Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Notes on the resistance of tropical woods against termites
1985 - IRG/WP 1249
This paper deals with a descriptive account on the effect of experimental methods, matrix, species of termites, solid wood and wood extract on the resistance and repellency of woods against three species of termites, i.e. Cryptotermes cynocephalus Light; Coptotermes curvignathus Holmgren and Reticulitermes lucifugus (Rossi). Two methods of experiment were used, the Forced Feeding Test and the Feed...
Nana Supriana


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Resistance of painted pine sapwood to mould fungi. Part 1. The effect of waterborne paints and fungicides on mould growth
1997 - IRG/WP 97-10233
The efficacy of different fungicides in acrylate and alkyd paints to protect pine sapwood against mould fungi was studied. The acrylate and alkyd paint systems with and without a preservative dipping treatment prior to painting were also used. Differences in the efficacy of the fungicides to protect the paint film were found. The paint films with isothiazolon and IBPC were resistant against mould ...
H Viitanen, P Ahola


Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


Theoretical and practical experiments with eradication of the dry rot fungus by means of microwaves
1992 - IRG/WP 92-1577
Engineer Claus Andersen constructed a device in 1986 for microwave treatment of fungal infested timber. The device was tested on ampullae with live fungal mycelium of the dry rot fungus. A 10 minutes treatment at 37°C gave satisfactory eradicating effect. The method has since been used in practice in approximately 100 instances. A spot-test control has shown satisfactory results....
J Bech-Andersen, C Andersen


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycetes
2001 - IRG/WP 01-10397
Lyophilization is an excellent technique for the long-term preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycotina. However, vegetative mycelial isolates are not lyophilizable. In this study, 10 brown-rot and 10 white-rot basidiomycetous non-sporulating, non-chlamydosporulating, and non-bubillerferous basidiomycetes fungi were tested for viability after lyophilization. ...
S C Croan


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


Documentation on Merulius (Serpula) lacrimans (Wulf.) Fr. according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1972 - IRG/WP 108
J Segmüller, O Wälchli


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Isolation of the dry rot fungus, Serpula lacrymans, from the forests of the Himalayan Foothills
1995 - IRG/WP 95-10129
Previous expeditions to the Himalayas (Singh 1993, 1994) have reported on the presence in this area of the dry rot fungus Serpula lacrymans. However, attempts to isolate the organism from material brought back from these expeditions were not successful. In this paper we report on the isolation of Serpula lacrymans from spores and cord material brought back from the Narkanda region of the Himalayas...
N A White, J W Palfreyman, J Singh, S Singh


Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris


The dry rot and other fungi in houses. Part 4
1995 - IRG/WP 95-10124
J Bech-Andersen


Ibuprofen inhibits in vitro growth of brown-rot fungi
1996 - IRG/WP 96-10160
Ibuprofen, a phenyl propionic acid derivative (2-(4-isobutylphenyl)propionic acid) inhibited growth in vitro of 17 brown-rot fungi at a concentration of 100 µg/mL, while exhibiting no growth inhibition for 8 white-rot fungi at the same concentration. Propionic acid did not inhibit fungal growth in vitro. Morphological changes were noted in fungi that were able to grow in the presence of ibuprofen...
C A Clausen


Analysis of volatile emissions as an aid in the diagnosis of dry rot
1992 - IRG/WP 92-2393
The dry rot fungus, Serpula lacrymans was grown in pure culture on malt extract and on sapwood of pine. The volatile compounds emitted from the cultures were determined by diffusion sampling on tubes filled with Tenax TA, thermal desorption and gas-chromatography-mass-spectrometry in order to find markers for attack of the fungus....
J Bjurman, J Kristensson


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel


The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Monographic information on Lentinus lepideus.markup
1973 - IRG/WP 115
W Liese, G Seehann


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...