Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


The extraction of boron from treated wood for quantitative analysis: A comparison of procedures
1992 - IRG/WP 92-2414
The extraction of boron preservative from treated rubberwood and scots pine samples was compared using methods based on refluxing and extraction in 1N NaOH or distilled water at 80°C. The extract solutions were analysed by Inductively Coupled Plasma spectroscopy (ICP/AES). A simple extraction procedure based on immersion of wood samples of approximate dimension 2 x 1 x 1 cm³ in distilled water a...
R J Murphy, D J Dickinson, P W McCormack, M K Lung


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Risk of extension of Hylotrupes bajulus attack in glued laminated timber
1977 - IRG/WP 278
Although efficient work-methods and maintenance procedures, which prevent the wood from becoming damp and are therefore successful in considerably reducing and even in excluding the risks of decay, such methods are ineffective in eliminating the risks of infestation and destruction of timber by the House Longhorn Beetle, Hylotrupes bajulus, the chief enemy of softwood timber structures. The possib...
M-M Serment


Exclusion of anions from the wood cell wall
1991 - IRG/WP 3661
Anionic components of wood preservatives and fire retardants such, as arsenates and phosphates, equilibrate at much lower concentrations in the cell wall bound water than in the free solution in the cell lumens. A degree of anion exclusion is expected in wood, due to the Donnan membrane effect. Fixed anions in the wood cell wall, produced by pH-dependent dissociation of the weak acid groups in woo...
P A Cooper


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Relating CCA fixation to leaching of CCA components from treated products
1995 - IRG/WP 95-50045
The relationship between chromium fixation in CCA-C treated wood, as determined by CrVI analysis of solution expressed from treated wood and the leaching of Cu, Cr, As and CrVI in a simulated rain test are evaluated for dimension lumber (2"x6") and pole sections. Leachate concentrations after 2 hour exposure to a misting spray (about 300 mm cumulative rainfall) decrease rapidly with increased degr...
P A Cooper, R MacVicar, Y T Ung


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


The effects of accelerated drying of green Pinus radiata on its attractiveness to Anobium punctatum as an egg-laying site
1984 - IRG/WP 1199
The methods and results are given for a series of experiments in drying Pinus radiata sapwood under a variety of conditions, then exposing the material to Anobium punctatum egg-laying. The results showed very clearly that the attractiveness of the wood to gravid females was drastically reduced when dried from green at temperatures much above 35°C. Both simple oven drying and steam kilning produce...
D J Cross


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel