Lignocellulotitic Hymenomycetes from native forest and Pinus elliottii Engelm in the Fontes do Ipiranga State Park, São Paulo, Brazil
1991 - IRG/WP 1468
Results show a distinct microflora for each forest type. A total of 9 families, 45 genera and 67 species were distributed among the two forest ecosystems were studied. Antrodiella, Auricularia, Grammothele, Steccherinum, Stereum and Trametes were found only in the native forest, where Antrodiella hydrophila (Berk. & Curt.) Ryv., Grammothele sp, Phellinus gilvus (Schw.) Pat., Rigidoporus microp...
M Aparecida de Jesus


Effect of borate on uptake and efficacy of an anti-sapstain treatment
2005 - IRG/WP 05-30380
The potential for using borates to enhance uptake and efficacy of propiconazole-based anti-sapstain chemicals was assessed on ponderosa pine sapwood wafers. Borates had no consistent effect on either net solution absorption or propiconazole distribution in the wood. Even small amounts of borate, however, markedly improved the performance of propiconazole against fungal discoloration. These resul...
Jianju Luo, Hua Chen, J J Morrell


The Effect of Soil pH on the pH of Treated Southern Pine in Ground Contact after 12 Months
2011 - IRG/WP 11-50281
Southern pine samples treated with soluble and particulate copper solutions were subjected to three soils that had been amended to provide acidic, neutral and alkaline conditions. Wood pH was measured prior to, and after 6 and 12 months after being placed in the soil to determine the effect of soil pH on wood pH....
L Jin, C Schauwecker, C Vidrine, P Walcheski, A Preston


Evaluation of Barrier Wrap Systems after 71 Months of Exposure
2013 - IRG/WP 13-40631
A 71 month study of the performance of booted samples in ground contact was conducted in AWPA hazard zone 4. Data indicated that excellent performance of wrapped systems, even over untreated wood, could be obtained. Instances of decay colonization or termite attack could all be attributed to some breaking of the integrity of the barrier system. Good performance for treatment below ground contact...
H M Barnes, M G Sanders, G B Lindsey, C McIntyre


Envelope treatment to protect softwood timbers from damage by subterranean termites
2003 - IRG/WP 03-30313
Two aboveground field trials were conducted in Australia to determine the effectiveness of envelope treatments of deltamethrin and permethrin for the protection of softwood framing timbers against termite damage. Radiata pine Pinus radiata D.Don and slash pine Pinus elliottii Englem., were treated with Tanalithä T (a novel solvent) to achieve 5-mm-depth envelopes. Details of a field trial against...
B C Peters, J W Creffield


The effect of steam conditioning on Southern yellow pine treated with copper naphthenate
1997 - IRG/WP 97-40086
The current study was undertaken to investigate the influence of steam conditioning on Southern yellow pine treated with copper naphthenate (Cu-N). Pre-steamed and /or kiln-dried Southern yellow pine were pressure treated with Cu-N. After treatment, one group of samples were post-steamed. It was found that samples changed color from green to dark-brown after post-steaming. To elucidate the effect ...
Jun Zhang, D P Kamdem, M H Freeman, R D Arsenault


Patterns of bacterial attack in preservative treated eucalypt power transmission poles
1984 - IRG/WP 1223
Patterns of bacterial decay have been examined using light and scanning electron microscopy. Two morphologically distinct patterns have been recognised in preservative treated eucalypt power transmission poles. Bacterial Decay I (BDI) involves the removal of the secondary wall layers initiating with erosion of the S3 layer from the cell lumen. As decay progresses the S2 layer and S1 layer are degr...
G A Willoughby, L E Leightley


The effect of treatment temperature on the biological performance of CCA treated wood
1990 - IRG/WP 3624
Birch and Scots pine sapwood blocks were treated with several concentrations of CCA at three different temperatures: 5, 20 and 35°C. The treated wood was maintained at the appropriate temperature for the fixation period. Leached and unleached samples were then exposed in a soft rot monoculture test using Chaetomium globosum and a brown rot monoculture test using Coniophora puteana. The treatment ...
S M Gray


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Marine performance of preservative treated Southern pine panels. Part 2: Exposure at Mourilyan Harbour, Queensland, Australia
2000 - IRG/WP 00-10337
Southern yellow pine panels treated with ACQ type B, ACQ type A, CCA type C, creosote, and copper naphthenate have been exposed at Mourilyan Harbour, north Queensland, Australia for almost 6 years. These panels have been inspected and rated for fouling and attack by Teredinid, Limnoria, Martesia, and Sphaeroma during this exposure. After 70 months exposure, overall performance of ACQ type B was eq...
A R Zahora, A F Preston, K J Archer, S Kleinschmidt


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Effect of permeability and extractives on the decay rate of southern pine sapwood in above grund exposure
2005 - IRG/WP 05-20310
The effects of wood permeability and hydrophilic and hydrophobic extractives on the decay rate of southern pine sapwood in above ground exposure were investigated. Permeability was determined by water sorption measurements, and the effect of extractives was studied by pre-extracting the test samples prior to outdoor exposure using water to extract hydrophilic extractives or sequential methanol/cy...
D D Nicholas, T Schultz, L Sites, D Buckner


Chemical analysis for TBTN in LOSP-treated wood and preservative fluids
1994 - IRG/WP 94-20027
Tributyltin napthenate (TBTN) is being substituted for tributyltin oxide (TBTO) in LOSP preservative formulations because its lower reactivity/better stability allows co-formulation with synthetic pyrethroids. Better stability may reduce molecular degradation both in-service and during analysis. It was considered necessary to check whether TBTO analysis methods were suitable for use on TBTN treate...
D P Wraight, M J Kennedy


The distribution of introduced acetyl groups and a linseed oil model substance in wood examined by microautoradiography and ESEM
2000 - IRG/WP 00-40169
Microautoradiography, a photographic method that shows the localization of substances labelled with radioactive isotope, and Environmental Scanning Electron Microscopy (ESEM) were combined to enhance sensitivity, resolution and reliability for examination of the distribution of introduced substances in wood. The preparation of microautoradiographs is less complicated when investigated with ESEM an...
M Rosenqvist


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Acetylation of lignocellulosic materials
1989 - IRG/WP 3516
A simplified procedure for the acetylation of lignocellulosic materials has been developed. The acetylation is done with a limited amount of liquid acetic anhydride without the addition of a catalyst or an organic co-solvent. Dimensional stability and biological resistance are both much improved by the acetylation. Equilibrium moisture content in acetylated material is considerably lower than in u...
P Larsson, A-M Tillman


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Testing method for the treatability of wood
1994 - IRG/WP 94-40031
In order to test and classify the treatability of wood species in pressure treatment processes with water-based solutions, a laboratory method was developed which allows the testing of small samples and limited sections of a stem, e.g. sapwood. The penetration of different liquids was determined separately concerning the three anatomical directions of wood. The common parameters for pressure impre...
A O Rapp, R-D Peek


Remedial treatment of joinery. Comparison of distribution of organic solvent preservative and ammonium bifluoride
1978 - IRG/WP 3115
It is some years since it was recognised in the United Kingdom that there was a problem of premature decay in untreated external joinery. Consequently, recommendations for preservative treatment were made by the Building Research Establishment, Princes Risborough Laboratory. In addition, the National House-Building Council has also included the preservative treatment of external joinery in its req...
J M Taylor


Incursion of Hylotrupes bajulus Linnaeus (European House Borer) into Western Australia
2005 - IRG/WP 05-10558
In January 2004, an adult Hylotrupes bajulus Linnaeus was detected emerging from a beam of Pinus pinaster in a house in Perth, Western Australia. The timber had been locally grown and milled. Surveys to define the extent of the infestation show it is restricted to dead pine trees in 28 sites around Perth. The biological and economic feasibility of eradication is being assessed. Since about 2001, k...
M Grimm


Influence of the peeling on the absorption in the sap displacement method
1990 - IRG/WP 3626
Results of tests on the Eucalyptus and pine fenceposts treated by sap displacement method are presented. Freshly cut post 2 m in length and 8 to 16 cm in diameter were placed for 6 days with their butt ends down in water soluble preservative solution (CCF) to a depth of about 65 cm, and these were inverted and kept in the same way for 3 days more. The treatment began a few hours after felling. The...