Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Thermal stability of a wood protective biofinish and the influence of flame retardants on Aureobasidium cells
2017 - IRG/WP 17-30716
In general there is an increasing need for sustainable resources, including sustainable building materials. Wood is one of these sustainable resources and is more used as an outdoor building material. Since unprotected wood will usually be degraded during outdoor exposure, many different protection systems are available on the market. Protection systems containing biocides however might create obs...
S Rensink, E A M Klein Rot, M F Sailer


Evaluation of timber bridges with special consideration of detail design
2017 - IRG/WP 17-40781
Since 1997 the use of wood in bridge construction has been increasingly criticized by the Hamburg federal state authority supposedly because of shortened service life due to decay. With regard to wood research, however, it is often suggested that use of timber is suitable for weathered structures as long as constructive protection measures will be observed. In order to unravel the reasons for the ...
K Robbers, J Fromm, E Melcher


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


The potential and the challenges of acetylated wood in timber bridges - experiences from an ongoing project
2017 - IRG/WP 17-40792
Acetylated wood is known to be a durable and dimensional stable alternative for high performance materials, and has high potential for exterior timber structures. Research has shown that acetylated wood can be effectively bonded by various adhesive types. However, one of the most common used adhesives for timber constructions, Melamine Urea Formaldehyde (MUF), shows a high degree of delamination o...
A Treu, R Bredesen, F Bongers


Dual Borate and Copper Naphthenate Treatment of Bridge Timbers:- Potential Performance Enhancements and Cost Savings
2017 - IRG/WP 17-40797
Dual treatment technology combining diffusible preservatives with oil borne preservatives, widely used for crossties in the USA, has now also been commercialized with bridge ties/timbers. In order to understand the implications of these changes, the historic service life of creosote treated bridge timbers in northern and southeastern USA were considered as well as field test data for both creosote...
J Lloyd, C Brischke, R Bennett, A Taylor


Surface Protection of Wood with Metal Acetylacetonates
2017 - IRG/WP 17-40802
Metal acetylacetonates are coordination complexes of metal ions and the acetylacetonate anion. They have diverse uses as catalysts, cross-linking and curing agents and adhesion promotors. Some metal acetylacetonates can photostabilise polymers whereas others are photocatalysts. We hypothesise that the ability of metal acetylacetonates to photostabilise wood will vary depending on the metal in the ...
Yuner Zhu, P D Evans


Review on protection of timber bridges in Norway and other countries
2017 - IRG/WP 17-40809
Wood plays a major role in design and construction of modern bridges in Norway. Typical elements of those bridges are double impregnated glued laminated members, stress laminated timber decks, slotted-in steel plates, metal cladding of the surfaces of loadbearing members, and cross girders made of steel. Selected examples of timber bridges in Norway are presented. This review paper gives an overvi...
K-C Mahnert, U Hundhausen


Functional silicones used for wood protection: preliminary study
2017 - IRG/WP 17-30720
Due to worldwide regulation the wood preservation domain is constantly changing. Silicones are used for different industrial applications as hydrophobic agents. This property could enable to reduce water uptake of wood treated with these compounds. Treated wood could then be less prone to dimensional variation and fungal attack, those parameters being driven by variations in wood’s moisture cont...
C Reynaud, F Marchal, F Pochon, M Kutnik


UV-curable coatings developed for aesthetic and biological protection of wood outdoors
2017 - IRG/WP 17-40821
To avoid wood greying, dimensional variations, and degradation by biological agents wood is protected with preservation products and coatings when used outdoors. For some wood species used for cladding, a treatment with a preservation product is required, and is frequently additionally protected with a coating. In this study, Mäder Group developed a new UV-curable coating for outdoors application...
C Reynaud, A S Schuller, M Kutnik, L Podgorski


Imports of African logs, do they harbor wood-decaying alien fungi and bacteria that could become a potential threat at temperate latitudes? – First results
2018 - IRG/WP 18-10904
In this project we investigate the potential threat of alien wood-decaying fungal and bacterial species imported to Germany with logs from African countries. In a first approach we analysed fungal species on imported logs by identification of fruit bodies by DNA sequencing of the internal transcribed spacer (ITS) regions ITS1 and ITS2. First results revealed the existence of at least one alien fun...
J Trautner, M Höpken, E Melcher


Biocontrol of wood decay insects and nematodes as an alternative to traditional chemical treatments
2018 - IRG/WP 18-10914
The protection of wood has been defined until relatively recently, as the application of a chemical to increase its durability. On the other hand, society is becoming more and more demanding in terms of the use of products which have the minimum ecological impact. This has led many countries to reduce the list of biocidal products that can be used (European Biocides Regulation), therefore it is ne...
L Robertson, J F Galván, F Llinares, R Viñambres, M T de Troya


Liquefied wood polyols: Ecofriendly bio-based preservative for sustainable protection of wood from Termite attack
2018 - IRG/WP 18-10916
The major problems encountered in both indoor and outdoor utilization of wood are biological decay due to termite. The modification of wood with liquefied wood polyols has been found to be effective against termite attack. The liquefaction of wood aims to utilize woody wastes which are being generated during primary and secondary processing of wood in wood based industry. One of promising approach...
A Kumar, A John, T S Mehra, A K Pandey, S Singh Chauhan


Hibernation or spring awakening? – The research on wood durability and protection in marine environment
2018 - IRG/WP 18-10929
Wooden structures in marine applications are exposed to severe degradation conditions caused by mechanical loads and wood degrading organisms. The present paper presents the use of wood in marine environments in Europe from a wood protection perspective and gives an overview over relevant research topics. It compiles the most relevant literature with an emphasis on new wood protection methods and ...
A Treu, K Zimmer, C Brischke, E Larnøy, L R Gobakken, F Aloui, S M Cragg, P-O Flæte, M Humar, M Westin


Superior kempas hardwood protection with two proprietary microemulsion termiticdes based on permethrin and cyermethrin against Coptotermes termite attack under H2 an H3 weathered conditions found in buildings
2018 - IRG/WP 18-10931
SARPECO® and AXIL® solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping treatment but also for vacuum pressure tr...
D Messaudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


Rapid Screening test of potential antimicrobial agents for wood coatings
2018 - RG/WP 18-20644
A two-part screening test has been developed to evaluate additives for wood coatings. First, an additive is tested in the microbial laboratory and evaluated based on its inhibitory properties against selected test organisms, directly on agar plates. A microbial growth analysis is prepared and evaluated. If the additive is considered effective, it will be tested in a standard top coating (acrylic o...
J Stenbæk, E Morsing, T Østergaard Jensen


Liquefied wood polyols: a bio-based preservative for protection of wood from fungal decay
2018 - IRG/WP 18-30725
The liquefaction of wood is one of promising approaches in utilization of woody waste which is generated during primary and secondary processing of wood and liquefied wood having various application including bio-based preservatives. The biological degradation of wood due to fungi is the major problem encountered in indoor and outdoor utilization of wood. In this study, woody waste recovered from ...
A Kumar, G Vijaylakshmi, S Singh Chauhan


Effects of wood protecting biofinish and linseed oil on fire behaviour and leachability of the fire retardant
2018 - IRG/WP 18-30728
A wood protecting biofinish is based on a protective and decorative fungal-based coating and a linseed oil impregnation (called Xyhlo biofinish). This biofinish enables the long-term use of wood in outdoor applications without using toxic chemicals. The fire resistant properties of materials used in buildings are very important. Since Xyhlo biofinish is relatively new, only little information is ...
S Rensink, E J van Niewenhuijzen, M F Sailer


Recent findings clarifying the mechanism of brown-rot decay protection in acetylated wood
2018 - IRG/WP 18-40827
This paper summarizes the findings obtained during my PhD research over the past three years. The results provide insights which help to understand the enhanced brown-rot decay resistance of acetylated wood with particular emphasis on the role of water. The protection acetylation provides is derived from moisture exclusion within the acetylated cell wall, but the exact mechanism by which water is ...
G Beck


An examination of the potential for the use of the Maillard reaction to modify wood
2018 - IRG/WP 18-40829
Finding efficient ways to decrease wood decay caused by fungi and increasing its dimensional stability is an important issue in the timber construction. A possible way to avoid wood decay by fungi is by reducing the water content of wood, since water is a primary condition for fungal growth. Bulking of the wood cell wall by chemical reagents occupies the space where water normally occurs. At the s...
K Peeters, E Larnøy, A Kutnar, Č Tavzes, C A S Hill


Properties and potential use of Irvingia gabonensis and Irvingia wombolu kernel extracts as natural wood adhesives: Towards formaldehyde free wood composite products
2018 - IRG/WP 18-40832
Irvingia species are widely distributed in central and West Africa as well as parts of Asia and are earmarked for domestication due to the multitude of potential products that can be obtained from them. With renewed interest in renewable sources, the current study establishes the feasibility of utilizing extracts from Irvingia gabonensis and Irvingia wombolu kernels as wood adhesives. Proximate an...
A O Alawode, S O Amiandamhen, M Meincken, L Tyhoda


Preventivephysical barriers against subterranean termites species for building protection: How to implement innovative materials to reach efficacy requirements
2018 - IRG/WP 18-40845
As the European regulation dealing with the use of biocides (BPR) for preventive protection of buildings against subterranean termites is leading to more and more pressure on physico-chemical barriers currently used (PT18), some existing developments are focusing attention on physical biocides-free barriers. The main target is then to avoid the use of active ingredients, to stay out of the BPR sco...
N Delourme-Fonseca, P Poveda, F Simon


Polyesterification of wood using sorbitol and citric acid under aqueous conditions
2018 - IRG/WP 18-40851
The aim of this research is to determine if the polyesterification of sorbitol and citric acid in wood has a future potential as a wood modification process. Pine wood was impregnated with an aqueous solution containing citric acid and sorbitol and was thereafter cured at 103, or 140°C for 18 hours. The dimensional stability and leaching resistance were studied for both modification temperatures....
E Larnøy, A Karaca, L R Gobakken, C A S Hill