IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1129 documents. Displaying 25 entries per page.


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Methylene Chloride compared with white spirit as a treatment solvent for wood preservation – results from decay and termite studies
2013 - IRG/WP 13-30611
Non-aqueous solvents have a long history in the treatment of wood products in various parts of the world. The most familiar solvent treatment is the ‘light organic solvent preservative’ (LOSP) treatment based on low density solvents such as white sprit. Until recently white spirit was the only non-aqueous solvent approved for use in wood preservation in New Zealand. Australia also permitted...
A Siraa, P Lobb, C Molloy


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Effect of soil contact on reacted copper(II) levels in micronized copper treated wood
2013 - IRG/WP 13-30616
Small 3 to 4 mm thick and approximately 80 to 100 mm long, samples were removed from wood treated with micronized copper quat (MCQ) or micronized copper azole (MCA) and buried full length in a soil bed. Samples were removed after 2, 4 and 8 weeks. The total copper was determined by x-ray fluorescence (XRF) spectroscopy and the amount of reacted micronized copper measured by electron paramagnetic r...
Wei Xue, P Kennepohl, Xingguo Jin, J N R Ruddick


Preparation of Copper Rosinate Emulsion and Its Resistance against Wood Decay Fungi
2013 - IRG/WP 13-30619
A leaching-resistant water-borne copper preservative was prepared by means of the following three steps: (1) Gum rosin was saponified with potassium hydroxide. (2) The soap reacted with copper sulfate to form copper rosinate. (3) The copper rosinate was emulsified with a mixture of Tween 20 and Span 80. Poplar (Populus ussuriensis) wood was impregnated with 0.5%, 1.0%, 1.5%, or 2.0% of the copper ...
Mingxin Zhang, Shujun Li, Qian Wang, Bo Li, Qiong Wu


Performance of untreated wood and wood impregnated with copper-ethanolamine based preservative solutions in Northern Adriatic Sea
2013 - IRG/WP 13-30623
Sea water applications of wood are among the most challenging ones. Impregnated wood is exposed to leaching and to variety of marine borers, Limnoria sp. and Teredo sp. being the most important. In the present research, durability of pine wood impregnated with copper-amine based preservative solution (Silvanolin) of different concentrations, exposed to the sea water, was investigated according to ...
M Humar, M Petrič, J Adamek, B Lesar


40 year results from the largest preservative in-ground stake trial conducted in Australia
2013 - IRG/WP 13-30624
The final results from Australia’s largest preservative in-ground stake trial are listed. There were eight test sites, six in Australia and two in Papua New Guinea. The preservatives tested include low and high temperature creosotes, PCP and various water-borne preservatives including CCA and copper chromate. The main timbers examined were sawn Pinus radiata sapwood, sawn Eucalyptus regnans hear...
L J Cookson


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Investigation of Nanocopper-Hygrothermally Treated Wood Properties
2013 - IRG/WP 13-40644
Nanometals with high thermal conductivity can be considered as modifiers, especially in thermal modification of wood. This study was aimed to investigate some physical and mechanical properties of nanocopper impregnated Iranian beach (Fagus orientalis Lipsky), which was hygrothermally treated. For this purpose, nanocopper solution (400 ppm) was used for impregnation process. Hygrothermal treatment...
G Rassam, B Jamnani, A Faraji Heris


Quantification of copper and chromium in field stakes after different exposure times: Remaining metal content and distribution
2013 - IRG/WP 13-50291
In order to determine the distribution of copper and chromium as well as their remaining concentration EN 252 specimens and thicker pine sapwood stakes (non standard format) were treated with a commercial CC salt in a vacuum pressure process. The stakes were installed in the test field of the Institute of Wood Research, Hamburg, in August 2010. In all cases three stakes were removed after 4, 8, 12...
T Liese, M Bahmani, E Melcher


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Incidence of soft rot attack on preservative treated Douglas-fir poles: a preliminary survey
2014 - IRG/WP 14-10818
Occurrence of soft rot decay in Douglas-fir poles treated with ammoniacal copper zinc arsenate (ACZA) or pentachlorophenol in oil was studied. Soft rot was less prevalent in poles treated with penta, but some soft rot was found in approximately 20 % of poles examined. Soft rot was more common in poles treated with ACZA, and, when present, was found in almost 20% of the cells examined. The potenti...
P Torres Andrade, J J Morrell


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Effectiveness of Copper Indicators in Treated Wood Exposed to Copper Tolerant Fungi
2014 - IRG/WP 14-20554
Wood treated with a copper based wood preservative will typically turn a green color. While the depth of copper penetration can be readily discerned from the green color of the copper it is standard practice in research and commercial treating plants to make use of a color reagent such as Chrome Azurol S, Rubeanic acid or PAN indicator to reveal the penetration more clearly. When copper treat...
L Jin, K Brown, A Zahora, K Archer


Previous Page | Next Page