IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 3: Report of first inspection of samples at Lae, Papua New Guinea
1978 - IRG/WP 446
Samples for the international marine test were placed on frames numbered I to VII. Frames numbered VII of both CCA and CCB trials are being stored dry in the laboratory at F.P.R. & D.C. Frames I to VI of both trials were suspended in the sea at Lae Harbour (Morobe Province, Papua New Guinea) on 6th December 1977. The first inspection of the CCA trial was carried out on 8th June 1978, at which ...
S M Cragg, C R Levy


Service life of outdoor wooden constructions. Expectations of private house owners in Sweden
2001 - IRG/WP 01-10401
Wood is traditionally used in indoor as well as outdoor applications. However, if not kept dry, wood is easily attacked by wood degrading micro-organisms. Thus the service life is heavily affected by construction design, choice of wood and wood treatment. For most constructions there is an expected service life. The expectations concerning wooden constructions and what kind of wood is chosen to fu...
M-L Edlund, J Jermer


Valid scientific names of wood-decaying fungi in construction timber and their vernacular names in England, Germany, France, Sweden, Norway and Denmark
1992 - IRG/WP 92-1546
The valid scientific names of 100 species of wood decaying fungi in construction timber are listed, the citation of authors' names is standardized, and an index of the most commonly used synonyms is compiled. For each species vernacular names used in England, Germany, France, Sweden, Norway and Denmark are listed. The list of names is an attempt to update the current use of the most impor...
F Rune, A P Koch


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


Alternatives to preliminary oven-drying prior to spot-testing treated timber for borate or TBTN preservative penetration
1995 - IRG/WP 95-20067
Commonly-used penetration test procedures for timber treated with borate or organotin wood preservatives demand preliminary oven-drying before application of the spot-testing reagent(s), in order to achieve reliable results. The delay of 12 hours or more during oven drying is often a nuisance. Modifications to the spot-testing procedures, involving alternative solvents and acidification conditions...
M J Kennedy, A Zosars, J Norton


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey


An environmental aspect relating to leachability of CCA from hardwood and softwood poles in Bangladesh
2001 - IRG/WP 01-50167
Leachability of CCA and the service performance of 8 softwood and 5 heartwood poles in service after 5 to 17 years in Bangladesh have been studied. The study included determination of retention of CCA-C in outer 6 mm zones at groundline (GL) and above groundline (AGL) along with the observation of decay and conditions of soils. The mean leaching of CCA-C derived from retention differential at GL a...
A K Lahiry


Effectiveness of some microbiocides against the development of molds and sapstain in Pinus elliottii
1981 - IRG/WP 3169
Eleven commercial biocidal formulations were tested in the field to determine their effectiveness in protecting logs and lumber of Pinus elliottii sapwood from sap stain and molds. Among these formulations 2-(thiocyanomethylthio) benzothiazole showed the best performance in controlling both types of fungi. Potassium N-hydroxymethyl-N-methyl dithiocarbamate and the mixture potassium N-methyl dithio...
S Milano


Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Quality assured wooden sidings - Criteria, performance evaluations and current status
2000 - IRG/WP 00-20216
Quality assured wooden sidings were brought to the Swedish market in 1998. The system was worked out during a six year period in a close cooperation between the sawmill industry and several research institutes. Centuries of use have given a wealth of experience of spruce boards as a siding material, showing that it works well in most cases but also that its longevity is highly variable, depending ...
F Englund, I Johansson, J Ekstedt, R Nussbaum


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Timber preservatives and corrosion
1983 - IRG/WP 3228
A survey of preservative treated timber commodities has illustrated problems that may be caused by corrosion. After treatment, timber should be compatible with commonly used fasteners. Whilst many corrosion methods have been used in the past, no standardized method is used by workers in timber preservation. The Queensland Department of Forestry is developing laboratory test methods for assessing c...
R I Davis


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of sixth inspection (60 months) in Australia
1983 - IRG/WP 499
The IRG/COIPM International Marine Test was installed at Goat Island, Sydney Harbour, in December, 1977. The results of inspections made at 6, 12, 24, 36 and 48 months have previously been reported. This document records the data obtained on the 16.12.82, i.e. after 60 months exposure, at which time only 4 of the test frames remained in test. The surface water temperature at the time of inspection...
L J Cookson, J E Barnacle


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross