IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 709 documents. Displaying 25 entries per page.


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Models of the critical time of humidity and temperature conditions for the development of mould fungi in pine and spruce sapwood
1995 - IRG/WP 95-20066
Regression models of the time factor for the growth of mould fungi in pine and spruce sapwood are studied. The first group of models are based on the results of exposures of mould fungi in static humidity and temperature conditions indicating the time for the start of mould growth in wood. The second group of models are based on the exposures of mould fungi in fluctuating or alternating humidity a...
H Viitanen


Laboratory trial to identify potential in-forest treatments to control fungal pre-infections of radiata pine logs
2000 - IRG/WP 00-30220
Development of fungal infections of radiata pine logs by wood degrading fungi commences immediately after tree felling. In general, subsequent antisapstain treatments are unable to control fungal degrade on logs where the pre-treatment log storage time exceeds 2-5 days. However, use of an in-forest treatment of logs may be advantageous to log exporters to control fungal pre-infections during the p...
D R Eden, B Kreber, R N Wakeling, J G Van der Waals, C M Chittenden


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Effect of bioextracts on colonisation of radiata pine sapwood by three sapstain fungi
2003 - IRG/WP 03-10485
The objective of this study was to investigate the effect of aqueous bioextracts prepared following two-week incubation of forest soil, garden compost and chicken manure respectively, on the ability of Ophiostoma flocossum, Leptographium procerum and Sphaeropsis sapinea to colonise unseasoned radiata pine sapwood. The research showed that all bioextracts tested retarded the rate of fungal colonis...
J van der Waals, C Chittenden, B Kreber


Leachability of didecyldimethylammonium chloride (a quaternary ammonium compound) from four wood species
1982 - IRG/WP 3204
Sapwood blocks prepared from red pine, ponderosa pine, southern yellow pine and hem-fir (a commercial mixture of western hemlock and amabilis fir) were treated with didecyldimethylammonium chloride, (an alkylammonium compound, AAC). After oven drying the blocks were vacuum impregnated with distilled water and subjected to a static leach cycle for 48 hours. The leachate was analyzed and the amount ...
J N R Ruddick, A R H Sam


Integrated protection of freshly sawn lumber using Bacillus subtilis and selected fungicide
1997 - IRG/WP 97-10235
Bioprotection against stain fungi has tremendous potential for reducing discoloration of freshly sawn wood while decreasing chemical consumption. Unfortunately, most bioprotectants appear to be unable to consistently perform under the array of conditions to which freshly sawn wood is exposed. While research is underway to understand the nature of the inconsistent performance, a more pragmatic appr...
M E Mankowski, M Anderson, J J Morrell


Performance of different treatments and finishes on wood out of ground contact. Preliminary results
1984 - IRG/WP 2221
Pinus and Eucalyptus L-joints treated with CCA, a water dispersable PCP and untreated ones were painted according to seven different finish's schedules and exposed at two sites in State of Sao Paulo. After ten months of exposure, it was possible to verify that preservative treatment improve the performance of both wood and finish. It was also possible to observe that wood substrate, prese...
S Milano


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


The effect of preservative distribution in small blocks of Pinus sylvestris on the toxicity of tributyltin oxide to Reticulitermes santonensis Feytaud
1971 - IRG/WP 206
Small blocks of Pinus sylvestris (50x25x15 mm³) were treated by a full-cell method with various concentrations of tributyltin oxide in benzene. Replicate blocks were then freeze dried, rapidly air dried or slowly air dried and exposed to surface attack by the subterranean moistwood termite Reticulitermes santonensis Feytaud. At all concentrations it was found that the freeze-dried blocks were mor...
M P Levi, D N R Smith


Diffusion into and bulking of the wood cell wall with polystyrene glycols (PEG)
1991 - IRG/WP 3660
The diffusion and equilibrium distribution of polyethylene glycol (PEG) in the cell walls of red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) were followed by analysing the free lumen solution concentration of vacuum treated wafers at various times after treatment. PEG was more-or-less excluded from the cell walls of wood, depending on the wood species and PEG molecular weight. ...
P A Cooper, Y T Ung, D Alexander, C Holzscherer


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 6: The length of the primary precipitation period
1975 - IRG/WP 359
The end of the primary precipitation fixation period of CCA preservatives coincides with the first peak in pH versus time. This offers a simple way of estimating the duration of the period. The duration is determined by a number of factors and their interactions, the most important of which are: wood species (anatomy, natural pH, accessibility of reducing agents), preservative type, preservative c...
S-E Dahlgren


Collaborative field trial out-of-ground contact
1982 - IRG/WP 2179
At the 12th meeting of the IRG in Sarajevo, Yugoslavia it was decided after considerable discussion that the best way to proceed with the work of the subgroup was to centre it around a co-operative field trial based on the L-joint test detailed in IRG/WP/2157. At the same time it was agreed that interested laboratories would also conduct their own methods, particularly the German planner test and ...
D J Dickinson, A F Bravery, J K Carey


The role of contact chemoreception in location of wood by the marine borer Limnoria (Isopoda)
1996 - IRG/WP 96-10157
This paper investigates the ability of Limnoria (Isopoda: Limnoriidae) to determine chemical differences in wood substrates, while in contact with the substrates. Test substrates were chosen on the basis of previous arguments concerning the chemical state of wood prior to Limnoria attack: microbial, ergosterol, metabolite, humic, extract and control (autoclaved) veneers were used as experimental s...
S M Henderson, S M Cragg


The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams


Assessing the leachability of chlorothalonil and methylene bis thiocyanate from antisapstain treated radiata pine
1998 - IRG/WP 98-30176
Rain wash-off and leaching of antisapstain fungicides from wood may cause pollution of waterways and may also lead to a decrease in the efficacy of a formulation against fungal degrade as chemicals deplete from the timber surface. In the current study, the leachability of chlorothalonil (CTL) and methylene bis thiocyanate (MBT), the active ingredients of a commercial antisapstain formulation, was...
B Kreber, T L Woods


Temperature and pressure inside wood during creosote impregnation
1991 - IRG/WP 3649
Creosote gives the best protection against decay for sleepers and poles. However, it has a major drawback - bleeding. Modified impregnation processes to reduce bleeding have been tried. For developing such processes it is important to know the actual temperature and pressure inside the wood. This paper describes measurement of temperature and pressure inside wood during creosote impregnation. The ...
Ö Bergman


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Field evaluation of CCA movement in sap-displaced copper chrome arsenic treated softwood poles
1989 - IRG/WP 3539
Commercial sap-displaced UK grown Scots and Corsican pine, and Sitka and Norway spruce poles were exposed in a field site at Dundee, Scotland and radial distribution profiles of CCA monitored prior to implantation and after subsequent field exposure. Results show that groundline levels of all preservative elements were higher after 1 and 2 years field exposure compared with those recorded prior to...
S D Hainey, G M Smith, A Bruce, P D Evans, B King, H J Staines


Performance of preservative-treated wood not in ground contact
1975 - IRG/WP 254
Experimental sash units of Pinus strobus L. and Pinus resinosa Ait. wood were removed from a test fence at Ottawa, Canada after outdoor exposure of over 20 years. The units were superficially treated, prior to painting, with preservatives containing either copper naphthenate, pentachlorophenol or a combination of zinc naphthenate and pentachlorophenol. Results indicated that all treatments were ef...
J K Shields, J Krzyzewski


Use of mixed populations of microflora to control sapstain on radiata pine
2002 - IRG/WP 02-10427
Most methods of biological control in the wood products field have focused on the use of single species of fungi or bacteria to control sapstain or decay. The approach taken in this study involved applying soil microorganisms, in combination with nutrients and various adjuvants that collectively form the biological control system. Radiata pine branch discs, autoclaved or fresh, were dipped in ...
C Chittenden, R Wakeling, B Kreber


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Previous Page | Next Page