Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
While not a new preservative system, Ammoniacal Copper Zinc Arsenate (ACZA), had not previously been used to protect crossties. Its performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercia...
T Carey


Copper naphthenate treatment for wood crossties and timbers
2014 - IRG/WP 14-30647
Copper naphthenate (CuN) has a long history in wood preservation and is recently finding increased usage as a treatment for wooden crossties and timbers. One of the principal reasons that CuN has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity and environmental impact. CuN is a well proven non-restricted use pres...
J Brient


Field performance of wax treated wood
2014 - IRG/WP 14-30649
The durability and outdoor performance of wax treated Scots pine sapwood was investigated in above ground field tests. Therefore wood impregnated with three different waxes was exposed in horizontal lap-joint test which is running since eight years. Durability, wetting resistance and the susceptibility to checking has been investigated. In summary, all wax treated wood performed better compared to...
C Brischke, E Melcher


Effect of polyurea coatings on performance of Douglas-fir in tropical above ground exposures
2014 - IRG/WP 14-40665
The potential for using polyurea barriers to limit fungal and termite attack was investigated on Douglas-fir lumber and timbers. Termites were capable of penetrating the barrier to attack non-treated wood as well as wood dip-treated with disodium octaborate. The coatings were also exposed above ground for 48 months in Hilo Hawaii. Samples were dissected to detect internal decay. Coated non-trea...
S Uysal, J J Morrell


Performance of some wood modification treatments against marine borers
2014 - IRG/WP 14-40668
Since some years, new treatment technology to protect wood against wood destroying fungi is introduced. Limited knowledge on their resistance to water organisms is available. Therefore, the resistance of chemically modified wood was assessed in a field test according to the European Standard EN 275 over a period of 3 resp. 5 years at sites in the North Sea and the Baltic Sea. Scots pine (Pinus syl...
A Klüppel, C Mai, H Militz, S Cragg


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Interpretation of moisture monitoring data - Relevance of moisture content thresholds for fungal decay
2015 - IRG/WP 15-10839
It is widely accepted that besides temperature wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. Many approaches to predict the service life of wooden structures have therefore been based on using wood MC as one major input-variable to develop dose-response relationships between material climate and decay response. However, to impr...
L Meyer, C Brischke


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


The combined effect of wetting ability and durability on field performance – verification of a new prediction approach
2015 - IRG/WP 15-20565
Comprehensive approaches to predict performance of wood products are requested by international standards and the first attempts have been made in the frame of European research projects. However, there is still an immanent need for a methodology to implement the durability and moisture performance of wood in a performance classification system. The aim of this study was therefore to establish an ...
C Brischke, G Alfredsen, P-O Flæte, M Humar, T Isaksson, L Meyer


Introduction of the COST FP 1303 Cooperative Performance Test
2015 - IRG/WP 15-20567
COST Action FP 1303 “Performance of bio-based building materials” successfully started in October 2013 and an ambitious program was set up for the four year programme. COST Actions provide an excellent opportunity for collaborative research, e.g. in the frame of Round Robin tests. The idea of this respective test was to distribute a fairly simple test set up to as many places in Europe as poss...
M Humar, C Brischke, L Meyer, B Lesar, N Thaler, D Jones, S Bardage, C Belloncle, J Van den Bulcke, J M Abascal, G Alfredsen, D Baisch, B Brunnhuber, G Cofta, E Grodås, E Frühwald Hansson, M Irle, H Kallakas, J Kers, M Klamer, P Larsson Brelid, A B Maider, K C Mahnert, E Melcher, R Möller, M Noël, L Nunes, G A Ormondroyd, S Palanti, N Pfabigan, A Pilgård, A O Rapp, P Schumacher, E Suttie, T Teppand, M Touza, J Van Acker


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Factors Affecting Performance of Preserved Wood Decking Against Decay Fungi
2015 - IRG/WP 15-30663
Decking is the largest market for residential preserved wood in the United States. Preserved decking must be resistant to colonization by decay fungi initiating from spores, and occasionally from mycelia due to elevated soil levels or adjacent untreated wood. The most vulnerable parts of a preserved wood deck are untreated, or under-treated, wood that becomes exposed by field cuts and checking. Fi...
R Stirling, P I Morris


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Tall oil – performance after a decade of field exposure
2015 - IRG/WP 15-30672
Water repellents have the potential to enhance biocidal activity by reducing leaching and lowering the moisture levels in wood exposed to rains. A range of studies have been performed in order to evaluate the potentials of tall oils as wood protective systems. The general conclusion has been that tall oil can provide some protection but that they cannot compete with the copper and organic biocide ...
G Alfredsen, P-O Flæte


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Investigation of Dimensional Stability and Coating Performance of Different Heat-Treated Poplar Wood Before and After Accelerated Aging
2015 - IRG/WP 15-40702
In this investigation, coating performance of heat-treated poplar wood (Populus tremuloioes) in different environments, before and after accelerated aging was studied. Specimens with 150×100×20 mm and 20×20×20 mm in dimensions were prepared. Heat treatments were performed in air, steam and linseed oil media. Specimens were coated by alkyd based stain. Adhesion strength before and after aging, ...
A Talaei, D Ansari Movahed, G Rassam