Assessment of the natural durability of four Ghanaian hardwoods against the white-rot fungus Coriolus versicolor and soft-rot using laboratory tests
2003 - IRG/WP 03-10498
The natural durability of two lesser-utilized species (LUS) (Corynanthe pachyceras Welw. (pamprana) and Glyphaea brevis (Sprengel) Monachino) (foto) from three forest districts, and two related primary species (Nauclea diderrichii (de Wild.) Merr. (opepe) and Nesogodornia papaverifera (A. Chev.) R. Capuron.) (danta) from one district in Ghana is assessed against Coriolus versicolor Linnaeus Quelet...
C Antwi-Boasiako, A J Pitman, J R Barnett


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Oxalic acid production of fifteen brown-rot fungi in copper citrate- treated southern yellow pine
2001 - IRG/WP 01-10388
Non-arsenical copper-based wood preservatives have grown in number since the 1980's as a response to environmental concerns posed by arsenicals. Interest in copper tolerant decay fungi has increased accordingly. Oxalic acid (OA) production by brown-rot fungi has been proposed as one mechanism of copper tolerance. Fifteen brown-rot fungi representing the genera Postia, Wolfiporia, Serpula,...
F Green III, C A Clausen


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Results of collaborative work on laboratory soft rot testing
1989 - IRG/WP 2341
S M Gray, D J Dickinson


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


IRG soft-rot stake test - Site 03 Australia. Progress Report No. 3
1982 - IRG/WP 3202
The performance of test stakes was examined after four (4) years. Hardwood stakes treated with CCA showed significant soft-rot attack. The exception to this was Alstonia scholaris which was similar in performance to Pinus sylvestris. A supplementary test containing stakes treated with CBC, PCP and creosote, showed attack in all hardwoods examined. Little decay was found in stakes of Pinus sylvestr...
L E Leightley, R S Johnstone


IRG soft rot stake test. Site: 03 Australia. Progress repor
1980 - IRG/WP 1114
IRG soft-rot test stakes were installed in site 03 Australia 16.6.77. The stakes have been inspected twice, (28.11.78 (Johnson, 1979) and 31.10.79) for signs of decay, and used to obtain fungal isolates. The condition of stakes in the supplementary soft-rot test has also been examined....
L E Leightley, D M Francis, R S Johnstone


Preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycetes
2001 - IRG/WP 01-10397
Lyophilization is an excellent technique for the long-term preservation of hyphal-forming brown- and white-rot wood-inhabiting basidiomycotina. However, vegetative mycelial isolates are not lyophilizable. In this study, 10 brown-rot and 10 white-rot basidiomycetous non-sporulating, non-chlamydosporulating, and non-bubillerferous basidiomycetes fungi were tested for viability after lyophilization. ...
S C Croan


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory


Theoretical and practical experiments with eradication of the dry rot fungus by means of microwaves
1992 - IRG/WP 92-1577
Engineer Claus Andersen constructed a device in 1986 for microwave treatment of fungal infested timber. The device was tested on ampullae with live fungal mycelium of the dry rot fungus. A 10 minutes treatment at 37°C gave satisfactory eradicating effect. The method has since been used in practice in approximately 100 instances. A spot-test control has shown satisfactory results....
J Bech-Andersen, C Andersen


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


The use of image analysis to quantify soft rot decay
1992 - IRG/WP 92-2410
Image analysis techniques can provide quantitative information from visual images. As part of a wider interest in decay assessment methods we have investigated the application of image analysis techniques for quantifying soft rot decay by Chaetomium globosum in transverse sections of birch wood and bamboo. A method for reducing contamination of the section (and image) by the fungal hyphae and of s...
P J Wickens, R J Murphy


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki