Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Potential for migration of boron from fused boron rods used as internal remedial treatments of utility poles
2014 - IRG/WP 14-50301
The distribution of boron in Douglas-fir utility poles and in the surrounding soil was assessed over a 54 month period following application of fused boron rods. Boron levels in the wood never reached the levels that might be predicted if diffusion were to produce a uniform chemical distribution, nor did levels in the soil suggest that boron was becoming more concentrated. The results suggest th...
M Konkler, C Freitag, C S Love, J J Morrell, J Renfroe


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Biological Performance of Triadimefon in combination with Tebuconazole in laboratory and field tests
2015 - IRG/WP 30668
The usage of Triazole-combinations for wood preservatives is common practice in several countries. Especially the combination of Tebuconazole and Propiconazole is preferred for this application due to its broad spectrum of efficacy against wood destroying fungi. 1-(4-Chlorphenoxy)-3,3-dimethyl-1-(1,2,4-triazol-1-yl)-butanon, also known as Triadimefon provides a good efficacy against the wood destr...
P Meckler, T Jaetsch


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker


Laboratory evaluations of woods from Pakistan and their extractives against Postia placenta and Trametes versicolor
2016 - M Mankowski, B Hassan, A Bishell, G Kirker
Natural durable wood species are those which exhibit innate tolerance to wood decay organisms such as fungi and termites. The goal of this study was to evaluate 4 wood species (Dalbergia sissoo, Cedrus deodara, Morus alba and Pinus roxburghii) from Pakistan in order to determine their resistance to both a model brown (Postia placenta) and white (Trametes versicolor) rot fungus compared to a durabl...
M Mankowski, B Hassan, A Bishell, G Kirker


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Evidence for a role for precipitated copper on the chemistry of micronized copper treatments
2016 - IRG/WP 16-30690
Micronized copper preservative treatments of softwoods, result in mobile copper being formed by reaction of the basic copper carbonate (BCC) with the carboxylic acid functional groups in hemicellulose and pectic substances present in wood. Typically, the amount of reacted copper formed is approximately 0.3% Cu m/m. In this paper, two examples are discussed where remaining unreacted basic copper ca...
Wei Xue, P Kennepohl, J N R Ruddick


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


A Case Study of Long-term CCA Preservative Leaching from Treated Hardwood Poles in a Humid Tropical Condition
2016 - IRG/WP 16-50324
Chromated copper arsenate (CCA)-treated Malaysian hardwoods have long been used as utility poles, posts, construction piles and motorway fencing in soil contact exposed to the threats of decay fungi and termites. Despite global concerns citing predominantly temperate conditions of long-term leaching of CCA toxic heavy metals from wood into surrounding soils and groundwater since the 1990’s, the ...
A H H Wong, W S M Chin


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Redwood Durability in NZ – Can pure culture laboratory tests predict outdoor service life
2017 - IRG/WP 17-20610
Coast Redwood (Sequoia sempervirens) is an alternative species in New Zealand to the large scale Pinus radiata plantations. Redwood is classified as moderately durable but its durability is extremely variable. In order to reduce this variability in future stock, understanding growth conditions, clone, and tree age effects are important however this involves many samples and is not suitable for ass...
D O’Callahan, C Chittenden, J van der Waals, D Meason, T Singh


Monitoring Diversity and Colonization Patterns of Wood-Inhabiting Fungi Using Field Stake Tests
2017 - IRG/WP 17-20614
Advances in molecular identification of microbial communities enabling rapid microorganism determination have allowed ecological data to be increasingly incorporated into standardized wood performance tests. Combining standard field tests with molecular methods to study wood-associated microflora can help to better understand fungal colonization and decay processes of wood in service. The potentia...
P Torres-Andrade, J Cappellazzi, J J Morrell


Activity of Two Strobilurin Fungicides Against Three Species of Decay Fungi in Agar Plate Tests
2017 - IRG/WP 17-30704
The objective of this study was to examine the toxicity of strobilurin fungicides against wood decay fungi in order to assess their potential to act as a co-biocide for copper-based wood protection. Two strobilurin fungicides, Heritage (50% azoxystrobin active ingredient) and Insignia (20% pyraclostrobin active ingredients), and copper sulfate pentahydrate were tested against one white rot fungus...
J D Tang, T Ciaramitaro, M Tomaso-Peterson, S V Diehl


Hybrid green composites manufactured with glass fiber and jute fabric skin by VARTM process: Fungal, mold, and termite resistance tests
2017 - IRG/WP 17-40780
Hybrid green composites are increasingly used in building applications due to the development of new production approaches. Biological performance of such composites is needed when they are employed in extreme conditions. Hybrid composite panels were manufactured by wood furnish, glass fiber, and jute fabric skin by the vacuum assisted resin transfer molding (VARTM). Petri dish test method was fol...
S N Kartal, E Terzi, M Muin, A H Hassanin, T Hamuoda, A Kilic, Z Candan