Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Chemical analysis of wood waste - The problem of sampling
1999 - IRG/WP 99-20168
A quantitative analysis of the content of active substances in wood is often demanded in quality control after processing and for the proper waste management. As a measure for quality control, analysis has the advantage that the type of preservative is known and assumptions can be made about its distribution in the treated wood.W aste wood may have been treated by a wide range of organic and inorg...
A Peylo, R-D Peek


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Melamine resins as preservatives results of biological testing
1996 - IRG/WP 96-40061
Based on previous work of the authors on resins, the upgrading of wood with a true solution of a methanol etherificated melamine resin in low aqueous concentration was performed. For the relative assessment of the biological resistance against brown and white-rot fungi were used not only untreated controls of pine sapwood (Pinus sylvestris L.), but also heartwood of European larch (Larix decidua M...
A O Rapp, R-D Peek


Evaluation of literature on adenocarcinomas in wood workers
1997 - IRG/WP 97-50092
Occupational exposure to wood dust alone or chemically treated is suspected to be associated with an increased risk of developing adenocarcinoma of the nasal cavity, which in the general population is very rare; fewer than 10% of nasal cancer deaths are adenocarcinomas, which have an annual incidence of 1-2 per million. However, the epidemiological data available are not sufficient to make a defin...
A Voss, R-D Peek


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


The chemical wood preservation in the former GDR - an overview
1995 - IRG/WP 95-50057
For the disposal of chemically treated wood waste and for the remedial treatment of contaminated soils in facility yards a profound knowledge is required concerning the kind of preservatives used and the degree of pollution. In order to record the production of wood preservatives and the location of impregnation plants in the former GDR, documents of the Office for Standardisation Measuring Affair...
E Melcher, R-D Peek


Alternative methodology for the environmental impact assessment of treated wood: the wood emissions ecotoxicology
2000 - IRG/WP 00-50161
Preservative products and technologies are important for optimising the use of wood and wood products in our society. The regulations of their use under the european Biocidal Products Directive 98/8/EC will require an evaluation of the environmental impact of treated wood. The methodology currently used for this determination is the PEC/PNEC ratio. It consists of calculating PEC values (Predictive...
P Marchal, H W Wegen, J Van Acker, E Melcher, R-D Peek, W J Homan, D Aston, D Rudolph, E F Baines


The waste wood situation in Germany - legislative and practical consequences
1998 - IRG/WP 98-50101-06
Waste wood or 'reclaimed wood' is produced in numerous areas of private and public life, in trade and in commerce, and its re-use is increasingly posing problems in Germany. This development has been reinforced as a result of legislation, such as the Trade Cycle and Refuse Act (KrW-/AbfG), the law regarding the supervision and control of the cross-frontier transportation of waste...
R-D Peek


COST Action E37. Sustainability Through New Technologies For Enhanced Wood Durability -
2008 - IRG/WP 08-40417
The main overall objective of the Action was to concentrate on the contribution of wood durability to sustainability through the development of systems for quality assurance and performance classification of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeked to improve and consequently to increase the cost-effective use of compon...