IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1740 documents. Displaying 25 entries per page.


In search of alternative antisapstain chemicals for use in Papua New Guinea
1988 - IRG/WP 3472
The paper presents results of antisapstain field trials from three locations in Papua New Guinea as part of the Research Centre's programme to find suitable antisapstains to replace the hazardous sodium pentachlorophenate. Effectiveness of seven tested chemicals varied between indigenous pines (Araucaria cunninghamii, Araucaria husteinii) and white coloured hardwoods (Alstonia scholaris, ...
A Oteng-Amoako


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 8: Panama test results
1980 - IRG/WP 458
Summary of damage to ITRG test stakes by pholadidae and teredinidae at the Panama test site - 8 Mar. '78 to 11 Oct. '79...
J R De Palma


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


A new wood preservative based on polymerized complexes of aminotriazole with copper acetate
1998 - IRG/WP 98-30169
This paper presents the results of preliminary fungitoxicity tests as carried out on new polymerized complexes of aminotriazole with copper acetate (PCC) against Coniophora puteana and Trichoderma viride. Laboratory tests on wood confirmed the findings arrived at in the screening test on agar medium. Deep penetration into pine wood of compounds studied was observed and particularly so at humidity...
K J Krajewski, A Lukasiewicz, J Wazny


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


Marine test of synthetic pyrethroids at Sekondi, Ghana
1981 - IRG/WP 478
The trials reported here are part of a new series of marine exposure tests (Ghana Series 80) begun in October 1979 and designed to assess the natural durability if indigenous timber species and the performance of preservatives and preservative combinations in indigenous wood substrates in Ghana's coastal waters....
F F K Ampong


Preliminary results of investigations on screening test of chemical compounds suitable for the preservation of lignocellulosic materials against biodeterioration
1976 - IRG/WP 262
This paper investigates the possibilities of reducing the time needed for the determination of the effectiveness of chemical compounds from the point of view of their eventual application to lignocellulosic materials for preservation against decay and soft-rot....
K Lutomski, S S Neyman


Response of the Formosan Subterranean Termite (Coptotermes formosanus) to Cellulose Insulation Treated with Boric Acid in Choice and No-Choice Tests.
2004 - IRG/WP 04-10532
The tunneling ability of the Formosan subterranean termite Coptotermes formosanus Shiraki through a cellulose insulation material containing11.1% boric acid was tested in choice and no-choice bioassays. We examined tunneling behavior and mortality of termites exposed to treated and untreated insulation material in miniature simulated wall voids. In a choice test termites tunneled through untreat...
M E Mankowski, J K Grace


The influence of crystalline and amorphous cellulose on extracellular hydrogen peroxide production by brown-rot fungi
1991 - IRG/WP 1482
The production of hydrogen peroxide (H2O2) has been suggested to play a key role in the degradation of wood by wood-rotting fungi. The production of extracellular hydrogen peroxide was studied by a quantitative method which detects the oxidation of the 2,2-azinobis(3-ethylbenzthiazoline-6-sulphonic acid) (ABTS) by H2O2 and horseradish peroxidase (HRP) in liquid culture medium. The carbon sources u...
A-C Ritschkoff, L Viikari


Short-term field test method with accelerated infection of Basidiomycetes in wood
1981 - IRG/WP 2155
In the ŠIPAD - IRC Wood Protection Laboratory an attempt has been made to develop a simple short-term method for field testing out-of-ground contact wood using accelerated infections with Basidiomycetes. This method makes it possible to obtain a preliminary assessment of a preservative's quality and to estimate the possibility of achieving promising results in more expensive long-term te...
N Vidovic


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Effects of a chitin synthesis inhibitor on spore germination of the decay fungi Gloeophyllum trabeum and Poria tenuis
1986 - IRG/WP 2253
This study sought to determine the effect of a chitin synthesis inhibitor - Polyoxin D, on spore germination and early hyphal development of a brown rot and a white rot fungus in-vitro. Polyoxin D is a competitive, substrate-analogue type of chitin synthtase inhibitor (2). The drawbacks to use of such a compound as a wood preservative tie. cost - $20,000/g, possible leaching or degradation) might ...
E L Schmidt


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


Field trials of anti-sapstain products. Part 1
1991 - IRG/WP 3675
The results obtained in two field tests of anti-sapatain products, carried out in four locations in Portugal, are presented. Boards from freshly cut logs were hand-dipped, close staked and left to dry for periods from four to six months. The results obtained seem to indicate that some of the products tested performed at least as well and sometimes better, than a 3% NaPCP solution which was used as...
L Nunes, F Peixoto, M M Pedroso, J A Santos


What information can we glean from field testing
1995 - IRG/WP 95-20057
To mathematically compare the performance of preservatives in a field test, equations were formulated to describe the relation between log score and time and between rate of decay and retention. By combining these equations, a model was derived for the performance of a number of waterborne preservatives. Some relations between the estimated parameters for different preservatives were noted and the...
P I Morris, S Rae


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Establishment of a laboratory method to characterise the ecotoxicity of a polluted soil
1998 - IRG/WP 98-50101-23
This method consists in using the underground grub of the Oxythyrea funesta beetle as a bioindicator of the soils pollution. Due to the significant tolerance of the organism, a large type of substrate of different nature and grain size could have been studied. We have tested substances and preparations such as wood preservation products even under powder or liquid form but also some wastes of di...
P Martinet


Report on International Conference on Marine Biodeterioration, Goa, India, January 1986
1986 - IRG/WP 4127
At the International Conference on Marine Biodeterioration - Advanced Techniques Applicable to the Indian Ocean, there were a number of papers relevant to the aims of Working Group IV of IRG. Abstracts of these papers and a brief commentary on the conference are presented....
S M Cragg


Mycological testing of plywood and board materials. Part 1: Review of information supplied by IRG members
1978 - IRG/WP 284
In December 1975 IRG members were asked for published information, information of current work in progress and views on mycological test methods for board materials. The object was to stimulate discussion and possibly establish a joint research effort within IRG in order to establish a meaningful test with reproducible results....
C R Coggins


Microcapsule formulation of fenitrothion as a soil termiticide
1991 - IRG/WP 1478
The efficacy and the mode of action of a microcapsule formulation of fenitrothion against Coptotermes formosanus Shiraki were investigated. The physicochemical property that this formulation does not allow the active ingredient to diffuse through the capsule wall contributed to a long lasting efficacy and safety for the men spraying. The residual effect of the fenitrothion microcapsule in soil was...
H Teshima, T Itoh, Y Abe


The effect of treatment method on CCA efficacy in Corsican pine
1992 - IRG/WP 92-3723
As part of a study into the influence of application method on preservative efficacy Corsican pine (Pinus nigra) samples (50 x 50 x 400 mm³) were treated with a CCA formulation using Bethel, Steam/Bethel or Lowry processes. Full penetration of the preservative at a gross level was confirmed using a copper disclosing reagent. The preservative was allowed to fix and then samples were converted into...
P R Newman, R J Murphy


On site test for indicative determination of leaching of components of preservatives from treated timber. Part 2: New data on CCA-C, CC and CCB treated timber
1994 - IRG/WP 94-50025
The 'on site test' was published at the IRG meeting in Cannes in February 1993 (IRG/WP 93-50001/12). Since this publication many on site tests were performed parallel to so-called shower tests. The correlation between the test results of the on site tests and the shower test has been established more clearly. For chromium the correlation between both tests is indistinctive of pre...
W J Homan


Update on lab and field test results for polymeric alkylphenol polysulfide treated wood
2002 - IRG/WP 02-40240
The possibility of using Polymeric Alkylphenol Polysulfide (PXTS) as a wood preservative has been undergoing evaluation in our laboratories for the past four years. Various formulations prepared from this compound have been tested and found to be effective against wood decay fungi and insects in field stakes after 42 months exposure. In accelerated soil bed tests, PXTS has been shown to be consi...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Previous Page | Next Page