Development of threshold values for boron compounds in above ground exposures: Preliminary trials
1998 - IRG/WP 98-30179
Boron is increasingly used both as an initial and remedial treatment for protecting wood against fungal and insect attack. While establishing lethal dosages for boron against insects through feeding tests is relatively simple, establishing thresholds for fungal attack poses more of a challenge. Tests using boron dispersed in agar artificially surround the fungus with both boron and excess nutrient...
J J Morrell, C M Freitag, S Unger


Defacement of freshly sawn Corsican pine lumber by sapstain and mould fungi and the influence of arthropods
1997 - IRG/WP 97-10227
In a trial to study the arthropods associated with sapstain and mould fungi, freshly sawn Corsican pine (Pinus nigra var. maritima (Aiton) Melville) boards were block stacked at a local sawmill. Each stack was constructed in a nest arrangement with smaller boards in experimental tanks, positioned in the centre of the stacks. Boards were converted from a stock of sawlogs at monthly intervals, to pr...
N J Strong, J F Webber, R A Eaton


Effect of compression wood on leaching of chromium, copper, and arsenic from CCA-C treated red pine (Pinus resinosa Ait.)
2000 - IRG/WP 00-30232
In this study, the effect of compression wood formation on the release rate of chromium, copper, and arsenic elements from red pine (Pinus resinosa Ait) was investigated. Wood blocks from red pine containing compression and normal wood portions were treated with a 1.0% CCA-C solution and were then allowed to fix at 23 ± ??2°C (74 ± 4°F) for 0, 6, 24, 48, 96, 192, and 336 hours. After each fixa...
S N Kartal, S T Lebow


The influence of causing primary blue-stain fungus Ceratocystis imperfecta on selected properties of Scots pine wood
2002 - IRG/WP 02-10425
The effects of development in wood the fungi causing blue-stain on the wood properties are not univocal. There were been undertaken investigation to clear the influence of such fungi on selected physical and mechanical properties of Scots pine wood. Wet sap wood samples of fresh cut Scots pine wood (Pinus sylvestris L.) were infested with pure culture of Ceratocystis imperfecta Mill. et Grenz and...
A Fojutowski


Log fumigation prevents enzyme-mediated sapwood discolorations in hardwoods
1993 - IRG/WP 93-10003
Non-microbial sapwood discolorations in hardwood lumber can cause economic loss by degrade of quality. Based on the hypothesis that the enzyme-mediated sapstain may develop in part from byproducts of parenchyma cells in wood, reshly felled logs of red oak (Quercus spp.) and sugar hackberry (Celtis laevigata) were fumigated under a plastic tarp with methyl bromide. Log sections were checked after f...
E L Schmidt, T L Amburgey


Kerfing and center-boring reduce checking in CCA-treated slash pine posts
1997 - IRG/WP 97-40082
Single and double kerfing, center-boring and incising were applied to green, peeled, slash pine posts. Posts were air dried for ten weeks and assessed for the number of surface drying checks greater than 1.0 mm in width. Posts were then pressure treated with a chromated-copper-arsenate (CCA-C) preservative and exposed outdoors in a horizontal position. The number of surface weathering checks in th...
P D Evans, R Wingate-Hill, R B Cunningham


Study of modulus of rupture, circumference taper, sapwood thickness and CCA treatment of Norwegian origin Pinus sylvestris poles
1994 - IRG/WP 94-20054
Nondestructive strength testing with Pilodyn (6J) of Norwegian Pinus sylvestris poles revealed effective modulus of rupture (MOR) of 54.39 N/mm² at wet conditions after CCA-C treatment and circumference measurement revealed circumference taper of 0.021 m/n. Sapwood thickness or penetration of CCA-C study revealed that 77% poles were with sapwood thickness equivalent to 39.6% of radius of poles an...
A K Lahiry, S Begum, G N M Ilias, M A B Fakir, R U Hafiz


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


Occurrence and importance of various types of fungal and bacterial decay in CCA-treated horticultural pine posts in New Zealand
1984 - IRG/WP 1234
A detailed microscopical examination has been carried out on samples taken from CCA-treated pine posts exposed in horticultural soils. The following decay types were observed: white rot, brown rot, soft rot, tunnelling bacteria, cavitation bacteria, and bacterial erosion. The occurrence and importance of the various decay types between different regions, and plots within a specific region, varied ...
T Nilsson


Minimum inhibitory concentration of methylene bisthiocyanate towards selected wood inhabiting fungi in liquid culture and on radiata pine
2001 - IRG/WP 01-30261
The objective of the current study was to determine the minimum inhibitory concentration (MIC) of methylene bisthiocyanate (MBT) towards wood inhabiting fungi common on unseasoned radiata pine (Pinus radiata D. Don). The fungi used were Ophiostoma floccosum, Leptographium procerum, Sphaeropsis sapinea and Trichoderma viride. Fungi were individually inoculated into nutrient media spiked with differ...
T Singh, B Kreber, C Chittenden, R N Wakeling, A Stewart


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


Validation of the sapstain danger index
2000 - IRG/WP 00-10333
The Sapstain Danger Index (SDI) is a model that is used to indicate sites in the New Zealand forest where felled logs are more prone to sapstain, specifically it should indicate how soon after felling of a log should it be treated for sapstain. The validation of SDI has the goal to identify whether the SDI can be used to predict sapstain development and to eventually minimise loss of value of logs...
P A Cooper, S Downs, R l Farrell


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


Wood preservation in Southern Africa
1984 - IRG/WP 3320
This report deals with the status of wood preservation in the countries of Southern Africa, namely Botswana, Lesotho, Mozambique, Namibia, South Africa, Swaziland and Zimbabwe. It includes some data on the timber production from the forests of these countries, as well as detailing the state of the timber products industries in South Africa which is the dominant country in the field in the sub-cont...
A Pizzi, W E Conradie, R Cockcroft


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


After 18 years, preservative dipping and brush treating continue to provide protection to shingles of western wood species
1997 - IRG/WP 97-30156
The presence of residual preservation in dip-treated and brush-treated shingles of various species from the western United States was assessed 18 years after installation using Aspergillus bioassays. The performance of western redcedar (Thuja plicata) was compared to western hemlock (Tsuga heterophylla), sugar pine (Pinus lambertiana) and western larch (Larix occidentalis). Untreated shingles of a...
T C Scheffer, D J Miller, J J Morrell


A trial of "sour" felling to prevent bluestain by depletion of sapwood nutrients
2001 - IRG/WP 01-10404
Discoloration of conifer wood caused by bluestain causes large economic losses in Canada. Most deep stain develops in the log stage during storage or transport. In a search for control strategies that will not disrupt woodlands productivity we tested "sour" felling, termed "hagarashi" in Japan. The practice involves delaying the delimbing of freshly harvested trees. The tree continues to transpire...
A Byrne, A Uzunovic, D Minchin, C Breuil


The role of mechanised harvesters in the dissemination of fungal inoculum into radiata pine logs in New Zealand
2002 - IRG/WP 02-10426
A joint research programme has been initiated between Forest Research, New Zealand and Forintek Canada Corp., Canada, to determine the role of mechanical tree harvesters on disseminating fungal inoculum into logs. Mechanical harvesters cause loosening and removal of bark and also damage the surface of the wood with their feed rollers leaving indentations up to several centimetres deep. Results ...
D O’Callahan, B Kreber, A Uzunovic


Decay potential of various New Zealand Phlebiopsis gigantea strains using a soil block method
1999 - IRG/WP 99-10309
The objective of the current study was to determine the decay potential of different strains of Phlebiopsis gigantea using Pinus radiata and European Fagus sylvatica, respectively. A soil block method was used to determine mass weight loss of P. radiata and F. sylvatica following 10 weeks incubation with different strains of P. gigantea. For comparison, Trametes versicolor, Postia placenta, Gloeop...
B Kreber, J G Van der Waals


Internal pressure development in Douglas fir lumber during pressure treatment
1997 - IRG/WP 97-40091
Preservative treatment of Douglas fir lumber to meet current industry standards poses a major challenge and a variety of methods have been developed to overcome these problems. One aspect for treatment improvement that has received less attention is the relative effect of treatment parameters on changes in pressure within the wood. Previous studies of spruce and radiata pine suggest that internal ...
P F Schneider, J J Morrell


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Bending strength of heat-treated spruce and pine timber
2002 - IRG/WP 02-40242
Heat-treatment of spruce (Picea abies) and pine (Pinus sylvestris) beams (45 x 145 mm) gave a reduction in bending strength of approximately 50%. The bending stiffness (modulus of elasticity) only decreased by 3.5%. Tests were carried out according to EN 408. Another effect of the heat-treatment was increased variation in bending strength. The 5th percentile value of the bending strength, the so c...
C Bengtsson, J Jermer, F Brem


Surface checking of CCA-treated radiata pine decking timber exposed to natural weathering
2000 - IRG/WP 00-40165
A field trial was established at four locations in Australia to assess the effect of CCA and CCA-wax treatment on the checking (cracking) of radiata pine decking timber exposed to natural weathering. Untreated decking timber and timber that had been pressure treated with water acted as controls. After 1 year's exposure the number and sizes of checks occurring in treated timber and control...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham