Co-operative research project on L-joint testing. Progress report to March 1984
1984 - IRG/WP 2211
Each participant was intended to expose L-joints in the main trial on 1 April 1983 and the first sampling, after 8 months exposure, was to be undertaken on 1 December 1983. Some participants have had to vary this schedule. Results are presented from CTFT (France) and PRL (United Kingdom). These show a greater effectiveness by the double vacuum treatments compared with the 1 minute dip treatments. ...
J K Carey, A F Bravery


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy


Applications of the shower test. Part B: Results from CC and CCB treated wood: influence of fixation process
1993 - IRG/WP 93-50010
This report outlines the results of shower tests conducted on CC and CCB treated wood. The results indicate the fairly good fixation of chromium and the reasonable fixation of copper in CC and CCB formulations, as judged by the leaching limits within the Environmental Regulations. In general boron leaches to a higher extent than chromium and copper. The shower test has proven to be a useful qualit...
W J Homan, H Militz


Assessment of dehydrogenase activity, fluoride content and total chromium content of soil profiles exposed to preservative treated wood within a model system
1993 - IRG/WP 93-10015
The development and prospective use of a closed model system to facilitate study of a number of indicators of environmental impact of wood preservatives laboratory conditions has been described (IRG/WP/2395-92). Chemical analysis of leachate samples collected from drained soil profiles containing creosoted pole sections remedially treated with a chromated fluoride preservative indicated small incr...
G M Smith, D C R Sinclair, A Bruce, H J Staines


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Valid names for some common decay fungi and their synonyms
1992 - IRG/WP 92-1522
The taxonomy of wood destroying fungi has changed noticeably within the last ten years. New genera and more well defined generic concepts have emerged with concomitant and necessary changes in nomenclature. The following is a revision of a list originally prepared by Kaarik (1979) in collaboration with Professor Dr. C. Jacquiot (France), Mr. J. G. Savory (United Kingdom) and Dr. G. Seehann (Federa...
M J Larsen, R M Rentmeester


The efficacy of remedial treatments for controlling fungal decay in window millwork used in the United States
1987 - IRG/WP 3432
Conventional window millwork was subjected to basidiomycete decay by inoculation and sampled for active growth of the decay fungus before and eight months after remedial preservative treatment with fused disodium octaborate rods (IMPEL) at boric acid levels of 1.5 and 4.0 kg/m³ or liquid bifluoride injections (IMPROSOL) at 1 kg/m³. The elimination of decay fungus after remedial treatment was nea...
M G Dietz, E L Schmidt


An electron spin resonance study of manganese changes in wood decayed by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1359
Electron spin resonance (ESR) spectrometry was used to examine wood decay by the brown-rot fungus, Postia placenta. Wood slivers of Douglas-fir, white fir, redwood, sweetgum and yellow poplar were incubated for 4 weeks in custom-made quartz ESR tubes with or without Postia placenta. In all wood species without fungus, a weak partially resolved signal (about g=2, presumably due to manganese) was de...
B Illman, D C Meinholtz, T L Highley


Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny


A termite field test with diffusion treated lumber
1991 - IRG/WP 3648
Douglas fir lumber, diffusion treated with concentrated sodium octaborate solutions, was tested against Coptotermes formosanus in an above ground field test wherein the samples were not exposed to a direct leaching hazard during the test period. After 2.5 years exposure, the untreated control samples were almost completely destroyed while poorly treated controls pressure treated with chromated cop...
K J Archer, D A Fowlie, A F Preston, P J Walcheski


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Incorporation of phenyl boronic acid treatment with vapor phase formalization
1997 - IRG/WP 97-40083
Phenylboronic acid (PBA) treatment was incorporated with vapor phase formalization (VPF) in order to increase dimensional stability and boron fixation as well as enhancement of biological resistance. Five and ten hours VPF were applied after PBA treatment as 0.34, 0.50, 1.00 and 2.00% concs. aqueous solutions. Anti swelling efficiency (ASE) attended to 71% in specimens impregnated with 0.50% PBA s...
M K Yalinkilic, S Yusuf, T Yoshimura, W-Y Su, K Tsunoda, M Takahashi


Effect of soil parameters on biocide depletion: laboratory and field studies of water- and emulsion-borne preservatives
2000 - IRG/WP 00-30234
Two field test sites with different soils were selected. Soil analysis showed that the soil at the two sites had considerable texture, base saturation, acidity, and cation exchange capacity differences. Five sets of field stakes were treated as follows: three with water-borne CCA to about 0.4 pcf (6.4 kgm-3) retention, one with 0.75% DDAC, and one with 0.75% DDAC:0.25% chlorothalonil. The last two...
T Schultz, D D Nicholas, D E Pettry, M G Kim


Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch


Termite and decay resistance of particleboard composed of white cypress pine and radiata pine
1997 - IRG/WP 97-10200
Phenol-formaldehyde bonded particleboard was manufactured from blends of non-durable radiate pine (P. radiate) and heartwood of the naturally durable species, white cypress pine (C. glaucophylla). Board specimens were subjected to bioassays using two termite species, M. darwiniensis and C. acinaciformis, and the basidiomycete fungi, C. puteana and P. ostreatus, and the durability of specimens was ...
P D Evans, J W Creffield, J S G Conroy, S C Barry


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Reaction of osmium tetroxide with a diphenolic compound as a model substance for demethylated lignin
1986 - IRG/WP 1303
By using caffeic acid as a model substance for diphenolic moieties of demethylated lignin it was found that electron dense particles called by the authors "osmiophilic particles" in former papers are reaction products of OsO4 with the model substance. By these products it is possible to indicate the enzymatic demethylation of lignin taking place during wood decay. The appearance of the electron de...
K Messner, E Srebotnik


Natural decay resistance of some lesser-used tropical hardwoods from Ghana
2002 - IRG/WP 02-10438
Ghana is a tropical African country that is rich in diverse timber species. In order to reduce over-exploitation of the popular timber species and increase the resource base for the wood industry, lesser-used or lesser-known timber species are being promoted locally and for export. To do this successfully, it is essential to determine the physical, mechanical and biological properties of these tim...
S A Amartey, F R Hanson


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Susceptibility of CCB treated wood to fungal colonization
2003 - IRG/WP 03-10492
CCB treated wood is generally resistant to all wood decay fungi. However, like CCA impregnated wood, susceptibility of CCB treated wood to copper tolerant fungi have been observed. The ability of various brown rot fungal hyphae to penetrate and overgrow the wood samples was investigated. Samples made of Norway spruce (Picea abies) were impregnated with 5 % CCB solution according to the EN 113 proc...
F Pohleven, U Andoljsek, P Karabegovic, C Tavzes, S A Amartey, M Humar


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Final proposals for a field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot
1976 - IRG/WP 367
A series of hardwood stakes have been prepared and treated in the UK from samples (mainly sapwood) supplied from participants around the world. The stakes include 4 reference species common to each site and, in most cases, at least 2 local species of importance. The treated stakes will be despatched to the co-operating scientists and installed under local conditions. It is hoped that with periodic...
D J Dickinson


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 2nd Interim Report
1990 - IRG/WP 4161
The results of a collaborative international test to evaluate the performance of elastomeric polyurethane coatings of wooden test samples exposed in seawater at 13 sites around the world are reported. The samples have been exposed at sites with known infestations by molluscan and/or crustacean wood borers. Performance data for up to 4 years exposure at some sites is presented providing information...
R A Eaton


Previous Page | Next Page