IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 690 documents. Displaying 25 entries per page.


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Variable tolerance of Ophiostoma spp. and Diplodia pinea to commercial antisapstain products
1998 - IRG/WP 98-10266
A recent survey of the occurrence of sapstain fungi in New Zealand, conducted at The University of Waikato, provided the opportunity to examine fungicidal tolerance amongst new isolates. It also enabled a comparison of tolerance amongst new isolates with those used in routine antisapstain screening trials at Forest Research. A rapid antisapstain laboratory disc trial was used to determine the ext...
D R Eden, C M Chittenden, B Kreber, J G Van der Waals, R N Wakeling, R L Farrell, T Harrington


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Effects of Prior Establishment of Trichoderma harzianum on Ophiostoma picea Growth in Freshly Sawn Douglas-fir Sapwood
2003 - IRG/WP 03-10476
Trichoderma harzianum has been shown to be an effective biocontrol agent against a number of wood inhabiting fungi under laboratory conditions, but this fungus has performed poorly in field trials. Understanding the interactions between biocontrol agents and their intended targets in wood may provide important clues for developing improved approaches to biocontrol, potentially reducing our relianc...
Ying Xiao, J J Morrell, L M Ciuffetti


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Revised South African standards for wood preservation: Protocols for approval of wood preservatives
1995 - IRG/WP 95-20072
In 1994 the South African timber treatment industry completed its revision of the South African Bureau of Standards (SABS) Code of Practice for the preservative treatment of timber. These revisions were undertaken in parallel with changes to the SABS specifications for preservative treated timber. As a result of shortcomings in the previous wood preservative classification system which was based o...
D Conradie, P Turner, W E Conradie, A D Currie, I S J Burger


Potential for using dip/supercritical fluid treatments for wood impregnation
2004 - IRG/WP 04-40276
While supercritical fluid impregnation offers tremendous potential for impregnating wood species that resist conventional liquid preservative treatments, the resulting treatments are often not uniform among samples in a charge or between charges. One factor that influences treatment is the dynamic change in pressure that occurs during introduction of the biocide laden supercritical fluid into the ...
Sung-Mo Kang, J J Morrell


Effect of origin and orientation of Radiata pine substrates on the development of fungal degrade
2000 - IRG/WP 00-30221
The objective of this study was to determine the influence of different radiata pine substrates on colonisation by sapstain fungi. Freshly-cut branch wood, stem wood and sawn lumber were used to prepare test samples with the largest wood surface area showing a transverse, radial or tangential face. Test samples were evaluated against sapstain fungi using a rapid laboratory antisapstain screening m...
B Kreber, D R Eden, C M Chittenden, B Carpenter, J G Van der Waals


Pretreatment decay in air-seasoning Scots and Corsican pine poles in England
1989 - IRG/WP 1390
British grown Scots and Corsican pine poles were sampled for colonization by basidiomycetes after air-seasoning for 6 to 9, or 16 to 20 months. The amount of infection present in these poles was compared with that in poles which were imported from Finland. After 6 to 9 months seasoning, the British grown pine poles were heavily infected with Peniophora gigantea, Cylindrobasidium evolvens, Stereum ...
A R Zahora, D J Dickinson


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


The effect of of sorbitol on the decay of boric acid treated Scots pine
1991 - IRG/WP 1509
The tetra-hydroxy borate ion is known to undergo complexation with polyols of biological importance and probably protects treated timber by this action. The inhibitory effect of boric acid upon fungal growth and dehydrogenases has been shown to be prevented by the addition of certain polyols. This work was extended, with a study of the effects of a polyol on the performance of boric acid in treate...
J D Lloyd, D J Dickinson, R J Murphy


Fluoride movement through Douglas-fir and hem-fir lumber following dipping in potassium/ammonium bifluoride
1995 - IRG/WP 95-40040
The ability of ammonium and potassium fluoride to diffuse through Douglas-fir and hem-fir lumber was evaluated over a 90 day period. Boards were dipped in a solution containing 10% (by weight) of ammonium and potassium bifluoride, then stored under cover for 90 days. Samples removed 30, 60 and 90 days after treatment indicated that the fluoride was unable to completely penetrate the wood. Penetrat...
J J Morrell, C S Love


Sentry®), a new antisapstain formulation for protecting logs and lumber. - Part 1: advances in protection of New Zealand radiata pine logs
1999 - IRG/WP 99-30188
Until recently antisapstain formulations gave approximately 10 weeks protection to radiata pine logs and even within this time frame protection was often not consistent. Industry requires 20 weeks protection. The degree of protection sought by industry is in the order of 90-95%. For example, this equates to a maximum of 5 - 10% surface cover of sapstain in the first whole veneer produced from a pe...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman, T Price, B Nairn


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...
J Bjurman


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Solid state NMR study on pine wood degraded by brown rot fungus Gloeophyllum trabeum
1994 - IRG/WP 94-10067
Blocks of Pinus koraiensis wood were degraded by Gloeophyllum trabeum and examined by solid-state 13C NMR spectroscopy. Chemical compositions were estimated from relative signal aras. There was no evidence for preferential degradation of the noncrystalline cellulose which accounted for about 4% by weight of the wood. Loss of partly ordered cellulose on crystal surfaces exceeded the loss of crystal...
Yoon Soo Kim, R Newman


Sediment toxicity study of marine piles treated with CCA-C
1995 - IRG/WP 95-50040-35
A study was undertaken to demonstrate the effects of 10-day exposure to sediments mixed with leachate from chromated copper arsenate Type-C (CCA-C) southern pine marine piles treated to a retention of 40 kg/m³ (2.5 pcf) and untreated southern pine piles on the benthic amphipod, Ampelisca abdita. The biological endpoint used to establish effects was organism survival. Leachate obtained during a 28...
W J Baldwin, E A Pasek, P D Osborne


Field studies investigating the efficacy of biological treatments in preventing decay of freshly-felled pine
1993 - IRG/WP 93-10022
Four species of fungi (Trichoderma viride, Ascocoryne sarcoides, Potebniamyces conifererum and Cryptosporiopsis terraconensis) and sterile distilled water were applied separately to unpeeled, freshly-felled pine billets. The fungi were all in the form of concentrated aqueous spore suspensions, and were spread onto the end-grains of the logs by brush. Destructive sampling of the billets was carried...
M W Schoeman, D J Dickinson


Oxidation of wood components during CCA-C fixation
1993 - IRG/WP 93-30024
Pre-extracted radial sections of southern yellow pine sapwood were treated with CCA-C and analyzed by X-ray photoelectron spectroscopy (XPS). The ratio of C1 (carbon bonded to carbon and/or hydrogen) to C2 (carbon bonded to one oxygen) in XPS Cls spectra was taken as a measure of the progress of oxidation of wood components during CCA fixation. This ratio was 0.82 before CCA treatment and increase...
M Kaldas, P A Cooper


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part II. Effect of extractive contents and taxifolin
2002 - IRG/WP 02-10446
The previous paper (Part I: Effect of density and growth rate) described the variation in natural durability of 4 Douglas fir (DF) seed origins (Darrington, J. Landing, Naselle and Hawkinsville) in a pure culture decay test and fungal cellar test. The pure culture tests were performed against two brown rot fungi (Coniophora puteana and Postia placenta). In the fungal cellar test soft rot was the p...
S Akhter, M D C Hale


Molecular phylogeny of Ophiostoma spp. related to blue-stain in pine
2002 - IRG/WP 02-10432
Blue-stain in coniferous woods is an economically important disease in many temperate countries, caused specially by genus Ophiostoma. Classical taxonomy of genus Ophiostoma is limited for the correct identification of many species, because of the similar macroscopic and microscopic characters, as well as the existence of some species complex. Molecular identification is a good complement to eluci...
M Villarreal, F Arenal, J Sánchez-Ballesteros, M T De Troya, F Llinares, V Rubio, A Navarrete


Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles
2001 - IRG/WP 01-40206
Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles. Fungal colonization of poles following peeling has been the subject of considerable concern among electric utilities. While the presence of fungi does not, in itself constitute a risk, the survival of these fungi through the conventional treating processes could allow them to continue to degrad...
J J Morrell, P G Forsyth, K L Levien


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields


Previous Page | Next Page