IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1628 documents. Displaying 25 entries per page.


Antifungal properties of metabolites produced by Trichoderma isolates from sawdust media of edible fungi against wood decay fungi
1994 - IRG/WP 94-10051
Trichoderma isolated from a sawdust medium of Pholiota nameko produced filtrates which had antifungal activities to four wood decay fungi tested on the agar plates. Filtrates produced from another isolate, from a sawdust medium of Lentinus edodes, had antifungal activities only to the white rot fungi, Coriolus versicolor and Pycnoporus coccineus. These results did not agree with those from earlier...
S Doi, M Mori


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


The use of propionic acid to prevent Pinus patula biodeterioration during outside chip storage in Zululand
1989 - IRG/WP 3531
Pinus patula SCHIEDE ET DEPPE IN SCHLD. ET CHAM. is susceptible to biodeterioration during outside chip storage (OCS), reducing pulp quality and tear and burst indices of resulting paper. Accelerated laboratory trials showed that chips treated with 2% (w/v) propionic acid and stored for 17 weeks, produced pulp of quality indistinguishable from fresh untreated chips. Pulp tests during field trials ...
S Ismail, E J Smith, A A W Baecker


Silafluofen, a new insecticide against wood-boring insects and termites
1991 - IRG/WP 3666
Hoe 084498 (proposed common name: Silafluofen) is a new insecticidal compound from Hoechst Aktiengeesellschaft and has been extensively tested to determine its potential use as an insecticide against wood-boring insects and soil termites. Various tests in official institutes indicate a good activity against several wood-boring insects and soil termites. The active ingredient is resistant to weathe...
G Rustenburg, C J Klaver


Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole. On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built. On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


Laboratory evaluation of potential antisapstain treatments for Pinus radiata
1983 - IRG/WP 3237
Twelve formulations were tested in the laboratory using a 'mini' board test for effectiveness on Pinus radiata (D. Don) against sapstain, mould and decay fungi. Three formulations, sodium pentachlorophenoxide (NaPCP) plus borax, Haipen 50 WP, and Mitrol 375, are used commercially in New Zealand. Busan 1009 (0.5% product), IWD Product A (0.2% ai), IWD Product B (0.3% ai), Fennotox...
J A Drysdale


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


The effect of precolonisation of blocks with common pole resident fungi on subsequent biological control of Lentinus lepideus by Trichoderma spp
1989 - IRG/WP 1387
Results of previous field studies have indicated that the spread of Trichoderma throughout the groundline regions of the interiors of creosoted poles are adversely influenced by the presence of large populations of resident mould organisms. Failure of the control fungus to develop and colonize all of the decay susceptible groundline region means that sucessful control of decay is most unlikely. Th...
A Bruce, T L Highley


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Laboratory and field evaluations of a novel formulation, BAM as an anti-sapstain agent
1991 - IRG/WP 3639
A novel anti-sapstain formulation, BAM, consisting of 2-(thiocyanomethylthio) benzothiazole (TCMTB) and methylene bis thiocyanate (MBT) was evaluated for ist anti-sapstain performance in the laboratory and in the field as well. BAM proved effective in controlling the growth of molds and a sapstaining fungus in the standardized Japan Wood Preserving Association (JWPA) tests. All the test fungi coul...
Y Nomura


Feasibility of using biological control agents to arrest and prevent colonization of Douglas fir and southern pine by decay fungi
1988 - IRG/WP 1345
The use of microfungi to control basidiomycetous decay has been evaluated in Europe for many years, where it has produced mixed results against Lentinus lepideus Fries, the fungus presumed to be the major cause of decay in Scots Pine poles. In the United States, remedial decay control has been largely chemical, with little use of alternative decay control strategies. Increasing restrictions on che...
J J Morrell, C M Sexton


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


Invasion and colonisation of bamboo culm material by stain and decay fungi
2002 - IRG/WP 02-10453
Two distinct stages of the fungal infection of bamboo culms can be identified: entry into the culm itself (invasion) and further colonisation by spread within the culm wall tissue. This laboratory study aimed to characterise different invasion strategies of a variety of fungi. Well-known isolates of white- (Coriolus versicolor, Schizophyllum commune), brown- (Coniophora puteana, Gloeophyllum tra...
G Kleist, I Morris, R J Murphy


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka


A survey of the incidence of decay in copper-chrome-arsenate treated trellis support posts used in horticulture in New Zealand
1984 - IRG/WP 1225
Copper-chrom-arsenate treated softwood posts used as trellis support structures in 5 major horticultural districts of New Zealand were systematically examined for presence of decay. Principal crops on properties examined were grapes and kiwifruit; a minority of properties grew hops, boysenberries, and dwarf apples. Occurrence and severity of decay were variable within specific age classes of posts...
M E Hedley, J A Drysdale


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


Previous Page | Next Page