IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 655 documents. Displaying 25 entries per page.


ATP assay for the determination of mould activity on wood at different moisture conditions
1992 - IRG/WP 92-2397
To determine fungal responses to fungicides and environmental conditions and for detection of microbial activity in wood, sensitive and objective methods are needed. We have developed a suitable assay based on analysis of adenosine triphosphate (ATP) by using the luciferin-luciferase reaction. With the aid of this assay the activity of Penicillium brevicompactum on wood at different RH levels was ...
J Bjurman


Test of N-tritylmorpholine in combination with synthetic pyrethroids against marine borers in tropical Australia and Panama
1991 - IRG/WP 4168
Test blocks ol Pinus sylvestris sapwood were pressure impregnated with white spirit solutions of N-tritylmorpholine, either alone or in combination with permethrin, deltamethrin or cypermethrin. They were exposed in the intertidal zone at Mourilyan Harbour, North Queensland, Australia and subtidally at either end of the Panama Canal. After 5 months' exposure at Naos Island at the Pacific ...
S M Cragg, J D Bultman


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


A study of the decay type potential of seven soils
1992 - IRG/WP 92-1539
The aim of this experiment was to determine the significance of the fungal inoculum potential and physico-chemical properties of five field trial test site soils, a garden compost known to cause white rot in copper treated fence palings, and soil from a zone between 2 and 15 centimetres from a CCA treated post with brown rot, in causing differential decay type in Pinus radiata and Poplus deltoides...
R N Wakeling


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Comparative study on leaching of CCA from treated timber: Modelling of emission data
1994 - IRG/WP 94-50027
Results of a comparative study on leaching of CCA from treated timber are reported. The study aims at investigating the applicability of prestandard leaching test methods for modelling purposes. Prestandards used are the European standard proposed by CEN/TC38/WG11 and NEN 7345 (Dutch prestandard for building materials). Parameters of study are type of fixation, wood species (pine - spruce), specim...
G M F Van Eetvelde, M Stevens, L Van der Mijnsbrugge


Essais de collage de bois traités pour la réalisation d'éléments de charpente lamellées. (+ abstract dated September 1971, Influence du traitement de préservation sur le collage d'éléments de charpente lamellés collés et efficacité vis-a-vis de larves néonates)
1971 - IRG/WP 203
Le but du travail est de vérifier les propriétés générales d'une poutre lamellée collée après traitement des éléments la composant au moyen de formulations insecticides et fongicides commerciales à solvant clair dans les conditions les plus usuelles de fabrication. Les essences utilisées ont été: Epicéa - Pin sylvestre - Sapin de Douglas en planches rabotées de 80 cm de lo...
J Guillemain-Thévenot


Preventive effectiveness of petrol derivatives against blue-stain fungi
1992 - IRG/WP 92-3716
A possible application of fractions obtained on petrol pyrolysis is their use as a wood preservative against wood-decay and sap-stain fungi. From two of these fractions were prepared three different products (ST, STL and SST). The aim of this work has been the possibility of utilizing these products in the treatment of wood used for external joinery, determining their effectiveness against blue-st...
A M Navarrete, M T De Troya, E Sanchez, A Guijarro


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Glulaminated poles - Progress report after 7 years' testing
1987 - IRG/WP 3444
In 1979 a number of glulaminated poles with various preservative treatments were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each lamination is treated wi...
J Jermer, Ö Bergman


The growth and behaviour of Australian isolates of dry rot fungi, mainly Serpula lacrymans (Schum. ex Fr.) S.F. Gray. A comparision with the world literature
1983 - IRG/WP 1190
In Australia Serpula lacrymans occupies a rather unique environment, being restricted to growth within basal regions of buildings containing masonry. Its rate of timber attack in these situations appears to be far faster than that experienced in other parts of the world. Therefore the question arises as to how Australian isolates (particularly 16508 which has become a "standard" test fungus for so...
J D Thornton, O Collett


Fumigant movement in Canadian wood species
1984 - IRG/WP 3296
Pole sections prepared from seven Canadian wood species (Thuja plicata, Thuja occidentalis, Pinus contorta, Pinus resinosa, Pinus banksiana, Pseudotsuga menziesii, southern yellow pine) were fumigated with chloropicrin, methylisothiocyanate and Vapam and the rates of fumigant penetration determined. All three fumigants were applied directly into holes bored radially into the pole sections. Analysi...
J N R Ruddick


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Previous Page | Next Page