Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Feasibility of using biological control agents to arrest and prevent colonization of Douglas fir and southern pine by decay fungi
1988 - IRG/WP 1345
The use of microfungi to control basidiomycetous decay has been evaluated in Europe for many years, where it has produced mixed results against Lentinus lepideus Fries, the fungus presumed to be the major cause of decay in Scots Pine poles. In the United States, remedial decay control has been largely chemical, with little use of alternative decay control strategies. Increasing restrictions on che...
J J Morrell, C M Sexton


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui


Invasion and colonisation of bamboo culm material by stain and decay fungi
2002 - IRG/WP 02-10453
Two distinct stages of the fungal infection of bamboo culms can be identified: entry into the culm itself (invasion) and further colonisation by spread within the culm wall tissue. This laboratory study aimed to characterise different invasion strategies of a variety of fungi. Well-known isolates of white- (Coriolus versicolor, Schizophyllum commune), brown- (Coniophora puteana, Gloeophyllum tra...
G Kleist, I Morris, R J Murphy


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka


A survey of the incidence of decay in copper-chrome-arsenate treated trellis support posts used in horticulture in New Zealand
1984 - IRG/WP 1225
Copper-chrom-arsenate treated softwood posts used as trellis support structures in 5 major horticultural districts of New Zealand were systematically examined for presence of decay. Principal crops on properties examined were grapes and kiwifruit; a minority of properties grew hops, boysenberries, and dwarf apples. Occurrence and severity of decay were variable within specific age classes of posts...
M E Hedley, J A Drysdale


A reliable spot test for TCMTB in wood
1992 - IRG/WP 92-2391
Test specimens of slash pine (Pinus elliottii) and spotted gum (Eucalyptus maculata) were treated with aqueous emulsions of Busan 30WB and Busan 31, containing the fungicide TCMTB (2-(Thiocyanomethylthio)benzothiazole), or with solutions of TCMTB in toluene. These and matching untreated specimens were subjected to a wide range of procedures in an attempt to reveal TCMTB penetration patterns. Most ...
D E Ferlazzo, M J Kennedy


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-Gütegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


Applications of the shower test. Part A: Results from CCA type C treated wood: influence of fixation process
1993 - IRG/WP 93-50009
This report outlines the results of shower tests conducted on CCA type C treated wood. The results indicate the inherent good fixation of CCA type C, as judged by the leaching limits within the Environmental Regulations. The shower test has proven to be a useful quality control and research test. It determines reasonably accurately the leaching under simulated conditions and, admittedly from a lim...
W J Homan, H Militz, D A Lewis


Venezuelan net of test fields for the study of the effectiveness of treatments of non commercial timbers from natural tropical forests
2005 - IRG/WP 05-20318
A net of 13 tests fields were established in Venezuela for the study of the effectiveness of the CCA and CCB treatment in secondary or non commercial woods from natural forests, two woods from fast growth plantations wee included for promote them as treated timber mainly for fence posts uses. Partial results after two years are presented and discussed the preliminary results obtained both in field...
O Encinas, N Mora


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


Growth of selected wood decay fungi on various agar-supplemented media
2003 - IRG/WP 03-10456
The growth rates of a selection of wood decay fungi (brown and white rots) on various agar-supplemented media have been determined and compared. The agar media investigated were Malt extract agar (MEA), Potato dextrose agar (PDA), YMPG agar (yeast extract, malt extract, bacto-peptone, glucose, asparagine and thiamine), YMPG agar (without amino acids) and Beech wood powder agar (BWA). The tested wo...
S A Amartey, M Humar, F Pohleven


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Update
1994 - IRG/WP 94-20032
It was agreed by members at the termite workshop at the 24th annual meeting of IRG in Orlando, USA, in May 1993 to initiate an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives (CCA and Cu-naphthenate) against t...
J R J French


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Performance of borate-treated sill plates (dodai) in a protected, above-ground field test in Japan
2002 - IRG/WP 02-30278
This document is supplemental to the previous IRG document (IRG/WP 2000-30239). An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT...
K Tsunoda, A Adachi, A Byrne, P I Morris, J K Grace


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 2: Computer-assisted miniaturisation of wood specimens
1994 - IRG/WP 94-20052
The mass loss of wood used as a criterion in the standarised agar-block method of evaluation of toxic value of preservatives depends upon the relationship between volume of specimens, their outspread planes and ratio of areas of particular anatomic sections. Upon the computer-assisted mathematical basis the dimensions of miniaturized specimens which make 1/2, 1/4, and 1/8 part of standarized ones ...
J Wazny, K J Krajewski


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Termites in Uruguay; control, prevention and environment
1991 - IRG/WP 1474
When Prof. La Fage's questionaire on termites was received by 1987, few were aware of termite damage in Uruguay and infestations were not much reported. Further contacts between scientists, operators and homeowners, are now shaping the real threat of termite attack. Before letting the problem faIl in the hands of the layman, with all ist environmental risks, it seemed reasonable to: 1) re...
A Aber, G Baillod


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy