Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Service life prediction of plywood
2007 - IRG/WP 07-20367
Plywood is the wood based panel showing the best physical and mechanical properties for application under moist construction conditions. Appropriate physico-mechanical durability for exterior applications in transportation or construction systems can be guaranteed by assessment of the glue bond quality and mechanical characteristics. However, due to the fact that mainly non-durable wood species ar...
J Van Acker, J De Smet


Expected service life of outdoor wooden structures such as guard fences and noise barriers indicated by questionnaire survey
2007 - IRG/WP 07-20372
Forestry Agency, Japan has intended to expand the utilization of domestic wood in many areas such as not only housing constructions also outdoor structures. In order to respond the policy, actual durability and service life of these structures should be clarified, and the guide line for archiving planned service life also should be established. Japan Wood Preservers Industries Association carried ...
K Yamamoto, A Makita, A Yamaguchi, T Shiraishi, K Maeda, D Tezuka, S Katsumata, M Higaki


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


End Coating Masson Pine Grown in South China to Prevent the Development of Blue Stain
2007 - IRG/WP 07-30428
One end (randomly selected) of logs of mason pine (Pinus massoniana) were coated with a wax-type end coating called ANCHORSEAL® immediately after tree cutting. The logs were then stored in summer weather in Guangxi, China. During the storage, at week 1, 2, 3, 4, 6, 8 and 12, five logs of mason pine were sawn into lumber or veneer for the visual observation and measurement of blue stain at the coa...
Zhao Youke, Qin Li, Huang Rongfeng, Lu Jianxiong


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


Treatment of Selected Lesser Used Timber Species against Subterranean Termites using Heartwood Extracts from Teak (Tectona grandis) and Dahoma (Piptadeniastrum africanum)
2007 - IRG/WP 07-30434
Lesser used timber species represent a valuable material for all-purpose uses but the problem is that most of them are not durable. They have, for this reason, been treated with all manner of chemicals to enhance their natural durability, especially in the tropics. Often, most of these chemicals pose a threat to the environment. Currently, one probable measure of avoiding such a threat to the envi...
A Asamoah, C Antwi-Boasiako


Tropical In-Ground Durability of CCB-treated Keruing and other Structural Sarawak Timbers after 8 – 10 Years Exposure
2007 - IRG/WP 07-30439
The heartwood of 12 mainly low-durability native timber species of Sarawak [4 Dipterocarpus (Keruing) species, Anisoptera grossivenia (Mersawa kunyit), Canarium apertum (Seladah), Dacryodes incurvata (Seladah laut), Dryobalanops oblongifolia (Kapur kelansau), Mesua macrantha (Mergasing), Podocarpus micropedunculatus (Kayu cina), Shorea compressa (Engkabang langgai), and Pterospermum javanicum (Ba...
A H H Wong, Ling Wang Choon


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


Durability of timber from exotic species against termite attack in Indian conditions
2007 - IRG/WP 07-10629
Exotic trees species, Acacia mangium Willd. and A. auriculiformis A. Cunn. ex Benth. and their hybrid are widely grown in India for multiple uses including use as timber. It is essential to know the natural durability of timbers against termites for predicting the service life of the timber and deciding on the application of preservatives to enhance the durability. Studies were conducted to test t...
O K Remadevi, R Muthukrishnan


Laser stain removal of fungus-induced stains on paper-based cultural relics
2007 - IRG/WP 07-40389
Laser techniques has been developed and applied in commercial use for 40 years, but it has not been used successfully to remove stains from paper-based cultural relics . The purpose of this study was to investigate the paper cleaning by using a technique of Nd-YAG laser. Artificial stained papers were inoculated with fungi and then were treated at different laser cleaning parameters, in order to f...
Tsang-Chyi Shiah, Han Chien Lin


Quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility
2008 - IRG/WP 08-10647
In this study, some quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility were evaluated. In experimental plots, volume of trees damaged by Dendroctonus micans (Kug.) was 34% of the volume of total standing spruce trees in the oriental spruce forests of Turkey. The volume of standing trees that D. micans damaged was ...
H A Akinci, M Eroglu, G E Özcan, Ü C Yildiz


Whole-of-house protection from subterranean termite attack and damage after four years of field exposure
2008 - IRG/WP 08-10665
This study reports the condition of the whole-of-house termite protection test in tropical Australia after four years. The study was designed to provide maximum protection to whole-of-house timbers in a natural situation posing the highest hazard from subterranean termite populations. The houses were constructed either on concrete slabs or suspended floors using untreated and treated timber fram...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J Hann, C Y Adam


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


Molecular Methods: a Reliable Tool for the Identification of Wood Decay Fungi in Construction Timber
2008 - IRG/WP 08-20386
In the present study, we tested the practical value of several DNA-based methods to identify at the species level the most common wood-decaying fungi infecting buildings. We successfully extracted and amplified fungal DNA from pure cultures of twelve species of wood-inhabiting fungi, from oak and pine wood infected in laboratory with known strains, and from unknown field samples of wood collected ...
M Maître, M Kutnik, I Le Bayon, L Harvengt


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Soft Rot Determines Service Life of L-joints with Low Borate Loading
2008 - IRG/WP 08-30470
As part of a research program on the potential use of borates by the Canadian wood products industry, Forintek set up an L-joint test of untreated and borate-diffusion treated hem-fir (western hemlock and amabilis fir) in 1990. The treated material had a low initial retention of only 0.2% boric acid equivalent and analysis after 5 years revealed no detectable borate close to the tenon. Nev...
P I Morris, J Wang, J K Ingram


The efficacy of commercial silicones against blue stain and mould fungi in wood
2008 - IRG/WP 08-30471
Scots pine (Pinus sylvestris L.) wood samples were vacuum pressure impregnated with quatsilicone micro emulsion (<40 nm particle size), aminosilicone macro emulsion (110 nm) and silicone macro emulsion with alkyl modified side groups (740 nm) and the resulting material properties were studied. Quatsilicone micro emulsion resulted in maximum bulking (4.8%) and anti-swelling efficiency (21.8%) in...
S C Ghosh, C Mai, H Militz


Treatment of Selected Lesser Used Timber Species against Subterranean Termites using Heartwood Extracts from Teak (Tectona grandis) and Dahoma (Piptadeniastrum africanum)
2008 - IRG/WP 08-30476
Lesser used timber species represent a valuable material for all-purpose uses. However, most of them are not durable. They are, for effective utilization, often treated with all manner of toxic synthetic substances to enhance their natural durability, especially in the tropics where conditions favour their deterioration. Most of these toxic synthetic substances often pose a threat to the environme...
A Asamoah, C Antwi-Boasiako, K Frimpong-Mensah


Wood protection, a tool for climate change mitigation?
2008 - IRG/WP 08-50257
In the context of global warming and the search for possible strategies to mitigate climate change, forest and forest products have important advantages. Sustainable management makes forest a carbon sink, wood products have the potential to be a carbon sink as well, and their low carbon intensity is a potential for reducing CO2 emissions by substitution to competing materials. After describing the...
G Deroubaix


Control biológico de la mancha azul en madera aserrada de Pinus radiata D. Don.
2008 - IRG/WP 08-10681
Radiata pine wood is highly susceptible to the attack of sapstaining fungi promoting a discoloration which results in important economical losses. The use of chemicals, a customary procedure to prevent its occurrence is becoming nowadays, due to environmental concern, a more questionable practice. The biological control of blue stain fungi with albino isolates of the Ophiostoma genera appear to ...
J Navarrete, A Segura, P Martínez, R Vera, C Segovia, P Herrera, L Reyes, D McNew, T C Harrington, R L Farrell, J M Thwaites, B Held, R A Blanchette


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh