IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 462 documents. Displaying 25 entries per page.


A hypothesis on a second non-biocidal property of wood extractives, in addition to toxicity, that affects termite behavior and mortality
2008 - IRG/WP 08-10638
While it is has long been recognized that heartwood extractives affect termite behavior, the exact cause and relationship between total extractives, extractive types, and termite resistance remains unclear. Generally, researchers have proposed that the extractives are toxic and/or repel termites. We propose, based on the well known fact that many extractives have excellent antioxidant properties...
T P Schultz, K Ragon, D D Nicholas


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Whole-of-house protection from subterranean termite attack and damage after four years of field exposure
2008 - IRG/WP 08-10665
This study reports the condition of the whole-of-house termite protection test in tropical Australia after four years. The study was designed to provide maximum protection to whole-of-house timbers in a natural situation posing the highest hazard from subterranean termite populations. The houses were constructed either on concrete slabs or suspended floors using untreated and treated timber fram...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J Hann, C Y Adam


Field Liners as physical barriers to prevent wooden utility pole decay in soil: An accelerated field simulation trial
2008 - IRG/WP 08-20384
Field Liners (FL’s), plastic sleeves used to protect in-ground wooden poles from fungal and termite damage, have been tested before as physical barriers to prevent contact between soil and wood and to retain wood preservative treatment. These earlier studies concentrated mostly on creosote preserved poles and early generation FL’s which were cumbersome in their application. The newer generatio...
A R Howgrave-Graham, L J Cookson, T Hale


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Natural Durability Variations of Malaysian Timbers from Sarawak after 26 Years Exposure by Stake Test
2009 - IRG/WP 09-10704
An extensive graveyard stake test site was established in 1977 in Sibu, Sarawak, Malaysia, to evaluate the in-ground durability of 132 Sarawak wood species, mainly hardwoods. Test samples were planted at 100 x 50 cm spacing. Authenticated wood specimens from 3 trees of each of 132 species were processed into 20 replicated outer heartwood (or else undifferentiated heartwood) stakes of 19 x 19 x 457...
A H H Wong, Ling Wang Choon


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Laboratory and above ground exposure efficacy of silicon-boron treatments
2009 - IRG/WP 09-30510
The study deals with silicon compounds, namely tetraethoxysilane (TEOS), phenyltriethoxysilane (PhTES) and methyltriethoxysilane (MTES) at concentrations of 23, 16 and 10% in combination with 1.2-1.5% boric acid. The aim with the study was to combine the chemical approach with the necessary biological tests of the impregnated wood. The tested silicon-boron combinations ensured mass loss less than ...
N Terziev, D Panov, A Temiz, S Palanti, E Feci, G Daniel


Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal


Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Ecological methods and products for wood protection used for restoration and conservation of built heritage cultural assets to increase natural durability and duration of exposure in open air museums
2010 - IRG/WP 10-40506
Wood is a perishable material, hygroscopic and fuel, which cause attention to selecting the wood species that is going to be exhibited in relation to humidity and soil. With variable depending on its humidity and moisture from the atmosphere or soil, wood is a good living environment for fungi and insects, but suffer biodegradation processes and dimensional changes. Observations over time on wood ...
M Pruna, D Purice, D Dumitru Copacean


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Quantitative design guideline for wood outdoors above ground applications
2011 - IRG/WP 11-20465
This paper describes the background and principles behind an engineering design guideline for wood in outdoor above ground applications, i.e. use class 3 according to EN 335. The guideline has been developed in the European research project WoodExter and can be seen as a first prototype for a quantitative design tool in the area of wood durability. It is based on a defined limit state for onset of...
S Thelandersson, T Isaksson, E Suttie, E Frühwald, T Toratti, G Grüll, H Viitanen, J Jermer


Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses new fixation systems based on bio-materials and presents up to five year outdoor exposure testing on full-size decks. Generally, the new f...
C R McIntyre, M A Lake


Previous Page | Next Page