Basisiospore production by Lentinus lepideus in vitro
1987 - IRG/WP 2276
Evaluation of fungicides active against the lower fungi by spore based bioassays is very common. Possibilities of using similar assays to evaluate preservatives against brown rot and white rot fungi, especially for use in above ground constructions, are limited by the lack of methods for production of basidiospores. Tested media containing glucose 10-30 g/l and ammonium tartrate concentrations 2-2...
J Bjurman


Emissions from the combusting of boron and fluoride containing wood
1995 - IRG/WP 95-50040-18
The combustion properties of waste wood and wood residues containing wood preservatives were investigated in several test series after having been blended with untreated wood at a ratio of 1:4. The results for CFB, SF and boric salt show that, provided an optimized combustion, the concentrations of the stack pollutants correspond approximately with those found for untreated wood. Only during the c...
T Salthammer, H Klipp, R-D Peek


Formation of polychlorinated dibenzo-p-dioxins (PCDD) and polychlorinated dibenzofurans (PCDF) during the combustion of impregnated wood
1995 - IRG/WP 95-50040-19
Wood waste and industrial wood residues often contain various preservatives. The waste management for these residuals can be recycling, deposition or combustion. Among the three possibilities, combustion seems to be the most efficient way of disposal. To obtain detailed information about emissions of organic compounds with environmental impact, especially polychlorinated dibenzo-p-dioxins (PCDD) a...
T Salthammer, H Klipp, R-D Peek


Selection of heat flux value for wood fire retardants testing using MLC
2018 - IRG/WP 18-40846
One of more crucial elements of investigating treated wood combustion properties with the use of a cone calorimeter is a proper selection of heat flux (HF). The HF level is directly reflected in time to ignition and a thermal degradation degree. The ignition of raw wood or of wood ineffectively protected against fire occurs at a low HF level, i.e. 10-20 kW/m2. By contrast, the ignition of wood whi...
B Mazela, W Perdoch, W Grześkowiak, A Batista


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


The influence of crystalline and amorphous cellulose on extracellular hydrogen peroxide production by brown-rot fungi
1991 - IRG/WP 1482
The production of hydrogen peroxide (H2O2) has been suggested to play a key role in the degradation of wood by wood-rotting fungi. The production of extracellular hydrogen peroxide was studied by a quantitative method which detects the oxidation of the 2,2-azinobis(3-ethylbenzthiazoline-6-sulphonic acid) (ABTS) by H2O2 and horseradish peroxidase (HRP) in liquid culture medium. The carbon sources u...
A-C Ritschkoff, L Viikari


Cytochemical localization of hydrogen peroxide in brown rot fungus Tyromyces palustris by cerium chloride technique
1999 - IRG/WP 99-10299
Cerium chloride (CeCl3) was used to localize H2O2 cytochemically for studying relationship between ultrastructural and functional characteristics of cellulose degradation by brown rot fungi. This technique proved very useful in localizing discrete electron-densereactionproducts at high resolution with minimal nonspecific deposition. The cytochemical localization of extracellular H2O2 by CeCl3 usin...
Yoon Soo Kim, Seung-Gon Wi


Studies on the infestation behaviour of the powder-post beetle Lyctus brunneus (Steph.) and its physical control in the wood yards of the Caspian forests of Iran
1985 - IRG/WP 1271
Lyctus brunneus (Steph.) is a pest which has not been previously thoroughly studied in Iran. It severely attacks Iranian hardwoods, especially those used in wooden houses and that have not been treated. Research work was necessary to determine the natural resistance of the most important timber species in Iran against this insect....
P Niloufari


Effect of fatty acid removal on treatability of Douglas-fir
1993 - IRG/WP 93-40008
Treatment of Douglas-fir with chromated-copper-arsenate (CCA) poses a major challenge. Several hypotheses based on the anatomical aspects as well as chemical reactivity of the preservative formulations with cell wall constituents and deposits have been proposed. Techniques to prevent pit aspiration or slow fixation reactions have, however, not significantly improved treatment. The presence of high...
S Kumar, J J Morrell


Collaborative soft rot tests: Results of analyses of soil samples
1976 - IRG/WP 263
C R Levy


The use of bifluorides-diffusion in remedial treatments
1983 - IRG/WP 3256
A description is given about the experience to date of a 14 years' development to bring bifluorides-diffusion from laboratory evaluation to commercial service application. The described treatment is an adjunct to good design and not a replacement for it. The process is also used with an injection method for the remedial treatment of premature decayed external joinery....
H F M Nijman


Diffusion of bifluorides and borates from preservative rods in laminated beams
1991 - IRG/WP 3644
Laminated beams from spruce, pine and larch were treated with two preservative rods, based on bifluorides and octaborate respectively. After 3 and 6 months placed in different climates (65% r.h., 100% r.h., water) the diffusion of the active ingredient was measured. After the 6 months period, the diffusion of the bifluorides was, in all species, ca. 5 times larger than the diffusion from octaborat...
H Militz


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Remedial treatment of joinery. Comparison of distribution of organic solvent preservative and ammonium bifluoride
1978 - IRG/WP 3115
It is some years since it was recognised in the United Kingdom that there was a problem of premature decay in untreated external joinery. Consequently, recommendations for preservative treatment were made by the Building Research Establishment, Princes Risborough Laboratory. In addition, the National House-Building Council has also included the preservative treatment of external joinery in its req...
J M Taylor


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


Evaluation of chlorpyrifos as an insecticidal component of a wood preservative
1984 - IRG/WP 3301
After two years of laboratory and field testing, chlorpyrifos is showing excellent potential as an insecticidal treatment to wood. In laboratory termite tests, retentions as low as 1-2 parts-per-million or approximately 0.0008 kg/m³ (0.00005 lbs/ft³) are effective against the Coptotermes formosanus. Laboratory leaching tests have shown no significant effect on the concentration of the retained c...
K Rose, J Kozuma, P Sparrow


A comparison of inductively coupled plasma spectroscopy and neutron activity analysis for the determination of concentrations in wood
1993 - IRG/WP 93-10048
As wood decays the ionic composition changes, with increases often being seen in the concentrations of Ca, Mg, Fe, Mn and sometimes K. The concentration of eight cations in red spruce sapwood and heartwood samples was determined independently by inductively coupled plasma spectroscopy (ICP) and by neutron activation analysis (NAA) as part of an effort to standardize our analytical procedures and c...
J Jellison, J Connolly, K C Smith, W T Shortle


Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


Utilization of nitrogenous substance by Serpula lacrymans
1989 - IRG/WP 1397
When Serpula lacrymans degrades wood, the fungus is considered to have to assimilate nitrogen, which is not abundant in the wood, from the third material. The strands/mycelium has grown into the soil under the floor of the wooden house damaged by the dry rot fungus. The authors analyzed the soil samples collected from the ground under the floors of the dryrotted houses. The samples which were coll...
S Doi, I Togashi


Production of exraxellular hydrogen peroxide and oxalic acid by brown-rot fungus Poria placenta
1995 - IRG/WP 95-10112
Hydrogen peroxide and oxalic acid have been suggested to be essential in the degradation of wood carbohydrates by brown-rot fungi. Hydrogen peroxide has been suggested to be one of the diffusible low molecular weight agents produced by brown-rot fungi for the degradation of wood carbohydrates by generating highly active radicals. The production of hydrogen peroxide and oxalic acid by Poria placent...
A-C Ritschkoff, M Rättö, J Buchert, L Viikari


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka