IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1387 documents. Displaying 25 entries per page.


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Effect of wood species on decomposition efficiency of metham sodium
1992 - IRG/WP 92-3699
The effect of wood species and temperature on efficiency of metham sodium (32.1% sodium N-methyldithiocarbamate) decomposition to methylisothiocyanate (MITC) was investigated on 10 hardwoods and 9 conifers over a 144 hour period. Gas chromatographic analyses of headspace samples and ethyl acetate extracts of the wood revealed that decomposition never approached the theoretical decomposition effici...
J J Morrell


Immunolocalization of xylanase produced by Clostridium xylanolyticum Rogers and Baecker during anaerobic decay of Pinus patula
1991 - IRG/WP 1505
The xylanolytic fraction from a 72h culture of Clostridium xylanolyticum ROGERS and BAECKER was separated using non-denaturing PAGE and then used to raise polyvalent antisera in rabbits. Antibodies were purified using an affinity gel column and coniugated with colloidal gold. Pinus patula was exposed to axenic cultures of Clostridium xylanolyticum for 3 weeks, fixed, embedded and converted to ultr...
A A W Baecker, G M Rogers


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


Effect of mini-block test conditions on activity of Coniophora puteana
2000 - IRG/WP 00-20184
The influence of various factors of the mini-block test method on growth and activity of different strains of Coniophora puteana was studied. Decay rates of spruce samples in Petri dishes of different depths, at different wood fibre orientations and at various distances between growth medium and wood were compared. In deep Petri dishes, there were no significant differences between activity of the...
F Pohleven, M Petric, J Zupin


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


Previous Page | Next Page