Comparison of exterior performance of two coating systems based polyurethane applied Pinus sylvestris L. and Picea orientalis L. wood
2012 - IRG/WP 12-40588
Some surface changes in sapwood and heartwood of two species before applying clear-coating were characterized after accelerated weathering time. Wood specimens covered with two types polyurethane (PU) films were also observed in accelerated weathering exposure. In this study, changes on the wood surface were compared of between wood specimens covered with two types polyurethane (PU) films after ir...
Ö Özgenç, Û Cafer Yıldız


Efficiency of the Amazon Forest Oils as Preservatives to the Attack of cellulolytic fungi in Pine Wood
2012 - IRG/WP 12-30599
The bobbins of wood are used for storage and field installation of cables from the electricity and telecommunications sectors. There are legal requirements governing the Brazilian ways of treating the wood used in these sectors, aimed at preventing pollution and protecting nature. When exposed to severe environmental conditions in Brazil these products are degraded and occurs many operational prob...
S Silveira, I M S Mendes, R S Paiva, J E Volponi, R C G Comar, R S Cruz


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


NIR spectroscopy for rapid determination of permethrin or bifenthrin retention in P. radiata sapwood
2013 - IRG/WP 13-20507
Near infrared spectroscopy of permethrin or bifenthrin treated radiata pine (P. radiata D.Don) has been used to develop calibration models to later predict the active retention in unknown samples. Calibrations were developed for both a laboratory NIR and a portable NIR using laboratory-prepared calibration samples at a range of target retention levels. Correlations were established between the act...
R Meder, N Ebdon


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Antifungal properties and bonding of menthoxymethylimidazolium ionic liquids with Scots pine wood
2013 - IRG/WP 13-30627
Antifungal activities of five chiral ionic liquids - menthoxymethylimidazolium derivates against brown-rot decay fungus (Coniophora puteana), white-rot decay fungus (Trametes versicolor) and blue-stain fungus (Sclerophoma pithyophila) were determined using screening agar-plate method. Results from antifungal tests revealed that 1-butyl-3- menthoxymethylimidazolium chloride exhibited the stronges...
J Zabielska-Matejuk, J Feder-Kubis, A Stangierska


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Chemical composition of extractives of different wood compartments of Pinus merkusii and their potential implication in wood durability
2015 - IRG/WP 15-10841
Amounts and nature of extractives differ strongly according to the compartment of wood and to the nature of the wood species. Previous studies reported that knotwood of several European Pinus sp. contains extractives contents much higher than stemwood consisting mainly of lignans which may find valuable applications in cosmetic, nutraceutic or pharmaceutic sectors. Different explanations have been...
A Wijayanto, S Dumarçay, R Kartika Sari, W Syafii, P Gérardin, C Gérardin-Charbonnier


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Evaluation of color and gloss in decorative applied to cases of Pinus radiata wood impregnated (D. Don) copper type C azole micronized
2015 - IRG/WP 15-20571
Six treatments (one control and five decoration coatings) were applied to radiata pine wood treated with micronized copper azole (uCA-C), for outdoor use (R3) at a rate of 3.08 kg/m3 retention (T2). One decoration coating was applied before impregnation treatment: Prestain P (T3), and two, were applied in mixture with the uCA-C preservative Black Cylinder (T5) and Red Cylinder (T4). Two varnish we...
R Garay, M Inostroza


Functional silicones used as a potential tool for the development of non-biocidal wood treatments
2015 - IRG/WP 15-30665
The increase of wood resistance against biological agents for outdoor use is conventionally performed by deep impregnation with preservatives. However, some of the traditional wood preservatives, used for decades for wood protection and regarded as the most effective, are currently subjected to severe restrictions because of their toxicity. In fact, new preservation technologies are constantly ent...
F Lhumeau, C Delaite, F Marchal, F Pochon, M Kutnik


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Remedial treatment of difficult to access timber in buildings
2015 - IRG/WP 15-40691
The quest to understand remedial treatment for timber framing begun following the ‘leaky building crisis’ in New Zealand which came to prominence in 2000. Several in-situ remedial treatment products are used in New Zealand. However, effectiveness of these treatments is still unclear particularly in situations where not all faces of the timber can be assessed. This research was conducted to det...
T Singh, I Simpson, D Page


Termite and insect resistance of acetylated wood
2015 - IRG/WP 15-40703
The benefits from acetylation of wood to enhance resistance against fungal decay and dimensional stability have been known for many years. Since 2007 Accsys Technologies has been commercially producing Accoya® wood that is based on acetylation of radiata pine. A number of studies on the resistance of acetylated wood to attack by wood destroying termites have been conducted, but there is no common...
F Bongers, M Kutnik, I Paulmier, J Alexander, H Militz


Formation of biofinishes on outdoor exposed wood; the impact of wood-oil combination and geographical location
2016 - IRG/WP 16-10864
Growth of dark moulds enables the use of a decorative and protective biofinish for wood, showing advantages compared to traditional wood-coatings in terms of sustainability and self-repair. Based on the formation of a uniform mould covering on oil treated wood during outdoor exposure, the utilisation of a biofinish is in development. Basic information is lacking on the correlation between exposure...
E J van Nieuwenhuijzen, L Ross Gobakken, M F Sailer, R A Samson, O C G Adan


CCA Treated Wood, Will It Last 100 Years?
2016 - IRG/WP 16-20575
Copper, chrome and arsenate (CCA) treated wood has a very successful history of use in New Zealand, for at least 60 years. In many parts of the world, CCA has been used for timber treatment since the mid-1930s. In this report, data are presented on the performance of CCA treated pine stakes and poles. Results from ground contact durability tests at Scion and other overseas test performance data su...
T Singh, D Page


Measurement of Cell Wall Moisture in Acetylated Radiata Pine Using Low-Field Nuclear Magnetic Resonance
2016 - IRG/WP 16-20583
Understanding the interaction of water with acetylated wood is necessary to explain how the protective mechanism of acetylation functions. Low-field nuclear magnetic resonance is one technique for assessing water in wood. Pinus radiata earlywood sapwood samples were acetylated to various weight percentage gains and then analysed with this method. Increased levels of acetylation showed significantl...
H G Beck, C A S Hill