reviewed. The physical and chemical characteristics of boron esters affecting the treatability of wood are discussed, in particular thermal decomposition and rates of hydrolysis. The uses and methods applying boron esters as wood preservatives include: (i) Solutions of boron esters for remedial and diffusible treatment of wood; (ii) soli...
J Romero, P Vinden, J A Drysdale


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


The influence of timber species and preservative treatment on spore germination of some wood-destroying Basidiomycetes
1988 - IRG/WP 2300
Basidiospores from six wood decay fungi exhibited varying germination rates on untreated softwood and hardwood blocks. Germination inhibition of all test fungi was recorded on pine sapwood. No preference for a certain timber species by a particular fungus was evident. Whereas almost complete inhibition of germination occurred on wood treated with a quarternary-ammonium based wood preservative, mos...
B M Hegarty, G Buchwald


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Boracol 40 - A potential remedial and preservative treatment for lyctids
1983 - IRG/WP 1192
The paper reports on a preliminary assessment of the efficacy of a diffusion formulation, Boracol 40, when applied as a brush treatment: to the surface of Eucalyptus obliqua against the powder-post borer Lyctus brunneus. After a five month bioassay, Boracol 40 has severely retarded the progress of active infestations of Lyctus brunneus and has been 100 per cent effective as a preventative treatmen...
J W Creffield, H Greaves, C D Howick


CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


Non-pressure preservation technique of five less durable timber species – Kadam (Anthocephalus cadamba), Shimul (Bombax ceiba), Pithalu (Trewia nudiflora), Am (Mangifera indica) and Boroi (Ziziphus jujube) of Bangladesh
2006 - IRG/WP 06-40322
Wood is a versatile renewable resource, which has been extensively used as a reliable construction material as well in furniture ever since the beginning of civilization. The Major disadvantage of wood is its susceptibility to biodeterioration by fungi, insects and bacteria. In tropical countries like Bangladesh, fungi is the most significant of these biodeterioration agents. Kadam (Anthocephalus...
G N M Ilias, A H Kabir, F Begum, M F Alam


Electrokinetic Accelerated Ingress of Boron After Surface Treatment of Wood
2007 - IRG/WP 07-40372
In this work electrokinetic acceleration of boron penetration after surface treatment is proposed in order to offer an alternative to the often low penetration rates based on diffusion. Electrodialytic experiments showed that boric acid could be transported as negatively charged complexes with tartaric acid in aqueous solutions at pH 4-5. Boric acid could not be transported when tartaric acid was ...
I V Christensen


Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury


Developments in Borate Treatment of Canadian Species for Decay and Termite Resistance
2007 - IRG/WP 07-30443
The increased interest in boron treatment of wood over the past 20 years is mainly due to its environmental acceptability, potentially deep penetration in wood, and its efficacy against decay and termites. Based on Forintek’s research in the past two decades, the boron penetration and retention requirements for decay and termite protection in various national and international standards for Cana...
Jieying Wang, P Morris, S McFarling, T Byrne


Development of boron/linseed oil combined treatment as a low-toxic wood protection. Evaluation of boron fixation and resistance to termites according to Japanese and European standards
2007 - IRG/WP 07-30448
Combinations of boric acid as a first step of treatment and linseed oil as a second step have been performed in order to enhance boron retention to leaching and wood resistance to termites. Classic leaching and termites resistance standards are inappropriate to evaluate this combination which can be considered as both a wood core preservation treatment and a coating. Japanese Industrial Standard...
F Lyon, M-F Thevenon, Y Imamura, J Gril, A Pizzi


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi