Influence of a dipping preservative treatment on the performance of wood finished with waterborne coatings
1998 - IRG/WP 98-40121
Within a larger European research project on the performance of joinery finished with waterborne coatings, the influence of a water based dipping preservative treatment was studied in several ways. Six different waterborne coatings were tested with and without a preservative underneath the coating. The performance was tested on pine sapwood and spruce panels in a 2-year outdoor weathering trial on...
M De Meijer, J Creemers, W Cobben, P Ahola


First draft of a monographic card for Gloeophyllum abietinum (Bull. ex Fr.) Karst
1973 - IRG/WP 116
T Hof


Effects of the addition of polyethylene glycol to the CCA-C preservative treatment
1985 - IRG/WP 3337
A modification of the CCA-C wood preservative system for utility poles has been investigated to see if spur penetration into the poles is assisted during climbing. Addition of polyethylene glycol to the CCA system has been shown to accomplish this purpose. This paper addresses the effects of the addition of polyethylene glycol to other physical properties germane to utility poles....
W P Trumble, E E Messina


Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


A behaviour of CCA penetration of fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications
2006 - IRG/WP 06-40346
A behaviour of CCA penetration of Bornmulleriana fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications was illustrated for the main flow directions by the experimental pictures....
I Usta, R Despot, M Hasan


Chapter 9 - Preservation of borak bamboo
2007 - IRG/WP 07-10635-09
Adequate penetration and retention of CCA and CCB have been obtained in pre-dried Borak bamboo (Bambusa balcooa Roxb. See Fig. below), abundantly grown in Bangladesh, with full-cell pressure process. The treated bamboo can be used as building materials; the sufficient treatability ensured its long-term best utilization at ground contact and indoors. This will keep the environmental and socioe...
A K Lahiry


On the Influence of Wood Destroying Fungi on the Feeding Intensity of Termites
2017 - IRG/WP 17-10893
The baiting and feeding stimulating effect of wood attacked by fungal isolates of the species Coniophora, Lentinus, Poria and Gloeophyllum on termites Reticulitermes santonensis is examined. There are significant relationships between the activity of fungal isolates and the feeding behaviour of termites. The most active isolates can be used for increase the attractiveness of wood to wood-destroyin...
W Unger, T L Woods


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


The distribution of introduced acetyl groups and a linseed oil model substance in wood examined by microautoradiography and ESEM
2000 - IRG/WP 00-40169
Microautoradiography, a photographic method that shows the localization of substances labelled with radioactive isotope, and Environmental Scanning Electron Microscopy (ESEM) were combined to enhance sensitivity, resolution and reliability for examination of the distribution of introduced substances in wood. The preparation of microautoradiographs is less complicated when investigated with ESEM an...
M Rosenqvist


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Sterilization of mango wood (Mangifera indica L.) without heat
1995 - IRG/WP 95-30065
Researches revealed that boric acid can play an important role for sterilizing wood instead of heating. Wet (green) mango boards (Mangifera indica L.) were pressure treated in treating cylinder at initial vacuum of 508 mm Hg for 15 minutes and impregnation pressure of 7 kg/cm² for 4 hours with 5% solution (w/v) of 1:1:1 commercial grade (95% pure) sodium dichromate, copper sulphate and boric acid...
A K Lahiry


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Oxalate production and calcium oxalate accumulation by Gloeophyllum trabeum in buffered cultures
1994 - IRG/WP 94-10075
Most basidiomycetous fungi produce oxalic acid as a result of their metabolic activities and nutrient procurement. There is currently a renewed interest in the role that oxalic acid may play in the decomposition of wood by basidiomycete fungi. It has been observed that although most wood degrading fungi have the capacity to produce oxalic acid, not all of these organisms express this capacity equa...
J H Connolly, J Jellison


Identification of terminal structures in cellulose degraded by the brown-rot fungus Postia placenta
1989 - IRG/WP 1389
To gain insight into the biochemical mechanism employed by brown-rot fungi to depolymerize cellulose, we identified the end-groups of chemically pure cellulose that had been depolymerized by the brown-rot fungus, Postia placenta. The depolymerized cellulose was acid hydrolyzed and the anion fractions isolated by ion chromatography. Sugar acids were identified by gas chromatographic and mass spectr...
T K Kirk, T L Highley, R E Ibach, M D Mozuch


Biosynthesis of ß-Glucan microfibrils by cellular fractions from brown-rot fungus Postia placenta (MAD-698 and ME-20) and white-rot fungus Schizophyllum commune (MAD-619)
1993 - IRG/WP 93-10025
In this study, we compared the brown rot fungus Postia placenta (MAD-698 and ME-20) with the white rot fungus Schizophyllum commune (MAD-619) to determine the location and distribution of glucan synthetase. We also measured the soluble protein content in subcellular fractions obtained by differential centrifugation MAD-698 is a degradative isolate, but ME-20 and MAD-619 do not produce significant ...
S C Croan, T L Highley


Durability of plywood made from soft- and hardwoods assessed according to ENV 12038 after artificial and natural ageing
2000 - IRG/WP 00-20191
Plywood was prepared from Norway Spruce and pure heartwood of Douglas Fir, Scots Pine, European Oak, False Acacia and Macoré using a phenol-formaldehyde glue. The panels of 38 mm in thickness were pre-conditioned according to the following procedures: a) 12 weeks storage at 20°C/65% rh, b) 2 weeks artificial weathering (with rain and UV-radiation at changing temperatures), and c) a natural weath...
H Leithoff, R-D Peek