IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1740 documents. Displaying 25 entries per page.


Glued laminated poles - Progress report after 30 years testing
2010 - IRG/WP 10-20427
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and in a power lane in Vuollerim in northern Sweden in order to study their resistance against biological degradation. The tests have shown that the best performance will be obtained if each lamination is treated with a water-borne pre...
Ö Bergman, J Jermer


Measurements of rot fungal activity as a function of moisture content by isothermal calorimetry
2010 - IRG/WP 10-20428
Measurements of heat production rate have been made on wood samples with the brown rot fungus Postia placenta at different moisture contents. The results clearly indicate that the heat production rate (a measure of respiration rate and activity) is moisture dependent. When the moisture content is decreased, less heat is produced, and when the moisture content is increased, more heat is produced. I...
L Wadsö, A Pilgård, G Alfredsen


Simulation and Investigation of Wood Degradation by Erosion Bacteria in Laboratory Experiments
2010 - IRG/WP 10-20431
A Microcosm experiment was successfully set up to establish, monitor and manipulate bacterial wood degradation under low oxygen conditions. Sound pine sticks were placed in waterlogged sediment from a heavily decayed pine pile foundation site in Amsterdam. The system was subject to different gassing treatment regimes in order to investigate the role of oxygen in the bacterial degradation process o...
J Gelbrich, E I Kretschmar, N Lamersdorf, H Militz


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Detection of Wood Destroying Fungi Using DNA Microarray Technology
2010 - IRG/WP 10-20435
Wood decay fungi of the phylum Basidiomycota cause serious damage to wooden constructions and building elements. The elimination and the appraisement of fungal decay require an assured species identification. Conventional fungal diagnostics are mainly based on morphological characteristics by macro- and microscopy analysis. For some years, standardised and highly sensitive molecular methods focuss...
K Jacobs, N Rangno, W Scheiding, B Weiss, D Müller, C Hiller, W Brabetz


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


A Review on Conditions for Decay Initiation and Progression
2010 - IRG/WP 10-20444
This paper reviews the key publications available on service life prediction of exterior wood applications, critical conditions for decay initiation and progression, and the impact of decay on wood strength. While it is helpful to use climatic data to predict general trend of decay potential, more precise decay initiation and progression information is required by hygrothermal modeling for its dam...
Jieying Wang, P I Morris


Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves


Non-destructive evaluation of termite and decay damaged to timber-in- service
2010 - IRG/WP 10-20451
A leading joint research project was financed by the ARC, engaging some of the leading Universities in Australia, to look at field techniques to determine if timber-in-service is infested with termites and decay fungi after which microwave technology will be employed to eliminate the termites and/or decay in-situ. The next step will be to quantify the damage caused on the sectional dimensions of t...
C Adam, B M Ahmed Shiday, G Brodie


Development of microbiological test methods for the wooden packaging of foodstuffs
2010 - IRG/WP 10-20453
Whereas different sampling methods already exist for analysing contaminated surfaces or packaging made of plastic or paper, there is no methodology that enables the sampling and quantification of microorganisms in packaging made of wood. The objective of this study was to compare the most commonly used microbiological methods and to develop a reliable quality control test adapted to wooden packagi...
I Le Bayon, H Callot, M Kutnik, C Denis, A-M Revol-Junelles, J-B Millière, M Giraud, M Gabillé, N Passédat


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Comparison of Bifenthrin Formulations for Their Skin and Eye Irritation Potential Using the Pollen Tube Growth Test
2010 - IRG/WP 10-30521
The Pollen Tube Growth Test (PTGT) is an effective screening method for measuring the potential of a chemical formulation to affect living cells. The PTGT has been compared against other types of testing, and it shows a good correlation with, for example, the Draize rabbit eye test and the human skin patch assay. It measures the EC50, which is the effective concentration at which 50% growth is o...
S Millward, P Lobb


Biological performance of wood treated with tar-oil recovered during slow pyrolysis of macadamia nut shells
2010 - IRG/WP 10-30523
This study evaluated decay and termite resistance of wood treated with tar oil obtained from a commercial pyrolysis process of macadamia nut shells. Vacuum-treated pine wood specimens were subjected to various brown and white rot fungi based on the soil-block test method specified by the American Wood Protection Association (AWPA) after leaching process. Treated specimens were also subjected to th...
S Nami Kartal, E Terzi, C Kose, J Hofmeyr, Y Imamura


Use of Internal Remedial Treatment to Extend Wood Life at the Fort Vancouver National Historic Site
2010 - IRG/WP 10-30525
The condition of wood in a reconstructed fur trading fort was assessed over a 30 year period. Poor initial treatment had resulted in the development of extensive early decay. While supplemental treatment with chloropicrin and methylisothiocyanate had arrested the attack, the results suggested that remedial treatments were unable to completely overcome the initial problems associated with treatmen...
C S Love, C Freitag, J J Morrell


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Antifungal Essential Oil Metabolites
2010 - IRG/WP 10-30531
New environmentally-friendly wood protection systems based on “green” technologies are needed to inhibit wood-inhabiting mold and decay fungi. Utilizing bioactive essential oils from select herbaceous plants is one promising approach, but the concentrations of bioactive compounds are somewhat variable even in the highest (therapeutic) grade essential oils. Purified primary metabolites from fou...
C A Clausen, B M Woodward, V W Yang


The Effects of Some Fire Retardant Chemicals on the Decay Resistance of Medium Density Fiberboard (MDF)
2010 - IRG/WP 10-30536
The objective of this study was to determine the decay resistance of Medium Density Fiberboard (MDF) treated with 5% and 10% concentration of various fire retardant (FR) chemicals. Experimental panels were produced using by melamine-urea-formaldehyde (MUF) resins having 10%, 15% and 20% of melamine content. MDF specimens were subjected to decay resistance test performed according to modified EN 11...
D Ustaömer, M Usta, Ü C Yildiz, S Yildiz, E D Tomak


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Laboratory evaluation of borate amine: Copper derivatives in wood for fungal decay
2010 - IRG/WP 10-30543
The aims of this study were to evaluate borate: amine: copper derivatives in wood for fungal decay protection as well as the permanence of copper and boron in wood. Wood treated with each of four derivatives of borate:amine:copper prevented fungal decay. Disodium tetraborate ecahydrate (Borax):amine:copper derivatives with retentions of 0.61 to 0.63% after water leaching prevented decay by Gloeo...
G Chen


Preventing decay in termite monitoring stations
2010 - IRG/WP 10-30546
In-ground monitoring stations and termite baits are widely used in the southern United States with the intent of detecting and eradicating subterranean termite activity near buildings. These stations comprise a wood (or other cellulose material) substrate (monitor) and perhaps a termiticidal toxicant (bait) held in a plastic cage that allows for both easy examination and access by termites. The us...
A M Taylor, Jae-Woo Kim, S Duarte, L Nunes, J D Lloyd


Previous Page | Next Page