End grain sealing by polymer impregnation
1992 - IRG/WP 92-3708
The solution and dispersion characteristics of several hydrophobic derivatives of cellulose have been studied and the abilities of these polymers to afford effective end grain sealing of Corsican pine have been examined. Both solution and dispersion treatments with ethyl cellulose imparted good water repellency and end grain sealing to wood samples, however, the disperse systems possessed lower vi...
J M Lawther, W B Banks, D G Anderson, J A Cornfield


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


Glue laminated poles - Progress report after 12 years' testing
1992 - IRG/WP 92-3685
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each laminate is first treated wi...
J Jermer, Ö Bergman


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Kinetics of the dissociation of Cr, Cu, and As in fixed CCA-treated wood
2001 - IRG/WP 01-50168
The results of an experiment showing the kinetics of the dissociation of CCA compo-nents in water within treated wood samples are presented. Dry red pine (Pinus resinosa Ait.) samples were simultaneously vacuum-treated with water, then expressed to re-move the water at successive time intervals. The expressate was then analyzed for Cr, Cu, and As concentration by inductively coupled plasma (ICP). ...
L Waldron, P A Cooper


A study of the rate of fixation of various chromium-containing preservatives
1991 - IRG/WP 3653
Denmark, and Scandinavia in general, has perhaps the widest range of approved industrial wood preservative types in the world. As an aid in setting realistic fixation periods, work was undertaken to investigate the rate of fixation of chromium in CCA salt, CCA oxide, CCP, CCB, CC and CCF formulations at summer and winter temperatures. The rate of fixation measured in terms of the concentration of ...
L B Sheard


An appraisal of anti-sapstain chemicals in Queensland, Australia
1985 - IRG/WP 3331
Eleven formulations were tested in the field for effectiveness against sapstain, mould and fungi on Pinus elliottii in Queensland. The commercially used sodium pentachlorophenoxide (0.5% a.i.) and Captafol (0.2% a.i.) performed well. Busan 1009 (0.3% a.i.), Protek T (5.0% a.i.), Woodgard E.S. and E.C. (0.8% a.i.), together with sodium tetrachlorophenoxide (0.5% a.i.) offer potential as anti-sapsta...
L E Leightley


Preliminary observations on tributyltin treated Scots pine sapwood using 119Sn (Mössbauer and NMR) spectroscopic techniques
1984 - IRG/WP 3312
119mSn Mössbauer data are presented for bis(tributyltin) oxide, tributyltin ethanesulphonate, bis(tributyltin) carbonate and tris(tributyltin) phosphate, both in the pure form and in Scots pine sapwood. The structures proposed for these compounds, in the solid state, are supported by 119Sn nuclear magnetic resonance spectroscopy.
R Hill


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


Chemical treatment of chips for outdoor storage. Evaluation of sodium N-methyldithiocarbamate + sodium 2,4-dinitrophenol treatment
1980 - IRG/WP 2134
Fresh slash pine chips were treated by spraying them with a dilute aqueous solution of sodium N-methyldithiocarbamate and sodium 2,4-dinitrophenol. The were then formed into an experimental chip file 10 feet high, and the pile was maintained for seven months. The treatment effectively slowed heat release and retarded losses in wood substances, tall oil, pulp yield, and pulp strenght. Under certain...
E L Springer, M Benjamin, W C Feist, L L Zoch, G J Hajny


Protection of freshly felled timber against attack by bark boring insects
1981 - IRG/WP 1143
This report describes two experiments with the insecticide formulation Perigen, which contains the synthetic pyrethroid permethrin. At 0.2% w/v active ingredient individual logs were protected against bark boring beetles for 18 weeks. At 0.3% w/v active ingredients Perigen gave similar protection against insect attack to stacks of recently felled unbarked pine logs. This protection was at least eq...
J Dominik, P R Skidmore


Cavitation bacteria
1984 - IRG/WP 1235
A form of bacterial wood degradation is described. The term "cavitation bacteria" has been coined in order to describe the discrete cavities that are formed within the wood cell walls. The bacteria observed within the cavities appeared to be polymorphic with rounded as well as filamentous forms recognised. TEM studies suggest that the bacteria produce diffusable wood-degrading enzymes. Cavitation ...
T Nilsson, A P Singh


"Refractory" is a relative term. Incised alpine fir is treatable
1991 - IRG/WP 3670
While certain wood species carry a reputation for being 'treatable' this normally refers to the sapwood. For most Canadian species, heartwood penetration is the major determinant of whether treatment meets Canadian, USA and Japanese standards and in this respect alpine fir turns out to be a treatable species. Alpine fir is the fir component of the Western Canadian spruce-pine-fir...
P I Morris


The role of chitinase in bioprotectant activity against staining fungi
1996 - IRG/WP 96-10175
Chitin is an important structural component of the hyphae of many wood staining fungi and its disruption can lead to dramatic declines in their growth. A number of bioprotectants have been shown to produce chitinases in liquid cultures, but the role of these enzymes in bioprotection remains poorly understood. The levels of these enzymes was studied by inoculating ponderosa pine sapwood wafers with...
J Liu, J J Morrell


An unusual soft-rot decay pattern caused by the Ascomycete Hypoxylon mediterraneum (de Not.) J Miller
1984 - IRG/WP 1222
A distinct pattern of soft-rot decay has been observed for the fungus Hypoxylan mediterraneum (de Not.) J. Miller. This fungus also produced decay patterns typical of brown and white rot decay. The production of characteristic cavities by Hypoxylan mediterraneum was prolific in the hardwoods Eucalyptus maculata and Eucalyptus regnans, but infrequent in the softwoods, Pinus elliottii and Pinus radi...
D M Francis, L E Leightley


Fungus cellar and antisapstain field trial studies of six triazole fungicides
1995 - IRG/WP 95-30077
The efficacy of six triazole fungicides was compared using a fungus cellar soil bed test, a rapid antisapstain laboratory trial and a 36 week antisapstain field trial. After 21 months in the fungus cellar the mean soundness of radiata pine treated with 1.5 kg/m³ of cyproconazole, azaconazole, hexaconazole, tebuconazole, propiconazole and flusilazole in combination with 1.0 kg/m³ didecydimethyl a...
R N Wakeling, J G Van der Waals, R D Narayan, J B Foster, B E Patterson, P N Maynard


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


Evaluation of the permeability of fast grown wood species
1995 - IRG/WP 95-40042
The low natural durability of certain species of wood, implies the need for applying a protecting treatment to increase its life in service. Because of this, a knowledge of the permeability properties of the wood is desired. In this work, a simple and reliable method to evaluate the wood permeability is presented. For that, we have been used fast grown species, with low natural durability, Poplar ...
M T De Troya, A M Navarrete, E Sanchez, J E Garcia de los Rios, E L Rodríguez Trobajo


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


Deltamethrin effectiveness against subterranean termite attack on wood under natural conditions
1989 - IRG/WP 1407
On fighting subterranean termites on wood, out of ground contact, the synthetic pyrethroid Deltamethrin shows positive aspects such as its efficiency and low mammalian toxicity. To evaluate its performance in conditions very similar to those in service use, specimens of Pinus sp were treated with solutions of Deltamethrin diluted in "white spirits" at 0.005% (w/w) and 0.01% (w/w) and exposed in a ...
P A Zanotto


Chemical and biological investigations of double-vacuum treated windows after 7½ years in service
1985 - IRG/WP 3339
Earlier investigations of double-vacuum treated windows after five years in service have shown that tributyltin oxide (TBTO) degrades to di- and monobutyltin compounds and that the resistance of the wood against decay decreases. An investigation 2.5 years later of the same windows shows that the degradation of TBTO proceeds fast. After 7.5 years in service only 15-35% of the remaining organotin co...
M-L Edlund, J Jermer, B Henningsson, W Hintze


Field evaluation of anti-sapstain products
1987 - IRG/WP 3402
Product A based on methylenebisthiocyanate, product B based on methylenebisthiocyanate plus 2-thiocyanomethylthio-benzothiazole, product C based on 2-thiocyanomethilthio-benzothiazole and product D based on didecyl dimethil ammonium chloride plus 3-iodo-2 propynil butyl carbarnate were evaluated on Pinus radiata sawn timber as fungicides for sapstain and mould in the Sawmill Division of the Univer...
M C Rose, A Bedoya


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund