Your search resulted in 1416 documents. Displaying 25 entries per page.
Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund
Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman
Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson
Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki
Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto
Improved techniques designed for evaluation of fungicides in soil for control of dry rot fungus Serpula lacrymans
1985 - IRG/WP 2238
Improved techniques provide a laboratory method for the evaluation of chemicals in soil for control of dry rot fungus Serpula lacrymans. Results with their application to three chemicals were reported. These techniques are useful to eliminate chemicals lacking the necessary toxicity and weatherbility for dry rot control when the chemicals have been applied to the soil....
M Takahashi, K Nishimoto
Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey
The restricted distribution of Serpula lacrymans in Australian buildings
1989 - IRG/WP 1382
Temperature data has been gathered over a number of years, not only for flooring regions of various buildings in Melbourne, but also within roof spaces and external to the buildings. Findings are discussed in relation to the distribution of Serpula lacrymans within Australia, its restriction to certain types of building construction and its restriction to flooring regions. The subfloor spaces of b...
J D Thornton
How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent.
The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen
Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot
On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald
Additions and corrections to recent names for some common decay fungi
1977 - IRG/WP 167
A Käärik
A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker
Laboratory decay test of Burmese in and kanyin treated with three wood preservatives
1982 - IRG/WP 3210
Laboratory decay tests were performed on samples of In (Dipterocarpus tuberculatus Roxb.) and Kanyin (Dipterocarpus alatus Roxb. and Dipterocarpus turbinatus Gaertn f.) pressure treated with three wood preservatives - copper arsenic additive (CAA - a variation of ammoniacal copper arsenate), Arquad C-33 (a waterborne quaternary ammonium formulation), and tributyltin acetate (TBTA) dissolved in eth...
J N R Ruddick, R S Smith, A Byrne
Studies on accelerated ageing procedures with TBTO-treated wood
1985 - IRG/WP 2244
The efficacy of various procedures for accelerated ageing of organotin based wood preservatives in treated wood has been investigated. It was found that leaching of the treated wood samples in water according to the European Standard EN 84 was not satisfactory for organotin based preservatives and is probably also unsuitable even for other types of organic solvent preservatives. Keeping tributylti...
J Jermer, M-L Edlund, B Henningsson, W Hintze
Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller
Effect of medium-term degradation of beech wood by erosive (Phanerochaete chrysosporium) and lignin-selective (Ceriporiopsis subvermispora) strains of white rot fungi on its selected physical properties
2004 - IRG/WP 04-40292
At the Faculty of Wood Sciences and Technology a fungal delignification of normal and tension beech wood by erosive and lignin-selective strains white-rot fungi has been studied. The pre-treatment of both kind of wood samples was accompanied by partial delignification and apparent changes of their physical properties influencing the polar liquids penetration....
R Solár, S Kurjatko, M Mamonová, J Hudec
A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada
Successive collections of Basidiospores from wood decay fungi (in vitro) show variation in germination levels on common media
1978 - IRG/WP 191
In the course of various preliminary experiments in which spore germination levels of 6 decay fungi on malt and water agar were recorded as controls, it was noted that one could not reliably obtain an expected level of spore germination for any particular fungus. Inconsistent 'control' spore germination levels of a fungus greatly complicates large scale experiments in which compa...
E L Schmidt, D W French
The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker
Respiration methods used to follow the decay of wood and the toximetric evaluation of wood preservatives
1975 - IRG/WP 249
When wood is attacked and decayed by fungi, wood substance and oxygen (02) are consumed, while carbon dioxide (CO2), water and heat are liberated. Early in the 1960's workers from England, Canada and Sweden began studying CO2 evolution, with respect to decay and its control using chemical preservatives, while in Germany and the USA O2 utilization was being similarly examined. Oxygen consu...
R S Smith
In-ground performance of two formulations of chlorothalonil after five years of exposure at three test sites in Australia
1996 - IRG/WP 96-30101
Sapwood specimens of Pinus radiata D. Don and Eucalyptus regnans F. Muell. were each treated to three retentions of each of two preservative formulations (chlorothalonil in oil; chlorothalonil plus chlorpyrifos in oil) and installed in-ground at three field test sites in Australia. Specimens were treated with each formulation to achieve 3.2, 6.4 and 12.8 kg/m³ of chlorothalonil a.i. and 3.2 + 0.2...
J W Creffield, T L Woods, N Chew
Valid names for some common decay fungi, their synonyms and vernacular names
1978 - IRG/WP 172
A Käärik
Influence of aliphatic acids on spore germination of wood decay fungi
1984 - IRG/WP 2224
Influences of eight saturated fatty acids (C5-C10, C12 and C16) on spores of four isolates of wood decaying basidiomycetes (white rot fungi: Poria tenuis and Trametes hispida; brown rot fungus: Gloeophyllum trabeum [two isolates]) were observed in-vitro. Spore response after 24 hr on malt extract agar containing 10, 10² , or 10³ ppm of each fatty acid included: no effect on normal germination, d...
E L Schmidt
An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong