Commercial potential of the four-cycle method for the impregnation of green beech sleepers in Yugoslavia
1975 - IRG/WP 347
This paper was presented to the Conference on Wood Protection held in Sarajevo (Yugoslavia) in 1973. The paper was based partially on the report prepared by J. Struhar and G. F. Franciosi, who were appointed in 1972 as FAO consultants to demonstrate the new impregnation process for green beech sleepers in Yugoslavia. The so-called 4-cycle method was developed at the State Forest Research Institute...
N Vidovic


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


Studies on the mobility of arsenic, copper and chromium in CCA-contaminated soil
1990 - IRG/WP 3571
CCA contaminated soils from six Swedish preservation plants were investigated primarily to study the mobility of arsenic but also that of copper and chromium in the soils. The soil samples represented average types with different amounts of clay, organic matter, arsenic, copper, chromium and different pH. The total soluble amounts of the elements were measured. The pH dependent solubility and the ...
J Bergholm


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


A method for the preliminary assessment of timbers for their treatability with preservatives under pressure
1977 - IRG/WP 3100
President Maurice Fougerousse has provided the following references to a IUFRO report, published in English, French and German, which may be of interest to IRG members: 'A method for the preliminary assessment of timbers for their treatability with preservatives under pressure', PANS Vol 23, No 2, 153 158, June 1977. 'Une methode d'evaluation preliminaire de l...
M Fougerousse


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Possibilities of improving the oscillating pressure method
1991 - IRG/WP 3668
Studies on the dynamics of pressure changes in wood during impregnation revealed no significant effect of fast pressure changes for green spruce as used by OPM (IRG/WP/3615). The following experiments were carried out on several hundreds of spruce palisades to examine the modification of single procedure parameters of common use OPM and to record the effects on the impregnation result with the aim...
S Goetsch, R-D Peek


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


A rapid method for collecting large numbers of subterranean termites from wood
1982 - IRG/WP 1165
A corrugated fiberboard trap is described which attracts large numbers of subterranean termites from infested logs. Single-trap collections in excess of 63 grams (wet wt.) for Reticulitermes virginicus (Banks) and 43 grams for Coptotermes formosanus Shiraki were taken one to three days following discovery by termites. If traps are removed from the source logs shortly after beeing attacked, termite...
J P La Fage, N-Y Su, M Jones, T Lawrence


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


Report on the co-operative leaching tests
1975 - IRG/WP 246
The Work reported here was undertaken at the request of CEN to see (1) whether the standard beaker leaching method under discussion at CEN, and based on the German DIN could be made less labour intensive; and (2) whether the leaching parameters could be expressed in more general terms so that alternative procedures could be used. A co-operative experiment was set up in which the amount of leaching...
J W W Morgan