A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Evaluation of Five Novel Organotin(IV) Complexes as Wood Preservatives
2012 - IRG/WP 12-30590
Three selected non durable tropical wood species namely Alstonia scholaris (pulai), Macaranga triloba (mahang) and Hevea brasiliensis (rubber) were chemically impregnated with five novel organotin(IV) complexes using vacuum-pressure treatment method. The objectives of this study were to determine the treatability and efficacy of novel organotin(IV) complexes against white and brown rot decay fungi...
M M Rahman, I Jusoh, M A Affan, A Husaini


Antifungal activities of acetone-soluble Eusideroxylon zwageri and Potoxylon melagangai crude extracts against white rot
2012 - IRG/WP 12-30591
The development of natural wood extracts as a wood preservative is a potentially attractive prospect for the wood preservation industry. This study attempts to evaluate the toxicity of Eusideroxylon zwageri and Potoxylon melagangai extractives as potential wood preservatives. These two species are well-known as among the heaviest and very durable timbers. It has been established that natural durab...
I Jusoh, A Tida Henry, Z Assim, F Badruddin Ahmad, S Ujang


The resistance of thermo and thermo-oil modified black poplar wood (Populus nigra L.) to Basidiomycetes fungi
2012 - IRG/WP 12-40585
The share of area taken by poplar tree species in Poland account for 2.0% of the area of state forests, 4.8% of national parks and for 2.3% in the privately-owned forests. It is shown and expected an increase in the share of poplar stands connected with plantation of fast growing trees. The poplar wood is not resistant to Basidiomycetes fungi, easy attacked by insects and in consequence is regarde...
A Fojutowski, A Kropacz, A Noskowiak


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


The activity of a wood-decaying fungus during drying and rewetting cycles measured by isothermal calorimetry
2013 - IRG/WP 13-20526
Wood decaying fungi are an essential part of any ecosystems as they are the main decomposers of cellulose and lignin-containing materials. But as wood is a common building material the risk for decay fungi growth and subsequent degradation of our construction material is a concern. There are important physiological aspects of the growth and activity of decay fungi that are unknown today, and witho...
S Johansson, L Wadsö, A Pilgård, G Alfredsen


Effect of biodiesel on Performance of Isothiazolone
2013 - IRG/WP 13-30625
Biodiesel has a number of attractive properties, including the ability to readily solubilize a number of biocides and a tendency to reduce odors associated with other solvents such as petroleum-based diesel. Biodiesels, however, have also been implicated in reduced performance of some, but not all preservatives. It is important to assess the effects of biodiesel on each biocide. Soil block tests ...
Cheng Hua-Kang, L Jin, C Freitag, J J Morrell


CT scanning of decay in creosoted poles for overhead lines
2013 - IRG/WP 13-30634
Creosote-treated poles have been examined by means of CT scanning in order to investigate the nature of soft spots that have been found more frequently during the last five years in Sweden. CT scanning provides a very good picture of the interior of the poles and decay can easily be detected. It was concluded that the soft spots in most cases were caused by decay which in turn had to do with extre...
C-J Johansson, A Clang, I Johansson, G Berggren


Investigations concerning liquid absorption of six heartwood species
2013 - IRG/WP 13-40618
In order to determine the liquid absorption and the penetration different heartwood species were treated with a boric acid containing solution. Heartwood of six wood species (Fir, Spruce, Douglas fir, Scots Pine, Oak and Black locust) were used in these investigations whereby the dimension corresponds to the EN 252 format. One half of the stakes were end sealed before treatment. All stakes were im...
E Melcher, J Zwiefelhofer


Postia placenta cellulase gene expression in modified wood during incipient decay
2013 - IRG/WP 13-40626
In optimization of modified wood, it is important to understand the mode of action of the wood modification and how the fungi response to it. The aim of this study was to investigate the expression of cellulases during the first two weeks of Postia placenta exposure in acetylated, DMDHEU-treated and thermally modified as well as in untreated wood. Using real-time PCR, the gene expression patterns ...
R Ringman, A Pilgård, K Richter


Effect of electron beam irradiation on the fire retardant penetration into wood
2013 - IRG/WP 13-40642
Electron beam processing which can fast and easy change the nature of the material has received considerable attention recently. Studies using electron beam has been conducted in various fields and it has been applied in many industrial sectors. Electron beam has higher energy than other electromagnetic waves. It has excellent object permeability. It affects degradation of intermolecular cross-lin...
Dong won Son, Jong Sin Lee, Mee Ran Kang, Sang Bum Park


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


The effects of copper proximity on oxalate production in Fibroporia radiculosa
2014 - IRG/WP 14-10823
Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess d...
K M Jenkins, C A Clausen, F Green III


Protein extraction from wood decay fungus Postia placenta
2014 - IRG/WP 14-10827
Wood decay fungi (often distinguished as white rot and brown rot) belonging to the basidiomycetes, are common inhabitants of forest litter, where they play an important role in carbon cycling. Brown rot fungi are perhaps the most important organism involved in the degradation of wood products, and of considerable economic importance. Brown rotted wood loses strength very early because of the rapid...
A Pilgård, P Arnold, K Richter


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao