IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1129 documents. Displaying 25 entries per page.


Copper linoleate: A new low toxcity wide spectrum, heavy duty wood preservative
1995 - IRG/WP 95-30082
Copper linoleate, a "fixed" copper soap has been developed and evaluated in South Africa over a 30-year period. The initial product, an organic solvent based preservative has been tested in pine poles against termites and fungi. Results indiate that the product has performed well against existing heavy duty wood preservatives such as CCA and creosote in long term field trials (30 years). The paper...
D Conradie, P Turner, W E Conradie, A J Pendlebury, T Pizzi


Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods


Boron treatment methods for lyctid susceptible hardwoods growing in Tasmania
1998 - IRG/WP 98-30168
A survey of existing boron plants that treat to protect hardwoods from attack by lyctids in Australia showed that hot and cold bath, and vacuum pressure impregnation (vpi), were the two most common methods employed. In experimental work, two of the treatment methods, vpi and dip diffusion, were used to treat seasoned and green messmate (Eucalyptus obliqua) and blackwood (Acacia melanoxylon). The t...
L J Cookson, D Scown, K McCarthy


Steam/hold/APM boron treatment - Treatability trials with green gauged radiata pine
1987 - IRG/WP 3439
Freshly sawn 100 x 50 mm radiata pine was green gauged, steam conditioned and preservative treated with a mixture of borax and boric acid using a modified Alternating Pressure Method (APM) treatment schedule. A 12 hour holding period between steam conditioning and treatment resulted in the necessary moisture loss and moisture re-distribution to facilitate treatment to NZ Timber Preservation Author...
P Vinden


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


Reinfestation of consolidated ancient wood by insects
1998 - IRG/WP 98-10290
Wooden artifacts are often attacked by wood-destroying insects. Therefore conservators have to stabilize numerous objects from such attack. Initially we studied the resistance of painting materials and consolidants on unaffected recent wood against wood-destroying insects (IRG/WP 97-10239). Further, we wanted an answer to the question: Are artifacts, formerly destroyed by wood-borers, reinfested b...
W Unger, A Unger, U Schiessl


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


Effect of boron compounds-furfuryl alcohol treatment of wood on dimensional stability, termite resistance and boron leachability
2001 - IRG/WP 01-40195
Sapwood blocks of Japanese cedar (Cryptomeria japonica) and Caribbean pitch pine (Pinus caribaea) measuring 20 (tangential) x 20 (radial) x 10 (longitudinal) mm were impregnated with furfuryl alcohol (FFA) by a vacuum-diffusion process followed by curing under heating. Boron compounds (boric acid, ammonium borate and ammonium biborate) were mixed in the impregnation solution of FFA. Anti- swelling...
S K Ozaki, M K Yalinkilic, Y Imamura, M F Souza


Remedial ground-line treatment of CCA poles in service. A final report after 60 months' testing
1989 - IRG/WP 3534
Remedial treatment of CCA treated utility poles of Pinus sylvestris with incipient decay was carried out in 1983 and the results of chemical and microbiological analyses 6 months after treatment were reported in Document No: IRG/WP/3388 while microbiological studies 12 and 28 months after treatment as well as chemical analyses of poles treated with boron rods or boric acid paste 28 months after tr...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Inadequacies in preservative retention and formulation as contributory causes of premature failure of CCA-treated vineyard posts
1984 - IRG/WP 3280
Analyses of severely decayed or failed vineyard posts and examination of stake test data on effectiveness of copper-chrome-arsenate (CCA) preservatives have suggested two contributory causes of premature failure of vineyard posts: 1. Preservative retentions in posts are such that after 15 years' exposure some decay is inevitable. 2. The high arsenic, low chrome formulations with which the...
M E Hedley


Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


Preservative ability of wood to be fixed hydroxyl apatite substituted for antimicrobial metals
2001 - IRG/WP 01-30272
We succeeded in forming hydroxy apatite (HAp) in wood. HAp is non-toxicity and safe. Preservative ability of the wood, which substituted one part of Ca of constituent element of this HA p for antibacterial metals was measured. When Ca was substituted for Ag or Zn, mass loss in decay by brown-rot fungus F. palustris was restrained in about 50% (Ag) ~30% (Zn) of value of control specimen. However, w...
Y Haruhiko, I Sumaru


Distribution of copper/chrome/boron preservative in light red meranti (Shorea leprosula) before and after exposure test for 72 months
1995 - IRG/WP 95-20073
Copper/chrome/boron (CCB) preservative at 6% w/w was impregnated into light red meranti (Shorea leprosula) by full cell process. The quantitative analysis for copper, chrome and boron contents in treated wood samples was carried out by Inductive Couple Plasma (ICP). Electron Probe Microanalyser (EPMA) was used to monitor the distribution of copper, chrome and boron in the various treated wood tiss...
S Salamah, S Ani


Tendency of the preservative use for impregnation industries in Japan
1998 - IRG/WP 98-50101-05
In Japan, since 1997, the acceptable limit of the arsenic in the waste water become to 0,1 mg/l and the additional regional severer restriction can be established. In this reason, Japanese wood preservation industries intend to use other than CCA, like DDAC, ACQ, Tanalith CuAz, copper-naphthate and zinc-naphthenate, as replacing from CCA. In Jan-June 1997, the share of CCA preservatives was less t...
K Suzuki


Effectiveness of the new chemical wood preservative Borosol 9? against a house longhorn beetle Hylotrupes bajulus
2004 - IRG/WP 04-30355
Chemical wood preservative Borosol 9, consisting of boric acid - alkanolamine complex, is a new wood preservative with proven efficacy against wood decay fungi. However, we were interested in its efficacy against larvae of house longhorn beetle (Hylotrupes bajulus). Thus, experiment according to the EN 46 procedure was performed. Specimens made of Norway spruce wood (Picea abies) were ...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


An evaluation of the synthetic pyrethroid cypermethrin in organic solvent and emulsion formulations
1984 - IRG/WP 3290
The studies reported indicate that cypermethrin (NRDC 149) has considerable potential as an insecticide for wood preservatives. Cypermethrin appears to be about twice as effective as permethrin. The effectiveness of cypermethrin compared with g-HCH varies depending on the insect species, the phase of the life cycle and size of larva: for example, against mature Anobium larvae cypermethrin is appro...
S J Read, R W Berry


Development of wood retification process at the industrial stage
1998 - IRG/WP 98-50101-16
Wood is a natural composite material which exhibits outstanding properties from the technical as well as from the ecological point of view. However, it is an anisotropic, hygroscopic material sensitive to biological attacks. We have to stabilise and preserve it if we want to ensure its market shares faced with competing synthetic material, whilst taking the new environmental rules into account. T...
P Gohar, R Guyonnet


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


Application of energy dispersive X-ray fluorescence spectrometry to the quantitative analysis of organotin preservative solutions and treated wood
1978 - IRG/WP 3125
One technique frequently used for the quantitative analysis of material containing inorganic compounds is energy dispersive X-ray fluorescence spectrometry. It has been shown previously that this technique can be readily used to determine the retentions of chromated copper arsenate and ammoniacal copper arsenate treated wood. This paper reports the results of a preliminary study to determine wheth...
J N R Ruddick


Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


Previous Page | Next Page