IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


The extraction of boron from treated wood for quantitative analysis: A comparison of procedures
1992 - IRG/WP 92-2414
The extraction of boron preservative from treated rubberwood and scots pine samples was compared using methods based on refluxing and extraction in 1N NaOH or distilled water at 80°C. The extract solutions were analysed by Inductively Coupled Plasma spectroscopy (ICP/AES). A simple extraction procedure based on immersion of wood samples of approximate dimension 2 x 1 x 1 cm³ in distilled water a...
R J Murphy, D J Dickinson, P W McCormack, M K Lung


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Risk of extension of Hylotrupes bajulus attack in glued laminated timber
1977 - IRG/WP 278
Although efficient work-methods and maintenance procedures, which prevent the wood from becoming damp and are therefore successful in considerably reducing and even in excluding the risks of decay, such methods are ineffective in eliminating the risks of infestation and destruction of timber by the House Longhorn Beetle, Hylotrupes bajulus, the chief enemy of softwood timber structures. The possib...
M-M Serment


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


The control and pretreatment decay in air seasoning Scots and Corsican pine poles in England
1990 - IRG/WP 1451
Previous work clearly showed that air-seasoned, British grown Scots and Corsican pine poles are subject to serious pretreatment decay. In order to control these infections a range of pretreatments are currently being investigated. One series of treatments is designed not only to control decay but also allow the development of mould and stain fungi in order to achieve the desired increases in poros...
D J Dickinson, A R Zahora, A P Dodson


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Immunolabelling studies on the detection of enzymes during the degradation of wood by Phanerochaete chrysosporium
1988 - IRG/WP 1364
The degradation of lignin in native lignocellulosic substrates by white rot fungi is poorly understood. Biochemical studies have shown the involvement of a number extracellular ligninolytic enzymes released by white rot fungi which are capable of the oxidative conversion of DHP's (lignin model compounds) in vitro, but to date conclusive evidence for occurrence of these enzymes in wood und...
G F Daniel, T Nilsson, B Pettersson


Use of the enzyme-linked immunoassay (ELISA) and immunocytochemistry to detect soft rot in preservative treated and untreated wood
1990 - IRG/WP 2347
A polyclonal antibody was raised against mycelial extracts from the soft rot fungus Phialophora mutabilis. In ELISA assays, the antibody showed strong reactions with its own antigen and strong to moderate cross reactions with 6 other Phialophora soft rot species. With the exception of Ceratocystis albida, the antibody gave only weak or negative reactions with 11 other mold, blue stain and rot fung...
G F Daniel, T Nilsson


Environmental impact of PCP and NaPCP in the aquatic and atmospheric compartment
1995 - IRG/WP 95-50040-06
PCP and NaPCP were studied for their aquatic toxicity on bacteria, microalgae and daphnids and for their behaviour in the atmospheric compartment with a climatic chamber. Results of aquatic toxicity bioassays showed that toxicity was higher at low pH. This can be explained by the pKa value of 4.7 of PCP and the higher concentration of the non dissociated form of the pesticide at more acidic pH. Vo...
P Marchal, P Vasseur, G Ozanne


New research data confirming the suitability of bifenthrin as a wood preservative
1996 - IRG/WP 96-30116
Bifenthrin has been further tested against wood destroying insects, and its behaviour in wood has been extensively studied. Bifenthrin proved to be highly effective as a curative and preventative treatment against Anobium punctatum and Hylotrupes bajulus, after both leaching and evaporative ageing. Results of penetration tests with water and solvent based formulations, applied by brushing, dipping...
S Shires, P Héloir, B Chen, G Rustenburg


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Identification of fungi colonising coated and modified wood exposed outdoors using sequencing and T-RFLP profiling
2006 - IRG/WP 06-20326
Wood decay and staining fungi are known to colonize coated and modified wood. Rapid and reliable ways of identifying fungi on coated and modified wood may improve diagnostics and product development. In this work nine fungi growing in painted wood panels exposed outdoors at a test field in Uppsala, Sweden, were identified using sequencing and T-RFLP (Terminal Restriction Fragment Length Polymorphi...
U Råberg, J Bijelovic, C J Land, S Bardage, N Terziev


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


Chemical reactions involved in furfurylation of solid wood - An investigation by ATR-IR spectroscopy
2006 - IRG/WP 06-40347
Wood modification with furfuryl alcohol (FA) has gained renewed interest during the last five to ten years because of advances in process technology and because of increased focus on the environmental hazards of traditional wood impregnation. The reaction mechanisms involved in the furfurylation process are not yet understood in detail. In the work presented here, the chemical reactions and their ...
T Mark Venås, L Garbrecht Thygesen, S Barsberg


Microwave curing of furfuryl alcohol modified wood
2007 - IRG/WP 07-40371
Furfurylated wood has shown to have promising properties for a wood modification agent during the last years. In this paper, an alternative curing method for furfuryl alcohol modified pine sapwood by means of microwave radiation was investigated. Different process parameters of microwave treatment such as output power, exposure time to microwave radiation, initial wood moisture content and evapor...
A Treu, E Larnøy, H Militz


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Resistance against basidiomycetes of 1,3-dimethylol-4,5-dihydroxy ethylene urea (DMDHEU)-modified plywood of Pinus sylvestris
2008 - IRG/WP 08-40398
Plywood produced with rotary-cut veneers of Pinus sylvestris impregnated with a solution of 1.3 M 1.3-dimethylol-4.5-dihydroxyethyleneurea (DMDHEU) and glued with a phenolic resin (Prefere 4976 DYNEA) were inoculated with Coniophora puteana, Coriolus versicolor and Pleurotus ostreatus, following the European standard ENV 12038. The specimens were leached following European standard EN 84. The re...
A Dieste, A Pfeffer, S Bollmus, H Militz


Cantilever bending test of furfurylated poles
2008 - IRG/WP 08-40424
Ten, 8 m long poles of Scots pine (Pinus sylvestris) were treated with furfuryl alcohol to a WPG of approximately 40 %. A bending test was performed according to the principles in the draft European standard for wooden poles, prEN 14229 - Structural timber - Wood Poles for overhead lines. The bending strength and stiffness (MOE) for the poles tested were compared to an earlier study by the Swedish Wood Preservation Committee. In the latter study untreated, CCA-treated, ammoniacal Cu-PCP treated and creosoted poles were tested in bending. These types of poles were considered not to differ in strength and stiffness. The results of the furfurylated poles fit well with the results from the previous study. The bending strength and MOE values obtained are compared to the upper and lower 95-percentile values of the results from the previous study and all poles treated with furfuryl alcohol fit within this interval.Thus, this study indicates that a treatment with furfuryl alcohol does not result in a decrease of strength or stiffness. Further testing with a larger population of poles is necessary in order to get a statistically reliable result. In addition to further demonstration of the durability, the treatment process must be optimised to ensure full sapwood penetration and measures have to be taken to avoid the serious cracking observed in this trial before furfurylation can be considered for treatment of Pinus sylvestris poles.