Proposal for a method aiming at the quantification of the impact of wood extraction in Life Cycle Assessment
1998 - IRG/WP 98-50113
Life Cycle Assessment has been accepted as an instrument for the assessment of the environmental impact of products. Characterisation factors for impact assessment of emissions from products have been established. To date no characterisation factor exists for the extraction of biotic resources, for example wood. Since the main disadvantage of using wood as a material lies in the extraction of reso...
P Esser, E Van der Voet


Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


Screening test methods with termites as first laboratory evaluation of new active substances for wood preservation
1995 - IRG/WP 95-10135
European test methods (EN) with termites have been compared with long-standing experience from screening test methods in the laboratory of Eberswalde. The results are discussed in terms on the possibility of using screening test methods as the first laboratory evaluation of new active substances in wood preservatives. The advantages and disadvantages of these methods are considered. Only a small a...
W Unger


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Preliminary agar screening studies as the first stage in the development of a biological control system against basidiomycetes in ground contact situations
1995 - IRG/WP 95-10111
Preliminary screening of Trichoderma isolates as possible biocontrol agents for protection of wood in ground contact situations against basidiomycete decay was undertaken on three types of media. Media used were 3% malt extract agar (MEA); a low nutrient synthetic media with a carbon: nitrogen ratio typical of that found in softwoods (LNM); and a similar synthetic media where the amino acid profil...
E J B Tucker, A Bruce


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Screening of fungal strains for wood extractive degradation
1998 - IRG/WP 98-10254
Fungal strains were screened for their ability to degrade apolar extractives in wood from scots pine. The degradation of total wood extractives by 91 different strains was monitored in stationary batch assays incubated for 6 weeks. The results obtained show that the ability of wood-inhabiting fungi to utilize wood extractives varied greatly, even for different isolates of the same species. Fungal ...
J Dorado, M J Martinez-Inigo, T A van Beek, F W Claassen, J B P A Wijnberg, R Sierra-Alvarez


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


Copper tolerance of various Antrodia vaillantii isolates
2001 - IRG/WP 01-10406
Copper based preservatives have been extensively used in the field of wood preservation. However, several brown-rot fungi to be tolerant to copper and consequently, efficacy of copper based wood preservatives may not be sufficient. Copper tolerance is especially by some fungi that are closely aligned to or included in genus Antrodia. The highest copper tolerance was found at some strains of wood r...
F Pohleven, A Malnaric, M Humar, C Tavzes


A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Acoustic technique for assessing decay in preservative treated wood
1998 - IRG/WP 98-20138
This study investigated the suitability of vibration techniques to assess the performance of wood preservatives in ground contact. Small stakes (10 x 5 x 100 mm3) of treated and untreated Scots pine sapwood were exposed to decay in lab-scale terrestrial ecosystems. Tests were conducted using three different soils including a garden compost soil, and soils obtained from a test field and a conifer f...
L Machek, M-L Edlund, R Sierra-Alvarez, H Millitz


Influence of the nature of the substrate and the method of inoculation on the degradative activity of soft rot fungi
1998 - IRG/WP 98-20133
The European Standard (ENV-807) determines the threshold of effectiveness of wood preservatives against the action of soft rot Ascomycetes fungi. Its application in the treatment of wood used in the hazard class 4 does not always offer repeatable results, which could be expected in an experimental norm. For this reason, in this paper, we have evaluated the diverse variables that might influence t...
M T De Troya, A M Navarrete, F Rubio, J Jiménez, D Muñoz-Mingarro, C Rodríguez-Borrajo, F Llinares, M Yuste


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


Changes in transverse wood permeability during the drying of rimu and radiata pine
1990 - IRG/WP 3636
When softwoods are dried and subsequently impregnated with waterborne preservatives two problems frequently occur, preservative screening of multi-salt preservatives and difficult re-drying. To study the causes, the permeability of rimu and radiata pine wood has been measured along the three principal directions. The radial and tangential permeabilities of the green sapwood of the two species were...
R E Booker


New method to find out the volatile organic compounds (VOC) of wooden material
2000 - IRG/WP 00-20189
Volatile organic compounds (VOC) of pine, spruce and larch wood were studied using a new technique developed at VTT Chemical Technology. 50 mg of crushed wood material was placed into glass tubes. The tubes were closed with a glass wool, which is pressed with a tube cap. Wood samples were analysed with a gas chromatograph after thermal desorption using four different temperatures (50°C, 100°C, 1...
H Viitanen, K Villberg, K Saarela


Estimating the size of subterranean termite colonies by a release-recapture technique
1980 - IRG/WP 1112
The technique is described and the results of an exploratory field trial are presented. The colony size estimate from weekly termite collections varied considerably, but nevertheless permitted assigning termites at three locations to three categories of greatly different colony size. The sizes of the three estimates were much greater than anticipated and included a multimillion termite complex of ...
G R Esenther


The results of detection on CCA components of the soils contacted with CCA-treated woods - A trial study for the availability of the burial Method as a disposal CCA treated wood waste
1993 - IRG/WP 93-50005
The objecteve of this experiment is to get a knowledge that, when CCA treated wood wastes were buried in a soil as a disposal, the soil would be or not be contaminated by the components of CCA preservatives in wood wastes. The specimens used were cutting logs and chips made of the CCA treated electric pole waste. The soil was buried to the 15 cm depth and the log specimens were set in the soil for...
K Suzuki, H Sonobe


The “wire-loop slicing technique” for the rapid field collection of large numbers of Coptotermes acinaciformis termites from above-ground mound colonies
2006 - IRG/WP 06-10583
This technique of rapidly slicing through an above-ground C. acinaciformis mound colony with a steel wire-loop attached to a vehicle allows the collection of large numbers of termites. The sliced mound topples onto a tarpaulin arranged on the ground, the outer wall layers break away in large segments, and the carton materials incorporating the termites are readily collected and transferred to larg...
B M Ahmed, J R J French


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...